Evaluation of Rutting and Fatigue Behavior of Modified Asphalt Binders with Nanocomposite Phase Change Materials

被引:6
作者
Amini, Nahid [1 ]
Hayati, Parham [1 ]
Latifi, Hassan [1 ]
机构
[1] Islamic Azad Univ, Dept Civil Engn, Sci & Res Branch, Tehran, Iran
关键词
TiO2; Nanocomposite PCM; Aging; Fatigue; TES; Rutting; HIGH-TEMPERATURE PERFORMANCE; CREEP; PREDICTION; RECOVERY; CRACKING; MODELS; ENERGY; TESTS; DSR;
D O I
10.1007/s42947-022-00156-z
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In this study, the influence of modifying asphalt binder with TiO2, Al2O3 as a phase change material, and multiwalled carbon nanotube (MWCNT) as an accessory of the nanocomposite PCMs, were investigated on rutting and fatigue behavior of asphalt binders. First, rotating thin-film oven (RTFO) and pressurized aging vessel (PAV) tests were conducted. Then, some analyses and tests, including scanning electron microscopy (SEM), differential scanning calorimetry (DSC), rotational viscosity (RV), multiple stress creep recovery (MSCR), linear amplitude sweep (LAS), and loaded-wheel tracking (LWT), were carried out. RV and DSR tests showed that the modified asphalt binders had more viscosity and aging resistance compared to pure asphalt binders, especially the ones including nanocomposite structure of PCMs role of TiO2 alongside MWCNT. Fatigue life in the LAS test for TiO2-MWCNT modified was more than 1.7 times the PP value (Control sample). MSCR test results indicated that the best improvement according to J(nr) values was for TiO2-MWCNT-modified asphalt binder, especially at higher temperatures because of their high specific heat capacity (C-p) as a PCM material. In addition, TiO2-MWCNT-modified asphalt binder almost met the Jnr limitation for much heavy traffic and heavy traffic loading at 64 & DEG;C and 70 & DEG;C, respectively. In general, combinations with the nanocomposite structure of PCMs were the best ones. In summary, aging index (AI) and G* x sin (& delta;) did not accurately confirm each other, while G* x sin (& delta;) and fatigue life from the LAS test were accurately correlated.
引用
收藏
页码:678 / 692
页数:15
相关论文
共 69 条
[1]  
AASHTO, 2012, AASHTO TP 101
[2]  
AASHTO T., 2011, Standard method of test for surface resistivity indication of concrete's ability to resist chloride ion penetration
[3]   Correlation between permanent deformation-related performance parameters of asphalt concrete mixes and binders [J].
Adorjanyi, Kalman ;
Fueleki, Peter .
OPEN ENGINEERING, 2013, 3 (03) :534-540
[4]  
American Association of State Highway and Transportation Officials (AASHTO), 2013, SPEC TEST PROC
[5]  
Amini N, 2021, JORDAN J CIV ENG, V15, P277
[6]  
[Anonymous], 2011, AASHTOT315
[7]  
[Anonymous], 2017, AASHTOT31613
[8]  
[Anonymous], 2015, D740515 ASTM ASTM IN
[9]  
[Anonymous], 2010, AASHTOMP19
[10]  
[Anonymous], 2015, D3418 STANDARD TEST