Effect of high-temperature thermo-oxidation on the mechanical and electrical properties of phenylethynyl-terminated polyimide/carbon fiber composite

被引:4
|
作者
Wang, Hao [1 ,2 ]
Wang, Ziqiao [3 ]
Kuang, Naihang [3 ]
Wu, Chao [1 ]
Lu, Yu [1 ,2 ]
Zhang, Chunhua [1 ,2 ]
机构
[1] Harbin Inst Technol, Sch Chem & Chem Engn, POB 1254, Harbin 150001, Peoples R China
[2] Harbin Inst Technol, Sch Chem & Chem Engn, MIIT Key Lab Crit Mat Technol New Energy Convers &, POB 1254, Harbin 150001, Peoples R China
[3] Harbin FRP Inst Co Ltd, Harbin 150000, Peoples R China
基金
中国国家自然科学基金;
关键词
Phenylethynyl-terminated polyimide; Carbon fiber reinforced composite; Thermal stability; Mechanical properties; Electrical properties; IMIDE OLIGOMERS; GRAPHENE OXIDE; THERMAL-DEGRADATION; CARBON; RESISTANCE; CONDUCTIVITY; DIANHYDRIDE; POLYANILINE; CURE; OLIGOIMIDES;
D O I
10.1016/j.polymdegradstab.2023.110544
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The thermal degradation behaviors of phenylethynyl-terminated polyimide and their carbon fiber reinforced composites (CFRC) are significant to be evaluated comprehensively as their high-temperature applications are gradually expanded. It is found that ether-containing thermoset polyimide (PI) film shows unique degradation behaviors near glass transition temperature (Tg). Though the triethylamine (Et3N) chemical imidization method is applied, the PI backbone shows thermal stability at 371 degrees C thermo-oxidation condition and the main degradation parts site at the curing structure. More aliphatic (C-C) linkages will be formed in the thermo-oxidation process and they are ascribed to the further crosslinking behaviors of polyene structure. However, the PI film shows stable mechanical properties after thermo-oxidation. Meanwhile, the formation of an amorphous carbon structure is found after thermo-oxidation treatment, which endows the composite with enhanced electrical properties. Though the micro-cracking phenomenon happens at the matrix/CF interface of composite surface and thus degrades its mechanical properties, the in-plane longitudinal and transverse conductivity of the composite perform an increase, factors of 1.13 to 2.56x104 S/m and 2.28 to 454.8 S/m, respectively. Mechanism study indicates that the formation of amorphous carbon components is caused by the structural rearrangement of the degrading polyene curing structure and becomes more in the thermo-oxidation process, not affecting the backbone integrity and mechanical stability of the PI matrix. As a result, thermo-oxidation treatment degrades the mechanical properties of the composite, whereas the formed amorphous carbon component acts as a self-growing carbon-based nano-filling structure at the PI/CF interface and enhances the electrical contact of the carbon fibers.
引用
收藏
页数:16
相关论文
共 50 条
  • [41] High-temperature mechanical properties and deformation behavior of carbides reinforced TiNbTaZrHf composite
    Li, Xiaofeng
    Fu, Ao
    Cao, Yuankui
    Xu, Shenghang
    Gao, Shenghan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 894
  • [42] Effect of Temperature and Time on Mechanical and Electrical Properties of HDPE/Glass Fiber Composites
    Alkan, U.
    Ozcanli, Y.
    Alekberov, V.
    FIBERS AND POLYMERS, 2013, 14 (01) : 115 - 120
  • [43] Effect of temperature and time on mechanical and electrical properties of HDPE/glass fiber composites
    U. Alkan
    Y. Özcanlı
    V. Alekberov
    Fibers and Polymers, 2013, 14 : 115 - 120
  • [44] Mechanical properties of ALON-based composite ceramics at high temperature (part 1) - Effect of oxidation on mechanical properties of ALON-BN composite ceramics
    Shimpo, A
    Ueki, M
    Naka, M
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2001, 109 (02) : 127 - 131
  • [45] Mechanical and thermal properties of carbon fiber epoxy composite with interlaminar graphene at elevated temperature
    Mulqueen, Daniel W.
    Sattar, Siavash
    Kravchenko, Oleksandr G.
    COMPOSITES PART B-ENGINEERING, 2023, 255
  • [46] Effect of Y Content on Precipitation Behavior, Oxidation and Mechanical Properties of As-Cast High-Temperature Titanium Alloys
    Shen, Jiafeng
    Fu, Binguo
    Wang, Yufeng
    Dong, Tianshun
    Li, Jingkun
    Li, Guolu
    Liu, Jinhai
    MATERIALS, 2023, 16 (13)
  • [47] Electrical resistivity measurement of carbon-fiber-reinforced ceramic matrix composite under thermo-mechanical load
    Boehrk, Hannah
    Leschinski, Peter
    Reimer, Thomas
    COMPOSITES SCIENCE AND TECHNOLOGY, 2013, 76 : 1 - 7
  • [48] Fabrication of thermally robust carbon nanotube (CNT)/SiO2 composite films and their high-temperature mechanical properties
    He, Jingyu
    Chen, Jingfu
    Shi, Liyi
    Li, Qingwen
    Lu, Weibang
    Qu, Shuxuan
    Qiu, Wenfeng
    Zhou, Gengheng
    CARBON, 2019, 147 : 236 - 241
  • [49] Effect of fiber length on the mechanical properties of high dosage carbon reinforced
    Capela, C.
    Oliveira, S. E.
    Pestana, J.
    Ferreira, J. A. M.
    2ND INTERNATIONAL CONFERENCE ON STRUCTURAL INTEGRITY, ICSI 2017, 2017, 5 : 539 - 546
  • [50] High-temperature mechanical properties of Nextel™ 610 fiber reinforced silica matrix composites
    Jiang, Ru
    Yang, Lingwei
    Liu, Haitao
    Sun, Xun
    Cheng, Haifeng
    CERAMICS INTERNATIONAL, 2018, 44 (13) : 15356 - 15361