Research on the energy properties and the storage stability of Al-Si-Li ternary alloy powders

被引:3
作者
Huang, Runkai [1 ]
Hu, Aobo [2 ]
Zhu, Yingcong [1 ]
Yang, Xi [1 ]
Zhang, Dong [1 ]
Cai, Shuizhou [1 ,3 ]
机构
[1] Huazhong Univ Sci & Technol, Sch Mat Sci & Engn, State Key Lab Mat Proc & Die & Mould Technol, Wuhan 430074, Hubei, Peoples R China
[2] Xian Modern Chem Res Inst, Xian 710065, Shaanxi, Peoples R China
[3] Huazhong Univ Sci & Technol, Dept Elect Sci & Technol, 1037 Luoyu Rd, Wuhan, Hubei, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2024年 / 28卷
基金
中国国家自然科学基金;
关键词
Al-Si-Li alloy powders; AlSiLi intermetallic compound phase; Thermal oxidation properties; Storage stability; Secondary ion mass spectrometry; ALUMINUM POWDERS; COMBUSTION; IGNITION; AGGLOMERATION; PROPELLANT; REACTIVITY; MECHANISM; BEHAVIOR;
D O I
10.1016/j.jmrt.2024.01.084
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To solve the problems of storage stability and compatibility of the Al-Li alloy powders, a series of Al-Si-Li alloy powders containing two-phase structure were prepared based on Al-Si-Li ternary phase diagram. The energy release, attenuation and compatibility of the Al-Si-Li alloy powders were studied by oxygen bomb calorimeter, XRD, SEM, TG-DSC and SIMS. As the content of the AlSiLi intermetallic compound phase increased, the measured mass combustion enthalpies increase before decreasing. When the proportion of the AlSiLi intermetallic compound phase is 20 wt.% (denoted as 20%-ASL), it has the maximum mass combustion enthalpy (31729 J.g(-1)) which is higher than the theoretical mass enthalpy of the pure aluminum powder (31000 J.g(-1)). The aging test of the 20%-ASL alloy powder show that its measured mass combustion enthalpy only decreased by 5.5 % (from 31739 J.g(-1) to 29921 J.g(-1)), along with the thermal oxidation weight gain decreasing from 95.82 % to 80.04 %, while mass combustion enthalpy of the Al-Li alloy powder with the same Li content decreased by 17.5 % (from 30325 J.g(-1) to 25031 J.g(-1)), and the weight gain decreased from 96.68 % to 41.05 %. This indicates that the AlSiLi phase effectively improves the oxidation resistance and storage stability of the Al-Li alloy powders. To explain this, surface Li distribution of the 20%-ASL alloy powder was analyzed by SIMS. The results show that the AlSiLi phase can immobilize Li inside the particles to reduce surface Li content from 2.920 x 106 to 1.439 x 106 and improve its oxidation resistance, thereby improving its storage stability and compatibility.
引用
收藏
页码:4805 / 4814
页数:10
相关论文
共 50 条
  • [41] Microstructures and properties in surface layers of Mg-6Zn-1Ca magnesium alloy laser-clad with Al-Si powders
    Zhang, Xiao-lin
    Zhang, Ke-min
    Zou, Jian-xin
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2018, 28 (01) : 96 - 102
  • [42] Effect of pre-annealing on microstructure and compactibility of gas-atomized Al-Si alloy powders
    Cai, Zhi-yong
    Zhang, Chun
    Wang, Ri-chu
    Peng, Chao-qun
    Qiu, Ke
    Wang, Nai-guang
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2016, 26 (09) : 2355 - 2362
  • [43] Microstructure and mechanical properties of foundry Al-Si-Cu-Hf alloy
    Xing, Yuan
    Jia, Zhihong
    Li, Jiehua
    Ding, Lipeng
    Huang, Huilan
    Liu, Qing
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 722 : 197 - 205
  • [44] Microstructure and Properties of Superhigh Strength Cu-Ni-(Al)-Si Alloy
    Li Sanhua
    Li Zhou
    Lei Qian
    Wang Mingpu
    Shen Leinuo
    Pan Zhiyong
    Liu Huiqun
    RARE METAL MATERIALS AND ENGINEERING, 2015, 44 (06) : 1427 - 1431
  • [45] An investigation of the effect of surface refining on the hardness and the wear properties of Al - Si alloy
    Saravanan, R.
    Sellamuthu, R.
    DYNAMICS OF MACHINES AND MECHANISMS, INDUSTRIAL RESEARCH, 2014, 592-594 : 53 - 57
  • [46] Effect of Sc and Sr on the Eutectic Si Morphology and Tensile Properties of Al-Si-Mg Alloy
    Xu, Cong
    Wang, Fang
    Mudassar, Hussain
    Wang, Chengyuan
    Hanada, Shuji
    Xiao, Wenlong
    Ma, Chaoli
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (04) : 1605 - 1613
  • [47] Free-Standing Si/Graphene Paper Using Si Nanoparticles Synthesized by Acid-Etching Al-Si Alloy Powder for High-Stability Li-Ion Battery Anodes
    Jiang, Heng
    Zhou, Xiong
    Liu, Gonggang
    Zhou, Yonghua
    Ye, Hongqi
    Liu, Yong
    Han, Kai
    ELECTROCHIMICA ACTA, 2016, 188 : 777 - 784
  • [48] Influences of quenching rate on mechanical and corrosion properties of Al-Cu-Li alloy
    Li, Chengbo
    Zhao, Cai
    Cao, Puli
    Xiao, Bo
    Chen, Qinyao
    MATERIALS TODAY COMMUNICATIONS, 2024, 40
  • [49] Effects of minor scandium addition on the properties of Mg-Li-Al-Zn alloy
    Wu, Horng-yu
    Gao, Zhen-wei
    Lin, Jia-yu
    Chiu, Chui-hung
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 474 (1-2) : 158 - 163
  • [50] Mechanical Properties and Microstructure Evolution of Al-Li Alloy Under the PHF Process
    Gong, Zhiang
    Huang, Xiang
    Wang, Peiliao
    Ma, Huijuan
    MATERIALS, 2025, 18 (03)