Effect of In-Situ Ti2N on Microstructure and Properties of SAF2906 Duplex Stainless Steel Fabricated by Laser Melting Deposition

被引:4
|
作者
Liang, Jing [1 ]
Yang, Sheng [1 ]
Liu, Ye [1 ]
Yin, Xiuyuan [1 ]
Chen, Suiyuan [1 ]
Liu, Changsheng [1 ]
机构
[1] Northeastern Univ, Sch Mat Sci & Engn, Key Lab Anisotropy & Texture Mat, Key Lab Addit Mfg & Remfg Mat,Minist Educ, Shenyang 110819, Liaoning, Peoples R China
基金
国家重点研发计划;
关键词
Laser melting deposition; SAF2906 duplex stainless steel; Molybdenum content; Nano TiN; Nano and submicron Ti2N; MECHANICAL-PROPERTIES; CORROSION-RESISTANCE; PROCESS PARAMETERS; METAL-DEPOSITION; WEAR BEHAVIOR; TIN; DUCTILITY; STRENGTH; POWDER; PARTS;
D O I
10.1007/s12540-022-01360-z
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
SAF2906 Duplex Stainless Steel (DSS) was fabricated by powder prepasted Laser Melting Deposition(LMD). The formation of ferrite was promoted by increasing the molybdenum content. The volume ratio of ferrite and austenite of LMDed SAF2906 DSS with 3 wt% molybdenum content reached 4:6. The effects of 2 wt% and 4 wt% nano TiN addition on the microstructure and comprehensive properties of LMDed SAF2906 DSS were investigated in detail. The results showed that in-situ generated nano (10 nm similar to 100 nm) and submicron (100 nm similar to 1 mu m) Ti2N particles were uniformly distributed in the LMDed SAF2906 DSS matrix, and some nano Ti2N particles preferred to be distributed among grain boundaries. The primary and secondary dendrite spacing of austenite of LMDed SAF2906 with 4wt% TiN addition decreased by 48% and 62%, respectively, while the austenite content increased by 15%. The wear resistance, strength, elongation and corrosion resistance of the LMDed SAF2906 were gradually improved with the increase of nano TiN addition from 0 to 4 wt%. The average microhardness for the sample with 4 wt% nano TiN addition (381 HV0.2) was 1.2 times that of the sample without TiN (326 HV0.2), while the wear rate (9.12 x 10(-13) m(3)/Nm) was only 71% that of the sample without TiN (1.28 x 10(-12) m(3)/Nm). The yield strength, tensile strength and elongation of the LMDed SAF2906 with 4wt% TiN addition increased to 801 MPa, 1028 MPa and 31.8%, respectively. The self-corrosion potential increased to 0.0216 V, and the self-corrosion current density also reached 4.57 x 10(-7) A center dot cm(-2) for LMDed SAF2906 with 4wt% TiN addition.
引用
收藏
页码:2052 / 2071
页数:20
相关论文
共 50 条
  • [41] Directed laser deposition of super duplex stainless steel: Microstructure, texture evolution, and mechanical properties
    Sayyar, Navid
    Hansen, Vidar
    Tucho, Wakshum Mekonnen
    Minde, Mona Wetrhus
    HELIYON, 2023, 9 (04)
  • [42] The deterministic effect of laser energy density on the microstructures of novel duplex stainless steel fabricated via in-situ alloying in laser powder bed fusion
    Li, X. C.
    Shen, F. L.
    Du, W. X.
    Cao, L. C.
    Pan, L. T.
    Ma, T. J.
    Fang, X. Y.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 891
  • [43] Effect of in-situ heat treatments on deposition characteristics and mechanical properties for repairs using laser melting deposition
    Oh, Wook Jin
    Son, Yong
    Shim, Do Sik
    JOURNAL OF MANUFACTURING PROCESSES, 2020, 58 : 1019 - 1033
  • [44] Formability, Microstructure and Properties of CxCrNiV Low-Alloy Steel Fabricated by Laser Melting Deposition
    M. E. Zhang
    S. Zhang
    X. Cui
    C. H. Zhang
    J. Chen
    J. B. Zhang
    Journal of Materials Engineering and Performance, 2020, 29 : 5018 - 5027
  • [45] Effect of heat treatments on the microstructure and mechanical properties of Ti2AlNb intermetallic fabricated by selective laser melting
    Zhou, Y. H.
    Wang, D. W.
    Song, L. J.
    Mukhtar, A.
    Huang, D. N.
    Yang, C.
    Yan, M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 817
  • [46] Effect of thermal cycles on microstructure of reduced activation steel fabricated using laser melting deposition
    Qian An
    Zhi-xin Xia
    Chi Zhang
    Zhi-gang Yang
    Hao Chen
    Journal of Iron and Steel Research International, 2021, 28 : 316 - 326
  • [47] Microstructure and mechanical properties of TiB2-reinforced 7075 aluminum matrix composites fabricated by laser melting deposition
    Bi Jiang
    Lei Zhenglong
    Chen Xi
    Li Peng
    Lu Nannan
    Chen Yanbin
    CERAMICS INTERNATIONAL, 2019, 45 (05) : 5680 - 5692
  • [48] Effect of boron element on microstructure and mechanical properties of 316L stainless steel manufactured by selective laser melting
    Zheng, Qi
    Chen, Hong Sheng
    Zhou, Jun
    Wang, Wenxian
    Xi, San Xiao
    Yuan, Ye
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 26 : 3744 - 3755
  • [49] EFFECT OF IN-SITU LASER POLISHING ON MICROSTRUCTURE, SURFACE CHARACTERISTICS, AND PHASE TRANSFORMATION OF LPBF MARTENSITIC STAINLESS STEEL
    Ali, Majed
    Almotari, Abdalmageed
    Algamal, Anwar
    Alafaghani, Ala'aldin
    Abedi, Hossein
    Qattawi, Ala
    PROCEEDINGS OF ASME 2023 18TH INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE, MSEC2023, VOL 1, 2023,
  • [50] Design, preparation, microstructure and properties of novel wear-resistant stainless steel-base composites using laser melting deposition
    Li, X.
    Zhang, C. H.
    Zhang, S.
    Wu, C. L.
    Zhang, J. B.
    Chen, H. T.
    Abdullah, Adil O.
    VACUUM, 2019, 165 : 139 - 147