High-temperature optoelectronic transport behavior of n-MoS2 nanosheets/ p-diamond heterojunction

被引:6
作者
Zou, Liangrui [1 ]
Sang, Dandan [1 ,2 ]
Ge, Shunhao [1 ]
Yao, Yu [1 ]
Wang, Guangyu [1 ]
Wang, Xueting [1 ]
Fan, Jianchao [2 ]
Wang, Qinglin [1 ,2 ]
机构
[1] Liaocheng Univ, Sch Phys Sci & Informat Technol, Shandong Key Lab Opt Commun Sci & Technol, Liaocheng 252000, Peoples R China
[2] Shandong Liaocheng Laixin Powder Mat Sci & Technol, Liaocheng 252000, Peoples R China
基金
中国国家自然科学基金;
关键词
n-MoS2 nanosheets/p-diamond heterojunction; Electrical transport behaviour; Photoluminescence; High temperature; MONOLAYER MOS2; ZNO NANORODS; PHOTOLUMINESCENCE; FABRICATION; RESISTANCE; EMISSION; DIODES; FILM; SI;
D O I
10.1016/j.jallcom.2023.172819
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In the past decades, even though the performance of electronic devices based on MoS2 has reached a very high level, the service life, failure rate and stability of the devices often deteriorate with the increase of temperature when they work in high temperature or harsh environment. In this work, n-MoS2 NSs/p-type boron-doped diamond (BDD) film heterojunction was fabricated by sol-gel method to investigate the temperature dependence of the optoelectronic transport behavior of the device, and the electrical properties of the heterojunction device at high temperature (RT-180 degrees C) were tested. The heterojunction presented all rectification characteristics from room temperature to 180 degrees C and exhibited good thermal stability. With the increase in temperature, the rectification ratio reached the maximum at 120 degrees C and turned into backward diodes at 160 degrees C and 180 degrees C. The mechanism of the current and rectification ratio of n-MoS2 NSs/p-BDD heterojunction changing with temperature was mainly attributed to the decrease of tunneling current caused by the shift of Fermi level of the two semiconductors at high temperature. The heterojunction undergoes a transition from tunneling current to thermal excitation current, and the shift of Fermi level to the valence band of n-MoS2 provides support for the transition to reverse diode. In accordance with the carrier transport behavior following ohmic laws, the current conduction of composite tunneling and the space charge limitation under different bias voltages and temperatures were also discussed, which provides theoretical and experimental basis for optimizing the design of new photoelectric devices in the field of high temperature optoelectronics.
引用
收藏
页数:8
相关论文
共 35 条
  • [31] Phase engineering of 1 T-MoS2 on BiVO4 photoanode with p-n Junctions: Establishing high speed charges transport channels for efficient photoelectrochemical water splitting
    Yu, Lianqing
    Xue, Kehui
    Luo, Huihua
    Liu, Chong
    Liu, Heyuan
    Zhu, Haifeng
    Zhang, Yaping
    CHEMICAL ENGINEERING JOURNAL, 2023, 472
  • [32] Effect of the Ar/N2 flow ratio on the microstructure, mechanical properties, and high-temperature steam oxidation behavior of Cr/CrxN coatings for accident-tolerant fuel coatings
    Chen, Qingsong
    Yang, Hongyan
    Wu, Lu
    Wu, Xiaoyong
    Zhu, Changda
    He, Linxin
    Liu, Ning
    Yang, Yuanyou
    Liao, Jiali
    Yang, Jijun
    CORROSION SCIENCE, 2021, 192
  • [33] Investigation of the high-temperature oxidation behavior of Fe-14Cr-9Mn-2.5Ni austenitic stainless steel in N2-21 vol%O2 environment
    Su, Minghua
    Zhao, Jianhua
    Gu, Cheng
    CORROSION SCIENCE, 2023, 220
  • [34] 0D/2D heterojunction constructed by high-dispersity Mo-doped Ni2P nanodots supported on g-C3N4 nanosheets towards enhanced photocatalytic H2 evolution activity
    Li, Chunmei
    Wu, Huihui
    Hong, Shihuan
    Wang, Yun
    Song, Ning
    Han, Zhonghui
    Dong, Hongjun
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2020, 45 (43) : 22556 - 22566
  • [35] High-temperature melt-infiltration preparation and erosion behavior of γ-Y 2 Si 2 O 7 /Y2O3-SiO2-Al2O3 glass coating on porous Si3N4 ceramics
    Fan, Xingyu
    Zhou, Chanchan
    Han, Chengcheng
    Li, Yang
    Zhang, Qiaoqiao
    CERAMICS INTERNATIONAL, 2024, 50 (20) : 39366 - 39373