Effect of silicon on the formation of protective scale on Fe-10Ni-10Cr-4Al alloy pre-oxidized at low oxygen pressure

被引:5
|
作者
Yuan, Manman [1 ,2 ]
Zhao, Jinyu [1 ,2 ]
Liu, Ya [1 ,2 ]
Li, Danhong [1 ,2 ]
Kolawole, Sharafadeen Kunle [3 ]
Su, Xuping [1 ,2 ]
机构
[1] Changzhou Univ, Sch Mat Sci & Engn, Changzhou 213164, Peoples R China
[2] Changzhou Univ, Jiangsu Key Lab Mat Surface Sci & Technol, Changzhou 213164, Peoples R China
[3] Fed Polytech, Sch Engn & Technol, Mech Engn Dept, PMB 420, Offa, Nigeria
来源
基金
美国国家科学基金会;
关键词
Fe-Ni-Cr-Al-Si alloys; FCC; Pre-oxidation; Diffusion; Activity; HIGH-TEMPERATURE OXIDATION; MODEL ALLOYS; AL; CORROSION; SI;
D O I
10.1016/j.mtcomm.2022.105167
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of Si on the high temperature oxidation of Fe-10Ni-10Cr-4Al-xSi (x = 0, 1, 2, 3 wt%) austenitic alloys were examined at 1000 & DEG;C by pre-oxidation under low oxygen pressure. The results showed that when Fe-10Ni-10Cr-4Al-xSi alloys were oxidized at 1000 & DEG;C under oxygen pressure of 10-20 atm for 5 h, without Si element, the oxidation products formed were continuous outer M2O3 (M: Al and Cr) scale and a small amount of inner dendritic Al2O3. When Si was added, inner Al2O3 increased obviously and SiO2 formed between M2O3 and Al2O3, and Cr2O3 decreased and Al2O3 increased in the external M2O3 oxide layer. When 3 wt% Si was added, the oxide was only external Al2O3 scale. The oxidation resistance of the alloys was improved with an increase in the Si content. Only external Al2O3 scale on Fe-10Ni-10Cr-4Al-2Si alloy pre-oxidized at 1000 & DEG;C for 5 h under low oxygen pressure of 10-30 atm. The addition of Si promoted the diffusion coefficient and activity of Al, increased the driving force of Al2O3 formation and reduced the critical concentration for the transition from internal oxidation to external oxidation of Al2O3.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Effect of Low-Temperature Severe Plastic Deformation on the Saturation Magnetization and the Crystal Geometry Characteristics of the Phases in a Metastable Fe–18Cr–10Ni Alloy
    E. N. Blinova
    A. M. Glezer
    M. G. Isaenkova
    O. A. Krymskaya
    M. A. Libman
    N. S. Perov
    A. A. Tomchuk
    N. A. Shurygina
    Russian Metallurgy (Metally), 2023, 2023 : 1462 - 1466
  • [32] Effect of Initial Grain Size on Deformation Mechanism during High-Pressure Torsion in V10Cr15Mn5Fe35Co10Ni25 High-Entropy Alloy
    Asghari-Rad, Peyman
    Sathiyamoorthi, Praveen
    Bae, Jae Wung
    Shahmir, Hamed
    Zargaran, Alireza
    Kim, Hyoung Seop
    ADVANCED ENGINEERING MATERIALS, 2020, 22 (01)
  • [33] Influence of Annealing Microstructure on the Low-cycle Fatigue Properties and Fatigue Microstructure of a Fe-15Mn-10Cr-8Ni-4Si Seismic Damping Alloy
    Nikulin, Ilya
    Sawaguchi, Takahiro
    Yoshinaka, Fumiyoshi
    Takamori, Susumu
    Kimura, Yuuji
    ISIJ INTERNATIONAL, 2022, 62 (02) : 389 - 398
  • [34] Effect of sulfur and oxygen on engulfment and pushing of deoxidation particles of ZrO2 and Al2O3 during solidification of Fe-10mass%Ni alloy
    Ohta, H
    Suito, H
    ISIJ INTERNATIONAL, 2006, 46 (04) : 472 - 479
  • [35] Effect of dissolved oxygen and coupled resistance on the galvanic corrosion of Cr-Ni low-alloy steel/90-10 cupronickel under simulated deep sea condition
    Xing, S. H.
    Li, Y.
    Wharton, J. A.
    Fan, W. J.
    Liu, G. Y.
    Zhang, F.
    Zhao, X. D.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2017, 68 (10): : 1123 - 1128
  • [36] Effects of Ti and Nb Additions on Microstructure and Shape Memory Effect of Fe-10Mn-6Si-4Ni-7Cr-0.3C Shape Memory Alloy
    Abbas, Aqeel
    Hsu, Jung-Wei
    Naqvi, Syed Murawat Abbas
    Lin, Hsin-Chih
    Lin, Kun-Ming
    JOM, 2024, 76 (11) : 6680 - 6691
  • [37] Effect of Strain Rate on the Extremely Low-Cycle Fatigue of Fe-15Mn-10Cr-8Ni-4Si Bidirectional-TRIP Steel
    Yoshinaka F.
    Nagashima N.
    Sawaguchi T.
    Zairyo/Journal of the Society of Materials Science, Japan, 2023, 72 (12) : 858 - 865
  • [38] Effect of nano-scale martensite and β phase on the passive film formation and electrochemical behaviour of Ti-10V-2Fe-3Al alloy in 3.5% NaCl solution
    Tang, Jun
    Luo, Hongyun
    Qi, Yameng
    Xu, Pingwei
    Lv, Jinlong
    Ma, Yue
    Zhang, Zheng
    ELECTROCHIMICA ACTA, 2018, 283 : 1300 - 1312
  • [39] Strengthening and Toughening Mechanisms of Precipitation- Hardened Fe53Mn15Ni15Cr10Al4Ti2C1 High-Entropy Alloy
    Sun, Shijie
    Tian, Yanzhong
    Zhang, Zhefeng
    Jinshu Xuebao/Acta Metallurgica Sinica, 2022, 58 (01): : 54 - 66
  • [40] Strengthening and Toughening Mechanisms of Precipitation-Hardened Fe53Mn15Ni15Cr10Al4Ti2C1 High-Entropy Alloy
    Sun Shijie
    Tian Yanzhong
    Zhang Zhefeng
    ACTA METALLURGICA SINICA, 2022, 58 (01) : 54 - 66