Fabrication of a model specimen for understanding micro-galvanic corrosion at the boundary of a-Mg and a-Mg17Al12

被引:17
作者
Shao, Zheng [1 ]
Nishimoto, Masashi [1 ]
Muto, Izumi [1 ]
Sugawara, Yu [1 ]
机构
[1] Tohoku Univ, Grad Sch Engn, Dept Mat Sci, 6-6-02 Aza Aoba, Aramaki, Aoba ku, Sendai 9800579, Japan
关键词
Magnesium alloy; a/ss phase boundary; Micro-scale observation technique; Micro-galvanic corrosion; Spark plasma sintering; SURFACE OXIDE-FILMS; MAGNESIUM ALLOY; MECHANICAL-PROPERTIES; MICROSTRUCTURE EVOLUTION; HEAT-TREATMENT; BEHAVIOR; PHASE; AZ91; RESISTANCE; INTERDIFFUSION;
D O I
10.1016/j.jma.2022.10.020
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
A model specimen with a single boundary of the a/ ss phase simulating Mg-Al alloys was successfully fabricated by spark plasma sintering. A small electrode area of a phase or ss phase was prepared using the model specimen, and the OCPs (open-circuit potentials) of each phase and a small electrode area containing the a/ ss phase boundary in 0.1 M NaCl at pH 8.0 were compared: the ss phase exhibited a higher potential, and the a phase showed a lower potential. The OCP of the small area containing the a/ ss phase boundary was the intermediate value of these phases. In a small area containing a/ ss phase boundary, discoloration and gas bubbles were observed on the a phase, but no bubble generation was detected on the ss phase. The gas bubbles were initially generated on the a phase near the ss phase, but as the discoloration (corrosion) of the a phase approached the ss phase, the bubbles were generated on the ss phase. In micro-galvanic corrosion of the a and ss phases, the ss phase did not always function as the preferred cathode. The a phase partially corroded (or discolored) and became the anodes, so that the surrounding areas were most likely to be the cathodes. When corroded areas (anodes) in the a phase approached the ss phase, the ss phase would become cathodes. In addition to the micro-galvanic corrosion mechanism, the role of Al in corrosion resistance at the a/ ss phase boundary was determined by surface analysis.
引用
收藏
页码:137 / 153
页数:17
相关论文
共 77 条
[11]   Review of Corrosion-Resistant Conversion Coatings for Magnesium and Its Alloys [J].
Chen, X. B. ;
Birbilis, N. ;
Abbott, T. B. .
CORROSION, 2011, 67 (03)
[12]   Influence of second phase on corrosion performance and formation mechanism of PEO coating on AZ91 Mg alloy [J].
Chen, Yan ;
Yang, Yange ;
Zhang, Wei ;
Zhang, Tao ;
Wang, Fuhui .
JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 718 :92-103
[13]   A Microelectrochemical System for In Situ High-Resolution Optical Microscopy: Morphological Characteristics of Pitting at MnS Inclusion in Stainless Steel [J].
Chiba, Aya ;
Muto, Izumi ;
Sugawara, Yu ;
Hara, Nobuyoshi .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2012, 159 (08) :C341-C350
[14]  
Dahle A.K., 2001, Journal of Light Metals, V1, P61, DOI DOI 10.1016/S1471-5317(00)00007-9
[15]   Superhydrophobic composite coating with active corrosion resistance for AZ31B magnesium alloy protection [J].
Ding, Chendi ;
Tai, Yu ;
Wang, Dong ;
Tan, Linghua ;
Fu, Jiajun .
CHEMICAL ENGINEERING JOURNAL, 2019, 357 :518-532
[16]   The effect of powder size on the mechanical and corrosion properties and the ignition temperature of WE43 alloy prepared by spark plasma sintering [J].
Dvorsky, Drahomir ;
Kubasek, Jiri ;
Roudnicka, Michaela ;
Prusa, Filip ;
Necas, David ;
Minarik, Peter ;
Straska, Jitka ;
Vojtech, Dalibor .
JOURNAL OF MAGNESIUM AND ALLOYS, 2021, 9 (04) :1349-1362
[17]   Fundamentals and advances in magnesium alloy corrosion [J].
Esmaily, M. ;
Svensson, J. E. ;
Fajardo, S. ;
Birbilis, N. ;
Frankel, G. S. ;
Virtanen, S. ;
Arrabal, R. ;
Thomas, S. ;
Johansson, L. G. .
PROGRESS IN MATERIALS SCIENCE, 2017, 89 :92-193
[18]   Protective coatings on magnesium and its alloys - a critical review [J].
Gray, JE ;
Luan, B .
JOURNAL OF ALLOYS AND COMPOUNDS, 2002, 336 (1-2) :88-113
[19]   Corrosion product formation during NaCl induced atmospheric corrosion of magnesium alloy AZ91D [J].
Jonsson, Martin ;
Persson, Dan ;
Thierry, Dominique .
CORROSION SCIENCE, 2007, 49 (03) :1540-1558
[20]  
Khan M.I., 2014, J MATER, V2014, P1, DOI [10.1155/2014/657647, DOI 10.1155/2014/657647]