Effects of W alloying and heating on microstructure and mechanical properties of a PM Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy for high temperature applications

被引:7
|
作者
Wu, Xiaogang [1 ]
Zhang, Bowen [1 ]
Zhang, Yanhu [1 ]
Niu, Hongzhi [1 ]
Zhang, Deliang [1 ,2 ]
机构
[1] Northeastern Univ, Sch Mat Sci & Engn, Shenyang 110819, Peoples R China
[2] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Peoples R China
基金
中国国家自然科学基金;
关键词
Powder metallurgy titanium alloys; W stabilization; Microstructural evolution; Effect of heating; Mechanical properties; SHORT-RANGE ORDER; ALPHA(2) PRECIPITATION; TENSILE PROPERTIES; ROOM-TEMPERATURE; TITANIUM; BEHAVIOR; PHASE; STABILITY; EXPOSURE; BETA;
D O I
10.1016/j.jallcom.2023.168966
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Powder metallurgy (PM) Ti-6Al-2Sn-4Zr-2Mo-0.1Si-(0, 2, 4)W (wt%) alloys were fabricated by thermo-mechanical consolidation of TiH2-based powder compacts and subsequent heat treatments. Samples of the as-fabricated alloys were also heated at 650 degrees C for 200 h. The addition of 2 or 4 wt%W to the base alloy changed its microstructure of parallel alpha/beta lamellar colonies and grain boundary alpha (alpha GB) to an interwoven alpha/beta t microstructure consisting of alpha GB and a network of interpenetrating alpha plates with beta transformed structure (beta t) domains comprising variants of fine alpha laths and beta matrix. The partition of the beta stabilizing W between beta and alpha phases and the low diffusivity of W atoms limited the growth of alpha plates/laths, decreasing the thickness of alpha plates/laths and increasing the volume fraction of beta. The increased hardening of the beta phase and enhanced alpha/beta interface strengthening associated with the 4 wt%W addition led to a significant increase in the tensile strength of the alloy from 1281 +/- 10-1411 +/- 12 MPa. However, the high flow stress and the very fine microstructure caused significant strain localization in the weak alpha GB, resulting in premature fracture of the alpha GB (intergranular fracture) and the low ductility (1.4%). Here, premature fracture meant the fracture occurred prior to the alloy reaching its ultimate tensile strength. The heating caused the beta interlaths in the W-free alloy to partially dissolve and become beta particles distributed along the original lines of beta interlaths accompanied by the precipitation of alpha 2-Ti3Al in the alpha plates. The addition of W inhibited the dissolution of beta interlaths and caused the precipitation of a higher volume fraction of alpha 2 precipitates during heating. The microstructural changes caused by heating resulted in a slight decrease in strength and a significant decrease in ductility for the W-free alloy, but a significant increase of the yield strength of the 2 W and 4 W alloys with some sacrifice of the tensile ductility. The microstructural reasons for the effects on mechanical properties were analyzed with the assistance of detailed characterization of the dislocations in the deformed specimens.(c) 2023 Elsevier B.V. All rights reserved.
引用
收藏
页数:17
相关论文
共 50 条
  • [31] High temperature creep behavior of an as-cast near-α Ti-6Al-4Sn-4Zr-0.8Mo-1Nb-1W-0.25Si alloy
    Zheng, Zhuangzhuang
    Xiao, Shulong
    Wang, Xiaosong
    Guo, Yingfei
    Yang, Jianhui
    Xu, Lijuan
    Chen, Yuyong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 803
  • [32] Effect of deformation temperature on the microstructure and texture evolution of Ti-6Al-4Zr-2Mo-6V alloy
    Sun, Kuishan
    Xu, Lingyu
    Song, Dejun
    Yan, Yangyang
    Li, Longteng
    Wu, Yukun
    Wang, Yang
    Liao, Zhiqian
    Zhang, Hao
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2024, 42 (06):
  • [33] Influence of heat treatments on microstructure and mechanical properties of laser additive manufacturing Ti-5Al-2Sn-2Zr-4Mo-4Cr titanium alloy
    Zhu, Yan-yan
    Chen, Bo
    Tang, Hai-bo
    Cheng, Xu
    Wang, Hua-ming
    Li, Jia
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2018, 28 (01) : 36 - 46
  • [34] Influence of alpha-case layer on the low cycle fatigue properties of Ti-6Al-2Sn-4Zr-2Mo alloy
    Gaddam, R.
    Antti, M-L.
    Pederson, R.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 599 : 51 - 56
  • [35] Microstructure and mechanical properties of heat-treated Ti-5Al-2Sn-2Zr-4Mo-4Cr
    Li, Hui-min
    Li, Miao-quan
    Luo, Jiao
    Wang, Ke
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (09) : 2893 - 2900
  • [36] Effects of microstructure characteristics on the mechanical properties and elastic modulus of a new Ti-6Al-2Nb-2Zr-0.4B alloy
    Yang, Zhijun
    Cao, Junhui
    Yu, Weixin
    Hou, Shusen
    Wang, Guanglong
    Lang, Shaoting
    Ding, Peng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 820
  • [37] Anisotropy in the tensile behaviour of Ti-6Al-2Sn-4Zr-6Mo alloy
    Corzo, M
    Manero, JM
    Anglada, M
    Mateo, A
    REVISTA DE METALURGIA, 2005, : 401 - 406
  • [38] Effect of heat input on microstructure and tensile properties of laser welded Ti-3Al-6Mo-2Fe-2Zr alloy joint
    Zhang, Kezhao
    He, Chaowei
    Liu, Dong
    Yan, Chunyan
    Niu, HongZhi
    Yang, Zhibin
    Bao, Yefeng
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 17 : 1652 - 1661
  • [39] Quantitative analysis on microstructure evolution of Ti-6Al-2Zr-2Sn-2Mo-1.5Cr-2Nb alloy during isothermal compression
    Gao, Jun
    Li, Miao-Quan
    Li, Xiao-Di
    Zhang, Dong
    Xue, Jian-Rui
    Jiang, Xue-Qi
    Zhang, Chao-Yue
    Liu, Lu-Yang
    RARE METALS, 2015, 34 (09) : 625 - 631
  • [40] Effects of the cooling rate on mechanical properties and microstructure of near-α Ti-6Al-3Zr-2Nb-Mo alloy
    Jiang, Haiyang
    Jiang, Fuqing
    Xie, Bijun
    Wang, Bing
    Xu, Bin
    Hu, Xu
    Xu, Liang
    He, Zhangxun
    Zhang, Hao
    Wu, Yuxi
    Sun, Mingyue
    MATERIALS CHARACTERIZATION, 2023, 195