Plastic wrinkling of thin-walled tubes under axial compression in non-uniform temperature field

被引:1
|
作者
Cui, Xiao-Lei [1 ]
Guo, Ju [2 ]
Wen, Shi-Yu [1 ]
Wu, Xiu-Min [2 ]
Lin, Peng [2 ]
机构
[1] Harbin Inst Technol, Natl Key Lab Precis Hot Proc Met, Harbin 150001, Heilongjiang, Peoples R China
[2] Taiyuan Univ Technol, Coll Mat Sci & Engn, Taiyuan, Peoples R China
基金
中国国家自然科学基金; 中国博士后科学基金;
关键词
Wrinkling behavior; tube; induction heating; non-uniform temperature field; axial compression; ALUMINUM-ALLOY TUBES; METAL BELLOWS; BEHAVIOR; COMPONENT;
D O I
10.1177/09544062221121987
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The main purpose of this paper is to reveal the wrinkling behavior of thin-walled tubes under axial compression in a non-uniform temperature field formed by induction heating on a local position. The distribution of non-uniform temperature fields induced by induction heating and the wrinkling behavior of tubes under axial compression were studied by combining experiments and simulations. Moreover, the thickness and hardness distribution of the wrinkled tube were analyzed. The results show that the maximum temperature difference along axial direction of 5052 aluminum alloy and AZ31B magnesium alloy tubes can reach 129.1 degrees C and 134.7 degrees C in experiments, respectively. In the non-uniform temperature field with a maximum temperature of 250 degrees C, axisymmetric wrinkles can be formed under axial compression on the tubes. With the increase of axial compression, the wrinkle width gradually decreases and its height gradually increases. The contour shape of wrinkles can be fitted accurately with GaussAmp function. There is an obvious thickening phenomenon on the wrinkles and the thickest point is located on the wrinkle top, where the thickness gradually increases with increasing the axial compression. In addition, the microhardness at the wrinkles is lower than that of the original tubes. It decreases with the increase in axial compression. The maximum reduction of microhardness of 5052 aluminum alloy and AZ31B magnesium alloy tubes at the wrinkles are 41.6% and 17%, respectively. This study not only can provide tube blank with useful wrinkles for hydroforming, but also can provide experimental data for establishing buckling theory of inhomogeneous tube shells.
引用
收藏
页码:406 / 419
页数:14
相关论文
共 50 条
  • [42] ELASTIC AND ELASTO-PLASTIC BUCKLING OF THIN-WALLED COLUMNS SUBJECTED TO UNIFORM COMPRESSION
    GRADZKI, R
    KOWALMICHALSKA, K
    THIN-WALLED STRUCTURES, 1985, 3 (02) : 93 - 108
  • [43] Wrinkling of circular tubes under axial compression: Effect of anisotropy
    Kyriakides, S., 1600, American Society of Mechanical Engineers (72):
  • [44] Wrinkling of circular tubes under axial compression: Effect of anisotropy
    Kyriakides, S
    Bardi, FC
    Paquette, JA
    JOURNAL OF APPLIED MECHANICS-TRANSACTIONS OF THE ASME, 2005, 72 (02): : 301 - 305
  • [45] Warm Hydroforming Process under Non-Uniform Temperature Field for Magnesium Alloy Tubes
    Morishima, Toshiji
    Manabe, Ken-Ichi
    METALS, 2021, 11 (06)
  • [46] NONLINEAR THEORY OF NON-UNIFORM TORSION OF THIN-WALLED OPEN BEAMS.
    Attard, Mario M.
    1600, (04):
  • [47] Non-uniform torsion of stiffened open thin-walled members of steel structures
    Gosowski, Bronislaw
    JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 2007, 63 (06) : 849 - 865
  • [48] Plastic wrinkling prediction in thin-walled part forming process: A review
    Liu Nan
    Yang He
    Li Heng
    Yan Siliang
    Chinese Journal of Aeronautics, 2016, (01) : 1 - 14
  • [49] Plastic wrinkling prediction in thin-walled part forming process: A review
    Liu, Nan
    Yang, He
    Li, Heng
    Yan, Siliang
    Chinese Journal of Aeronautics, 2016, 29 (01): : 1 - 14
  • [50] MODE INTERACTION IN THIN-WALLED TRAPEZOIDAL COLUMN UNDER UNIFORM COMPRESSION.
    Kolakowski, Z.
    1600, (05):