Experimental investigations into groove bottom surface roughness for Zr-based bulk metallic glass by using milling

被引:2
|
作者
Liu, Yin [1 ,2 ]
Song, Zhichao [3 ]
Liang, Zhengyi [1 ,2 ]
Cui, Xiaoqing [1 ,2 ]
Gong, Yadong [4 ]
Sun, Xingwei [1 ,2 ]
Dong, Zhixu [1 ,2 ]
Yang, Heran [1 ,2 ]
Liu, Weijun [1 ,2 ]
机构
[1] Shenyang Univ Technol, Sch Mech Engn, 111 Shenliao West Rd, Shenyang 110870, Peoples R China
[2] Shenyang Univ Technol, Liaoning Prov Key Lab Complex Surface NC Mfg Techn, 111 Shenliao West Rd, Shenyang 110870, Peoples R China
[3] AVIC Shenyang Aircraft Corp, 1 Lingbei St, Shenyang 110850, Peoples R China
[4] Northeastern Univ, Sch Mech Engn & Automat, 3-11 Wenhua Rd, Shenyang 110819, Peoples R China
基金
中国国家自然科学基金;
关键词
Zr-based bulk metallic glass; Groove milling; Surface roughness value; Milling groove bottom surface; Milling parameters; CHIP FORMATION; MORPHOLOGY;
D O I
10.1007/s00170-022-10720-3
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
In order to study the milling machinability of Zr-based bulk metallic glass, a comparative experimental study on the surface roughness of the milling groove bottom surface for Zr-based bulk metallic glass was carried out in this paper. Through different processing materials, milling tools with different coatings, milling tools with different geometric parameters, and different processing conditions, a large number of comparative tests were carried out on the surface roughness of the milling groove bottom surface for Zr-based bulk metallic glass. The surface roughness values of the milling groove bottom surface are compared, studied, and analyzed from many angles (surface roughness Sa, Sq, Sz, Ssk, and Sku). The test results show that Zr-based bulk metallic glass has good milling machinability. It can obtain a low surface roughness value through the processing conditions and methods used in the test. The research content of this paper provides experimental basis for groove milling of Zr-based bulk metallic glass. At the same time, it also provides a strong test basis for the manufacture of Zr-based bulk metallic glass parts.
引用
收藏
页码:855 / 872
页数:18
相关论文
共 50 条
  • [21] Quasicrystal formation in a Zr-based bulk metallic glass\
    Liu, L
    Chan, KC
    Pang, GKH
    AMORPHOUS AND NANOCRYSTALLINE METALS, 2004, 806 : 113 - 118
  • [22] Macrophage responses to a Zr-based bulk metallic glass
    Huang, Lu
    Zhang, Tao
    Liaw, Peter K.
    He, Wei
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2014, 102 (10) : 3369 - 3378
  • [23] Serration Dynamics in a Zr-Based Bulk Metallic Glass
    Z. Wang
    J. W. Qiao
    H. J. Yang
    P. K. Liaw
    C. J. Huang
    L. F. Li
    Metallurgical and Materials Transactions A, 2015, 46 : 2404 - 2414
  • [24] Cutting Characteristics of Zr-Based Bulk Metallic Glass
    Han, D. X.
    Wang, G.
    Li, J.
    Chan, K. C.
    To, S.
    Wu, F. F.
    Gao, Y. L.
    Zhai, Q. J.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2015, 31 (02) : 153 - 158
  • [25] The onset of plasticity of a Zr-based bulk metallic glass
    Huang, Yongjiang
    Khong, J. C.
    Connolley, Thomas
    Mi, J.
    INTERNATIONAL JOURNAL OF PLASTICITY, 2014, 60 : 87 - 100
  • [26] Quasicrystal formation in a Zr-based bulk metallic glass
    Liu, L
    Chan, KC
    Pang, GKH
    QUASICRYSTALS 2003-PREPARATION, PROPERTIES AND APPLICATIONS, 2004, 805 : 225 - 230
  • [27] Extrusion properties of a Zr-based bulk metallic glass
    Yu, G. S.
    Lin, J. G.
    Li, W.
    Wen, C. E.
    MATERIALS LETTERS, 2009, 63 (15) : 1317 - 1319
  • [28] Notched fatigue of Zr-based bulk metallic glass
    Nakai, Yoshikazu
    Sei, Naoki
    Kim, Bok-Key
    MECHANICAL BEHAVIOR OF MATERIALS X, PTS 1AND 2, 2007, 345-346 : 259 - +
  • [29] Experimental and Statistical Analysis of Fatigue Behavior in Zr-based Bulk Metallic Glass
    Yao, Zhifeng
    Qiao, Jichao
    Jean-Marc, Pelletier
    Yao, Yao
    RARE METAL MATERIALS AND ENGINEERING, 2024, 53 (11) : 3010 - 3016
  • [30] Superconductivity in a representative Zr-based bulk metallic glass
    Li, Y
    Bai, HY
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2005, 351 (30-32) : 2378 - 2382