Study on the mechanical properties and microstructure of a rich-watered grouting material

被引:9
作者
Wang, Bo [1 ]
Li, Bo [2 ,3 ]
Huang, Laisheng [1 ]
Zhang, Junxiang [4 ,5 ]
机构
[1] China Univ Min & Technol Beijing, Sch Emergency Management & Safety Engn, Beijing 100083, Peoples R China
[2] Henan Polytech Univ, Sch Safety Sci & Engn, Jiaozuo 454003, Henan, Peoples R China
[3] Henan Polytech Univ, Collaborat Innovat Ctr Coal Work Safety & Clean Hi, Jiaozuo 454003, Henan, Peoples R China
[4] Zhongyuan Univ Technol, Sch Energy & Environm Engn, Zhengzhou 451191, Henan, Peoples R China
[5] Anhui Univ Sci & Technol, Key Lab Safety & High efficiency Coal Min, Minist Educ, Huainan 232001, Anhui, Peoples R China
来源
MATERIALS TODAY COMMUNICATIONS | 2023年 / 35卷
基金
中国国家自然科学基金;
关键词
Rich-watered material; Microstructure; Mechanical strength; Hydration products; Borehole sealing; MULTIFIELD COUPLING MODEL; EARLY STRENGTH; GAS EXTRACTION; CEMENT PASTE; HYDRATION; DRAINAGE;
D O I
10.1016/j.mtcomm.2023.106261
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effective method of mine gas control and efficient development is gas extraction technology. The sealing effect of grouting material on borehole directly affects the efficiency of gas extraction. The new type of richwatered sealing material with suitable mechanical strength and significant plastic characteristics was developed based on the addition of accelererant, alkali activator, expansion agent and reinforcing agent to Portland cement for mining. The effect of reinforcing agent on the mechanical properties of materials under different w/c ratios was tested by RMT. By means of X-ray diffraction (XRD), scanning electron microscopy (SEM) and other test methods, the microstructure evolution of grouting materials and its influence mechanism on macroscopic mechanics were revealed. The results show that the crystal structures of hydration products AFt, Ca(OH)2 and CA-H regulate the development of mechanical strength of materials. The uniaxial compressive strength of richwatered grouting materials can reach 3.5-5.6 MPa and the residual strength is greater than 3 MPa in the range of rich-watered ratio of 0.9-1.3. The new rich-watered grouting material developed has significant plastic deformation characteristics under high rich-watered ratio conditions, which can greatly adapt to borehole deformation and reduce the gap width of slurry-coal interface, and can meet the technical requirements of longterm sealing of gas extraction boreholes.
引用
收藏
页数:11
相关论文
共 48 条
  • [1] Hydration Mechanism of Gypsum-Slag Gel Materials
    Ai Yong-ping
    Xie, Shi-kun
    [J]. JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2020, 32 (01)
  • [2] A review of early-age properties of cement-based materials
    Bentz, D. P.
    [J]. CEMENT AND CONCRETE RESEARCH, 2008, 38 (02) : 196 - 204
  • [3] Preparation of Ca/Al-Layered Double Hydroxide and the influence of their structure on early strength of cement
    Cao, Lei
    Guo, Jintang
    Tian, Jianhua
    Xu, Yang
    Hu, Miaomiao
    Wang, Meiyu
    Fan, Jinjie
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2018, 184 : 203 - 214
  • [4] Effect of optimized pore structure on sealing performance of drilling sealing materials in coal mine
    Dong Kai
    Ni Guanhua
    Xu Yuhang
    Xun Meng
    Wang Hui
    Li Shang
    Sun Qian
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2021, 274
  • [5] Effect of individual phases on multiscale modeling mechanical properties of hardened cement paste
    Gao, Xiang
    Wei, Ya
    Huang, Wei
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2017, 153 : 25 - 35
  • [6] Studies on combined effects of graphene oxide-fly ash hybrid on the workability, mechanical performance and pore structures of cementitious grouting under high W/C ratio
    Gao, Yuan
    Jing, Hongwen
    Fu, Guangping
    Zhao, Zhenlong
    Shi, Xinshuai
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2021, 281
  • [7] Experimental investigation of cement-based sealing materials for degasification using coal-bed methane drainage system
    Hao, Min
    Song, Xiaolin
    Shi, Haitao
    Zhou, Fubao
    Shi, Bobo
    [J]. MATERIALS EXPRESS, 2018, 8 (02) : 113 - 122
  • [8] Micromechanical multiscale fracture model for compressive strength of blended cement pastes
    Hlobil, Michal
    Smilauer, Vit
    Chanvillard, Gilles
    [J]. CEMENT AND CONCRETE RESEARCH, 2016, 83 : 188 - 202
  • [9] Physicochemical effects of nanosilica on C3A/C3S hydration
    Hou, Pengkun
    Wang, Xinming
    Zhao, Piqi
    Wang, Kejin
    Kawashima, Shiho
    Li, Qinfei
    Xie, Ning
    Cheng, Xin
    Shah, Surendra P.
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2020, 103 (11) : 6505 - 6518
  • [10] A review on the mechanical properties of cement-based materials measured by nanoindentation
    Hu, Chuanlin
    Li, Zongjin
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2015, 90 : 80 - 90