Ash deposition and corrosion mechanisms of tubes in Waste-to-Energy plants

被引:0
作者
Naganuma, Hiroshi [1 ]
Mori, Takehito [1 ]
Watanabe, Sho [1 ]
Sawada, Akihiro [1 ]
Goto, Taeko [1 ]
Ueki, Yasuaki [2 ]
Yoshiie, Ryo [2 ]
Naruse, Ichiro [2 ]
机构
[1] Tohoku Elect Power Engn & Construct Co Inc, 53 Shinnakahori, Sendai, Miyagi 9810113, Japan
[2] Nagoya Univ, Furo cho,Chikusa ku, Nagoya, Aichi 4648603, Japan
来源
MECHANICAL ENGINEERING JOURNAL | 2024年 / 11卷 / 02期
关键词
Waste-to-Energy; Ash deposition; Hot corrosion; Adhesion force; Surface treatment technique; Accelerated oxidation;
D O I
10.1299/mej.23-00486
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In order to decrease ash deposition and hot corrosion in Waste-to-Energy plants, it is necessary to understand mechanisms of the ash deposition and the corrosion, and to develop new solutions. In this study, an adhesion force between an ash pellet and an alloy specimen were firstly measured to investigate the increase mechanisms of the ash deposition and the corrosion, using a tensile testing machine with an electrical furnace. Second, mass loss of the alloy specimens was measured as hot corrosion tests based on Japanese Industrial Standards. Third, phenomenon on the interface was evaluated with production amount of molten salts which were calculated by thermodynamic equilibrium. As a result, the adhesion force and the mass loss of all specimens increased with the interface temperature, and there was exact materials dependency, which indicated that a high chromium content design to improve corrosion resistance was valid also for decrease of the ash adhesion. Moreover, it was observed that mass loss of the alloy specimens with the ash sample collected from an actual boiler had a temperature dependence, and molten salts and accelerated oxidation induced by chlorides attacked the alloy specimens. In addition, generation of HCl gas and molten salts with temperature increase was confirmed with the thermodynamic equilibrium calculations. Judging from these results, starting temperature of the adhesion could be correspond to one which the alloy started to be severely corroded.
引用
收藏
页数:6
相关论文
共 6 条
[1]   An Overview on Corrosion-Resistant Coating Technologies in Biomass/Waste-to-Energy Plants in Recent Decades [J].
Kawahara, Yuuzou .
COATINGS, 2016, 6 (03)
[2]   Ash deposition mechanisms in Waste-to-Energy plants [J].
Naganuma, Hiroshi ;
Mori, Takehito ;
Watanabe, Sho ;
Sawada, Akihiro ;
Goto, Taeko ;
Ueki, Yasuaki ;
Yoshiie, Ryo ;
Naruse, Ichiro .
MECHANICAL ENGINEERING JOURNAL, 2022, 9 (04)
[3]   Reduction mechanisms of ash deposition in coal and/or biomass combustion boilers [J].
Naganuma, Hiroshi ;
Ikeda, Nobuya ;
Ito, Tadashi ;
Matsuura, Mikio ;
Nunome, Yoko ;
Ueki, Yasuaki ;
Yoshiie, Ryo ;
Naruse, Ichiro .
FUEL, 2013, 106 :303-309
[4]   The implications of chlorine-associated corrosion on the operation of biomass-fired boilers [J].
Nielsen, HP ;
Frandsen, FJ ;
Dam-Johansen, K ;
Baxter, LL .
PROGRESS IN ENERGY AND COMBUSTION SCIENCE, 2000, 26 (03) :283-298
[5]   High temperature corrosion mechanism of type 304 stainless steel embedded in corrosion ash [J].
Nishikata, A ;
Shibahashi, T ;
Tsuru, T ;
Kobayashi, S ;
Urabe, T .
JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1999, 63 (07) :844-850
[6]  
Shino Y., 2016, ZAIRYO TO KANKYO, V65, P454