Spall damage in laser-powder-bed-fusion manufactured Ti-6Al-4V: Mechanisms and microstructure effects

被引:7
作者
Yang, K. [1 ]
Yang, X. [1 ]
Zhang, Z. L. [1 ]
Zhu, T. T. [2 ]
Li, J. [1 ]
Xiao, X. S. [1 ]
Liang, Y. X. [3 ]
Jian, B. [2 ]
Li, C. [1 ]
Luo, S. N. [1 ]
机构
[1] Southwest Jiaotong Univ, Sch Mat Sci & Engn, Chengdu, Sichuan, Peoples R China
[2] Peac Inst Multiscale Sci, Chengdu, Sichuan, Peoples R China
[3] Chongqing Univ, Coll Mat Sci & Engn, Int Joint Lab Light Alloys, Minist Educ, Chongqing, Peoples R China
关键词
Laser powder bed fusion; Titanium alloy; Martensite; Spall; Crack propagation; VARIANT SELECTION; DYNAMIC-RESPONSE; TITANIUM; BEHAVIOR; ALLOY; PHASE; DEFORMATION; MARTENSITE; ANISOTROPY; INITIATION;
D O I
10.1016/j.jallcom.2023.169379
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Spall damage of Ti-6Al-4V alloy fabricated via laser powder bed fusion (LPBF) is investigated via plate impact along the build direction (BD) and the transverse direction (TD), as regards its underlying me-chanisms and microstructure effects. Conventional hot-rolled Ti-6Al-4V alloys processed with annealing and quenching are also examined for comparison. Hugoniot elastic limit (HEL) and spall strength of the LPBF-fabricated samples are derived from free-surface velocity histories, and are higher for the TD loading than for the BD loading. The LPBF-fabricated alloy has a lower HEL but similar spall strength compared to the conventionally fabricated alloys. Quantitative analysis of recovered samples reveals that, the number of cracks is smaller and the mean crack length is larger in the LPBF-fabricated and quenched hot-rolled samples containing  martensite laths than the annealed hot-rolled sample containing equiaxed alpha grains. For the LPBF-fabricated samples, the TD loading induces cracks of similar length along  grain boundaries (GBs) and  {0001} planes, but much longer cracks along prior beta GBs compared to the BD loading. Anisotropy in mechanical properties and damage is due to columnar prior beta grains, morphological and crystallographic texture of  laths.(c) 2023 Elsevier B.V. All rights reserved.
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Dynamic a globularization in laser powder bed fusion additively manufactured Ti-6Al-4V
    Chen, J.
    Fabijanic, D.
    Brandt, M.
    Zhao, Y.
    Ren, S. B.
    Xu, W.
    ACTA MATERIALIA, 2023, 255
  • [2] Understanding the effect of scanning strategies on the microstructure and crystallographic texture of Ti-6Al-4V alloy manufactured by laser powder bed fusion
    Liu, Jiangwei
    Li, Guichuan
    Sun, Qidong
    Li, Hu
    Sun, Jie
    Wang, Xiebin
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2022, 299
  • [3] Microstructural evolution during post heat treatment of the Ti-6Al-4V alloy manufactured by laser powder bed fusion
    Lakroune, Yassine
    Connetable, Damien
    Hugues, Jonathan
    Hermantier, Paul
    Barriobero-Vila, Pere
    Dehmas, Moukrane
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 23 : 1980 - 1994
  • [4] The effects of specimens geometry on solidification conditions and microstructure formation in laser powder bed fusion fabricated Ti-6Al-4V alloys
    Zhao, Rijie
    Kou, Ronghui
    Wang, Haoliang
    Song, Chenghao
    Li, Chuan
    Sun, Zhenzhong
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 33 : 5030 - 5039
  • [5] Investigation of fatigue behavior of laser powder bed fusion Ti-6Al-4V: Roles of heat treatment and microstructure
    Liu, Jianwen
    Zhang, Kai
    Liu, Jie
    Wang, Hao
    Yang, Yi
    Yan, Liangming
    Tian, Xinni
    Zhu, Yuman
    Huang, Aijun
    INTERNATIONAL JOURNAL OF FATIGUE, 2023, 176
  • [6] Microstructure control in additively manufactured Ti-6Al-4V during high-power laser powder bed fusion
    Dhiman, Sahil
    Chinthapenta, Viswanath
    Brandt, Milan
    Fabijanic, Daniel
    Xu, Wei
    ADDITIVE MANUFACTURING, 2024, 96
  • [7] Laser powder bed fusion (L-PBF) of Ti-6Al-4V/Ti-6Al-2Sn-4Zr-2Mo and Ti-6Al-4V/γ-TiAl bimetals: Processability, interface and mechanical properties
    Fan, Haiyang
    Wang, Chengcheng
    Tian, Yujia
    Zhou, Kun
    Yang, Shoufeng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 871
  • [8] Effect of energy density on the microstructure and texture evolution of Ti-6Al-4V manufactured by laser powder bed fusion
    Cepeda-Jimenez, C. M.
    Potenza, F.
    Magalini, E.
    Luchin, V
    Molinari, A.
    Perez-Prado, M. T.
    MATERIALS CHARACTERIZATION, 2020, 163
  • [9] Microstructure and mechanical properties of laser powder bed fusion Ti-6Al-4V after HIP treatments with varied temperatures and cooling rates
    Derimow, Nicholas
    Benzing, Jake T.
    Joress, Howie
    McDannald, Austin
    Lu, Ping
    DelRio, Frank W.
    Moser, Newell
    Connolly, Matthew J.
    Saville, Alec I.
    Kafka, Orion L.
    Beamer, Chad
    Fishel, Ryan
    Sarker, Suchismita
    Hadley, Chris
    Hrabe, Nik
    MATERIALS & DESIGN, 2024, 247
  • [10] Numerical Modeling of Distortion of Ti-6Al-4V Components Manufactured Using Laser Powder Bed Fusion
    Ninpetch, Patiparn
    Kowitwarangkul, Pruet
    Chalermkarnnon, Prasert
    Promoppatum, Patcharapit
    Chuchuay, Piyapat
    Rattanadecho, Phadungsak
    METALS, 2022, 12 (09)