Inclusion Characteristics and Acicular Ferrite Formation in the Simulated Heat-Affected Zone of Ti-Zr-Killed Low-Carbon Steel

被引:8
作者
Liu, Fangce [1 ]
Bi, Yue [1 ]
Wang, Chao [2 ]
Kang, Jian [2 ]
He, Tong [3 ]
Liu, Yandong [1 ]
Yuan, Guo [2 ]
机构
[1] Northeastern Univ, Key Lab Anisotropy & Texture Mat, Minist Educ, Shenyang 110819, Liaoning, Peoples R China
[2] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Liaoning, Peoples R China
[3] Northeastern Univ, Res Acad, Shenyang 110819, Liaoning, Peoples R China
基金
中国国家自然科学基金;
关键词
Low-carbon steel; Heat-affected zone; Impact toughness; Acicular ferrite; Inclusion; MECHANICAL-PROPERTIES; INTRAGRANULAR FERRITE; NUCLEATION; MICROSTRUCTURE; TRANSFORMATION; TOUGHNESS; MN; PARTICLES; BEHAVIOR; METAL;
D O I
10.1007/s12540-022-01254-0
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this paper, high temperature hot rolling and weld simulations were performed in Al-killed and Ti-Zr-killed steels. The microstructure and impact toughness of the heat-affected zone (HAZ) of the two experimental steels were investigated, and the ferrite transformation behavior in HAZ was also observed. The characteristic inclusions in the Ti-Zr-killed steel were studied using electron probe microanalysis (EPMA) and electron backscatter diffraction (EBSD). The results suggested that the HAZ microstructure of the Al-killed steel consisted of coarse bainite ferrite (BF) and granular bainite (GB) packets. The HAZ microstructure of Ti-Zr-killed steel was significantly refined and mainly contained fine acicular ferrite (AF) and BF. The Ti-Zr-O + MnS inclusions were 0.3-2.1 mu m and could effectively promote the formation of AF after the weld simulations. MnS had a specific orientation relationship: {111}(MnS) parallel to{0001}(Ti-Zr-O), < 110 >(MnS)parallel to < 2<(1)over bar>(1) over bar0 >(Ti-Zr-O) with Ti-Zr-O inclusion, and its precipitation promoted the formation of the Mn-depleted zone (MDZ). AF formed around it. The formation of an interlocked AF structure in the HAZ of the Ti-Zr-killed steel obviously increased the proportion of high angle grain boundaries (HAGBs) and refined the average effective grain size of the HAZ microstructure. Consequently, the impact toughness of the Ti-Zr-killed steel had no deterioration, but the impact toughness of Al-killed steel had an obvious loss after the weld simulation with a heat input of 70 kJ/cm. The impact absorption energy of HAZ of Ti-Zr-killed steel was improved from 6 to 219 J compared to Al-killed steel.
引用
收藏
页码:715 / 729
页数:15
相关论文
共 50 条
[21]   Effect of Thermomechanical Treatment on Acicular Ferrite Formation in Ti-Ca Deoxidized Low Carbon Steel [J].
Wang, Chao ;
Wang, Xin ;
Kang, Jian ;
Yuan, Guo ;
Wang, Guodong .
METALS, 2019, 9 (03)
[22]   Investigation of Inclusion Characteristics and Intragranular Acicular Ferrite Nucleation in Mg-Containing Low-Carbon Steel [J].
Wu, Xiaoyan ;
Wu, Shujing ;
Yan, Chunliang ;
Ma, Xuegang ;
Liu, Zengxun ;
Zhu, Liguang ;
Zhang, Qingjun .
METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2021, 52 (02) :1012-1022
[23]   The contribution of intragranular acicular ferrite microstructural constituent on impact toughness and impeding crack initiation and propagation in the heat-affected zone (HAZ) of low-carbon steels [J].
Xiong, Zhihui ;
Liu, Shilong ;
Wang, Xuemin ;
Shang, Chengjia ;
Li, Xiucheng ;
Misra, R. D. K. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 636 :117-123
[24]   Nucleation of intragranular acicular ferrite in the heat affected zone of Ti-bearing HSLA steel [J].
Zhang, Liqing ;
Wu, Kaiming .
ADVANCES IN BUILDING MATERIALS, PTS 1-3, 2011, 168-170 :837-841
[25]   In-situ Observations of Acicular Ferrite Growth Behavior in the Simulated Coarse-grained Heat-affected Zone of High-strength Low-alloy Steels [J].
Wan, Xiangliang ;
Wu, Kaiming ;
Cheng, Lin ;
Wei, Ran .
ISIJ INTERNATIONAL, 2015, 55 (03) :679-685
[26]   Effects of Mg-Al-O-Mn-S inclusion on the nucleation of acicular ferrite in magnesium-containing low-carbon steel [J].
Lin, Chi-Kang ;
Pan, Yan-Chi ;
Su, Yen-Hao Frank ;
Lin, Guan-Ru ;
Hwang, Weng-Sing ;
Kuo, Jui-Chao .
MATERIALS CHARACTERIZATION, 2018, 141 :318-327
[27]   Mechanism of BN-Promoting Acicular Ferrite Nucleation to Improve Heat-Affected Zone Toughness of V-N-Ti Microalloyed Offshore Steel [J].
Shi, Zhongran ;
Pan, Tao ;
Li, Yu ;
Luo, Xiaobing ;
Chai, Feng .
MATERIALS, 2022, 15 (04)
[28]   Effect of microstructure of simulated heat-affected zone on low- to high-cycle fatigue properties of low-carbon steels [J].
Nishikawa, Hide-aki ;
Furuya, Yoshiyuki ;
Igi, Satoshi ;
Goto, Sota ;
Briffod, Fabien ;
Shiraiwa, Takayuki ;
Enoki, Manabu ;
Kasuya, Tadashi .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2020, 43 (06) :1239-1249
[30]   Characterization of the Acicular Ferrite in Al-Deoxidized Low-Carbon Steel Combined with Zr and Mg Additions [J].
Min, Yi ;
Li, Xiaobing ;
Yu, Zhe ;
Liu, Chengjun ;
Jiang, Maofa .
STEEL RESEARCH INTERNATIONAL, 2016, 87 (11) :1503-1510