High-strength Mg-10Gd-3Y-1Zn-0.5Zr alloy fabricated by wire-arc directed energy deposition: Phase transformation behavior and mechanical properties

被引:27
作者
Cao, Qianhui [1 ]
Zeng, Caiyou [1 ]
Cai, Xinyi [1 ]
Zhang, Ruize [2 ]
Wang, Fude [2 ]
Wang, Haibo [3 ]
Zhang, Yu [4 ]
Qi, Bojin [1 ]
Cong, Baoqiang [1 ]
机构
[1] Beihang Univ, Sch Mech Engn & Automat, Beijing 100191, Peoples R China
[2] Capital Aerosp Machinery Co Ltd, Beijing 100076, Peoples R China
[3] North China Univ Technol, Sch Mech & Mat Engn, Beijing 100144, Peoples R China
[4] Beijing Univ Technol, Fac Mat & Mfg, Dept Mat Sci & Engn, Beijing 100124, Peoples R China
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
Magnesium rare-earth (Mg-RE) alloys; Wire-arc directed energy deposition (WA-DED); Microstructural evolution; Long period stacking ordered (LPSO) phase; Mechanical properties; MG-GD; MICROSTRUCTURE EVOLUTION; MAGNESIUM ALLOYS; WT.PERCENT ALLOY; BUILDING-BLOCK; ZR ALLOYS; AS-CAST; PRECIPITATION; COMPRESSION;
D O I
10.1016/j.addma.2023.103789
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Magnesium rare-earth (Mg-RE) alloys have great potential in lightweight applications because of the high specific strength. Wire-arc directed energy deposition (WA-DED) exhibits great prospects for the fabrication of largescale monolithic structural components with high manufacturing flexibility. In this work, a single-pass multilayer Mg-10Gd-3Y-1Zn-0.5Zr (wt%, GWZ1031K) deposit was prepared via WA-DED. Electron backscatter diffraction (EBSD), scanning electron microscopy (SEM), and transmission electron microscopy (TEM) are conducted to systematically explore the microstructural evolution during the WA-DED process and the subsequent heat treatment. The GWZ1031K alloy deposit fabricated by WA-DED exhibits uniform equiaxed grain structure whose average grain size is 22.3 +/- 5.6 mu m. The (Mg,Zn)(3)(Gd,Y) phase and RE segregation can be observed along the alpha-Mg grain boundaries (GBs). A number of needle-like gamma'/gamma '' phases embedded in the alpha-Mg grain interior (GI). In addition, there is a small number of fine RE-rich cubic phase and (Gd,Y)(2)O-3 particles. The deposit shows significantly enhanced ductility and slightly improved strength after solution treated at 500 degrees C for 12 h. After the solution treatment, the intergranular (Mg,Zn)(3)(Gd,Y) eutectics dissolve into the matrix and long period stacking ordered (LPSO) phases precipitate from the GBs into the GI, contributing to the enhancement in ductility. Besides, the LPSO phase along with the existing RE-rich cubic phase, (Gd,Y)(2)O-3 and Zr particles at GBs also play a role in hindering grain growth. The high-density nanoscale beta' phases appear in the GI after aging treated at 200 degrees C for 24 h, resulting in the remarkable precipitation strengthening. In comparison with the solution-treated GWZ1031K deposit, the aging-treated exhibits a prominently improved ultimate tensile strength of 337 +/- 7 MPa in the building direction (BD) and 331 +/- 5 MPa in the travelling direction (TD). It is envisaged that the WADED manufacturing method will provide a simple and effective route to fabricate large-scale Mg-RE alloy components for various applications.
引用
收藏
页数:18
相关论文
共 63 条
  • [1] Effects of additive manufacturing processes and isothermal aging on the microstructure and properties of 13-8 Mo precipitation hardening martensitic stainless steel
    Benoit, M. J.
    Tabaie, S.
    Waqar, T.
    Ganton, T.
    Amirkhiz, B. S.
    Hadadzadeh, A.
    Nasiri, A.
    [J]. ADDITIVE MANUFACTURING, 2023, 72
  • [2] Microstructure and mechanical properties of AZ91 Mg alloy fabricated by cold metal transfer additive manufacturing
    Bi, Ji
    Shen, Junqi
    Hu, Shengsun
    Zhen, Yahui
    Yin, Fengliang
    Bu, Xianzheng
    [J]. MATERIALS LETTERS, 2020, 276 (276)
  • [3] Design of an additively manufactured functionally graded material of 316 stainless steel and Ti-6Al-4V with Ni-20Cr, Cr, and V intermediate compositions
    Bobbio, Lourdes D.
    Bocklund, Brandon
    Simsek, Emrah
    Ott, Ryan T.
    Kramer, Matt J.
    Liu, Zi-Kui
    Beese, Allison M.
    [J]. ADDITIVE MANUFACTURING, 2022, 51
  • [4] Cai X., 2022, J. Magnes. Alloy.
  • [5] Excellent isotropic mechanical properties of directed energy deposited Mg-Gd-Y-Zr alloys via establishing homogeneous equiaxed grains embedded with dispersed nano-precipitation
    Cao, Qianhui
    Zeng, Caiyou
    Qi, Bojin
    Jiang, Zihao
    Zhang, Ruize
    Wang, Fude
    Cong, Baoqiang
    [J]. ADDITIVE MANUFACTURING, 2023, 67
  • [6] Microstructure evolution and mechanical properties of a high-strength Mg-10Gd-3Y-1Zn-0.4Zr alloy fabricated by laser powder bed fusion
    Deng, Qingchen
    Wu, Yujuan
    Wu, Qianye
    Xue, Yanting
    Zhang, Yu
    Peng, Liming
    Ding, Wenjiang
    [J]. ADDITIVE MANUFACTURING, 2022, 49
  • [7] Fabrication of high-strength Mg-Gd-Zn-Zr alloy via selective laser melting
    Deng, Qingchen
    Wu, Yujuan
    Luo, Yuanhang
    Su, Ning
    Xue, Xiaoyu
    Chang, Zhiyu
    Wu, Qianye
    Xue, Yanting
    Peng, Liming
    [J]. MATERIALS CHARACTERIZATION, 2020, 165
  • [8] Additive manufacturing of high performance AZ31 magnesium alloy with full equiaxed grains: Microstructure, mechanical property, and electromechanical corrosion performance
    Fang, Xuewei
    Yang, Jiannan
    Wang, Shuaipeng
    Wang, Chuanbin
    Huang, Ke
    Li, Haonan
    Lu, Bingheng
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2022, 300
  • [9] Microstructure and mechanical behavior of an additive manufactured (AM) WE43-Mg alloy
    Gangireddy, Sindhura
    Gwalani, Bharat
    Liu, Kaimiao
    Faierson, Eric J.
    Mishra, Rajiv S.
    [J]. ADDITIVE MANUFACTURING, 2019, 26 : 53 - 64
  • [10] Effects of rare-earth elements Gd and Y on the solid solution strengthening of Mg alloys
    Gao, L.
    Chen, R. S.
    Han, E. H.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 481 (1-2) : 379 - 384