Effects of W alloying and heating on microstructure and mechanical properties of a PM Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy for high temperature applications

被引:7
|
作者
Wu, Xiaogang [1 ]
Zhang, Bowen [1 ]
Zhang, Yanhu [1 ]
Niu, Hongzhi [1 ]
Zhang, Deliang [1 ,2 ]
机构
[1] Northeastern Univ, Sch Mat Sci & Engn, Shenyang 110819, Peoples R China
[2] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Peoples R China
基金
中国国家自然科学基金;
关键词
Powder metallurgy titanium alloys; W stabilization; Microstructural evolution; Effect of heating; Mechanical properties; SHORT-RANGE ORDER; ALPHA(2) PRECIPITATION; TENSILE PROPERTIES; ROOM-TEMPERATURE; TITANIUM; BEHAVIOR; PHASE; STABILITY; EXPOSURE; BETA;
D O I
10.1016/j.jallcom.2023.168966
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Powder metallurgy (PM) Ti-6Al-2Sn-4Zr-2Mo-0.1Si-(0, 2, 4)W (wt%) alloys were fabricated by thermo-mechanical consolidation of TiH2-based powder compacts and subsequent heat treatments. Samples of the as-fabricated alloys were also heated at 650 degrees C for 200 h. The addition of 2 or 4 wt%W to the base alloy changed its microstructure of parallel alpha/beta lamellar colonies and grain boundary alpha (alpha GB) to an interwoven alpha/beta t microstructure consisting of alpha GB and a network of interpenetrating alpha plates with beta transformed structure (beta t) domains comprising variants of fine alpha laths and beta matrix. The partition of the beta stabilizing W between beta and alpha phases and the low diffusivity of W atoms limited the growth of alpha plates/laths, decreasing the thickness of alpha plates/laths and increasing the volume fraction of beta. The increased hardening of the beta phase and enhanced alpha/beta interface strengthening associated with the 4 wt%W addition led to a significant increase in the tensile strength of the alloy from 1281 +/- 10-1411 +/- 12 MPa. However, the high flow stress and the very fine microstructure caused significant strain localization in the weak alpha GB, resulting in premature fracture of the alpha GB (intergranular fracture) and the low ductility (1.4%). Here, premature fracture meant the fracture occurred prior to the alloy reaching its ultimate tensile strength. The heating caused the beta interlaths in the W-free alloy to partially dissolve and become beta particles distributed along the original lines of beta interlaths accompanied by the precipitation of alpha 2-Ti3Al in the alpha plates. The addition of W inhibited the dissolution of beta interlaths and caused the precipitation of a higher volume fraction of alpha 2 precipitates during heating. The microstructural changes caused by heating resulted in a slight decrease in strength and a significant decrease in ductility for the W-free alloy, but a significant increase of the yield strength of the 2 W and 4 W alloys with some sacrifice of the tensile ductility. The microstructural reasons for the effects on mechanical properties were analyzed with the assistance of detailed characterization of the dislocations in the deformed specimens.(c) 2023 Elsevier B.V. All rights reserved.
引用
收藏
页数:17
相关论文
共 50 条
  • [1] Joining of Dissimilar Alloys Ti-6Al-4V and Ti-6Al-2Sn-4Zr-2Mo-0.1Si Using Linear Friction Welding
    Rajan, Sidharth
    Wanjara, Priti
    Gholipour, Javad
    Kabir, Abu Syed
    MATERIALS, 2020, 13 (17)
  • [2] Coarsening Behavior and Plastic Flow of Ti-6Al-2Sn-4Zr-2Mo-0.1Si with an Ultrafine Microstructure
    Semiatin, S. L.
    Sun, F.
    Crist, E. M.
    Yu, K. O.
    Sargent, G. A.
    Sanders, D. G.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2016, 47A (09): : 4374 - 4377
  • [3] Achieving synergy enhancement of strength and ductility in Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy by fabricating a new multiscale microstructure
    Zhou, Yu
    Wang, Ke
    Wen, Xin
    Xin, Renlong
    Wang, Jingfeng
    Liu, Qing
    SCRIPTA MATERIALIA, 2023, 226
  • [4] Correlation between microstructures and tensile deformation behavior of a PM near α Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy
    Wu, Xiaogang
    Zhang, Bowen
    Zhang, Youyun
    Niu, Hongzhi
    Zhang, Deliang
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 825
  • [5] Microstructure, Tensile Properties, and Fatigue Behavior of Linear Friction-Welded Ti-6Al-2Sn-4Zr-2Mo-0.1Si
    Rajan, Sidharth
    Wanjara, Priti
    Gholipour, Javad
    Kabir, Abu Syed
    MATERIALS, 2021, 14 (01) : 1 - 21
  • [6] Strength and fatigue strength of a similar Ti-6Al-2Sn-4Zr-2Mo-0.1Si linear friction welded joint
    Garcia, Juan Manuel
    Morgeneyer, Thilo F.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2019, 42 (05) : 1100 - 1117
  • [7] α ⇆ β changes in Ti-6Al-2Sn-4Zr-2Mo-Si alloy:: characterization, microstructure, and mechanical properties
    Tarin, P.
    Rodriguez, M. C.
    Simon, A. G.
    Piris, N. M.
    Badia, J. M.
    Antoranz, J. M.
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART G-JOURNAL OF AEROSPACE ENGINEERING, 2006, 220 (G3) : 241 - 246
  • [8] Fatigue Behavior of Linear Friction Welded Ti-6Al-4V and Ti-6Al-2Sn-4Zr-2Mo-0.1Si Dissimilar Welds
    Rajan, Sidharth
    Wanjara, Priti
    Gholipour, Javad
    Kabir, Abu Syed
    MATERIALS, 2021, 14 (11)
  • [9] Effect of Microstructures on Mechanical Properties of Ti-6.5Al-2Sn-4Zr-4Mo-1W-0.2Si Alloy
    Zhou, Gang
    Xin, Shewei
    Xing, Hui
    Zhang, Kai
    Zhang, Siyuan
    Liu, Zhibo
    Zhang, Jiahao
    Huang, Jian
    Yang, Yi
    Wang, Hao
    Huang, Aijun
    ADVANCED ENGINEERING MATERIALS, 2023, 25 (12)
  • [10] Comparison of Microstructure Refinement in Wire-Arc Additively Manufactured Ti-6Al-2Sn-4Zr-2Mo-0.1Si and Ti-6Al-4V Built With Inter-Pass Deformation
    Davis, A. E.
    Caballero, A. E.
    Biswal, R.
    Williams, S.
    Prangnell, P. B.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2022, 53 (11): : 3833 - 3852