Martensite content effect on fatigue crack growth and fracture energy in dual-phase steels

被引:1
|
作者
Avendano-Rodriguez, D. [1 ]
Rodriguez-Baracaldo, R. [2 ,6 ]
Weber, S. [3 ]
Mujica-Roncery, L. [4 ,5 ]
机构
[1] Fdn Univ Amer, Res Grp Diseno Avanzado, Bogota, Colombia
[2] Univ Nacl Colombia, Res Grp Innovac Proc Manufactura & Ingn Mat, Bogota, Colombia
[3] Ruhr Univ Bochum, Inst Werkstoffe, Lehrstuhl Werkstofftechn, Bochum, Germany
[4] Univ Pedag & Tecnol Colombia, Res Grp Grp Invest Mat Siderurg, Tunja, Boyaca, Colombia
[5] Univ Pedag & Tecnol Colombia, INCITEMA, Tunja, Boyaca, Colombia
[6] Univ Nacl Colombia, Car 30 45-03, Bogota, Colombia
关键词
crack propagation; dual-phase steels; EBSD; fatigue; martensite volume fraction; VOLUME FRACTION; BEHAVIOR; MICROSTRUCTURE; PROPAGATION; MORPHOLOGY; TOUGHNESS; STRENGTH; PREDICTION; OVERLOAD; TENSILE;
D O I
10.1111/ffe.14209
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The effect of different microstructural factors on crack growth and fatigue fracture mechanisms in dual-phase (DP) steels has yet to be fully understood. The present research examines the relationship between crack growth, microstructure, and fracture mechanisms. The samples were intercritically annealed at different temperatures to produce three different martensite volume fractions (MVFs). The results show that the mechanical incompatibility of ferrite and martensite promotes continuous crack tip deflection. MVF increases are associated with elevated fracture tortuosity, more significant fracture energy surface formation, and higher Paris law exponent m values. The interaction of the microstructure with the crack tip, the strain energy density, and the softening caused by secondary microcrack propagation are all illustrated by Electron backscatter diffraction (EBSD) maps. Increasing MVF promotes slow crack growth and a fracture energy increase of 22.9% between the as-received and heat-treated steels. Martensite content in dual-phase steels generate greater crack propagation resistance.Martensite volume increase produces a more significant number and extension of secondary microcracks.Differences in ferrite and martensite phases promote continuous crack tip deflection.
引用
收藏
页码:884 / 902
页数:19
相关论文
共 50 条
  • [31] Study on microstructure and deformation behavior of dual-phase steels with high-martensite content
    Material Science and Engineering College, Shanghai University, Shanghai 200072, China
    Cailiao Rechuli Xuebao, 2008, 5 (49-52):
  • [32] Fatigue crack growth and fracture in steels
    Wasen, Jonas
    Chalmers Tekniska Hogskola, Doktorsavhandlingar, 1988, (688):
  • [33] The unexpected low fracture toughness of dual-phase steels caused by ferrite/martensite interface decohesion
    Liu, Lang
    Li, Liejun
    He, Jiazhen
    Liang, Zhiyuan
    Peng, Zhengwu
    Gao, Jixiang
    Luo, Zhichao
    Huang, Mingxin
    SCRIPTA MATERIALIA, 2024, 244
  • [34] FATIGUE CRACK-GROWTH IN AN AS-ROLLED DUAL-PHASE STEEL
    CHEN, DL
    WANG, ZG
    JIANG, XX
    AI, SH
    SHI, CX
    STEEL RESEARCH, 1988, 59 (07): : 319 - 322
  • [35] Stability of martensite with pulsed electric current in dual-phase steels
    Lu, W. J.
    Qin, R. S.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 677 : 252 - 258
  • [36] Influence of microstructural morphology and prestraining on short fatigue crack propagation in dual-phase steels
    Nakajima, K
    Urabe, T
    Hosoya, Y
    Kamishi, S
    Miyata, T
    Takeda, N
    ISIJ INTERNATIONAL, 2001, 41 (03) : 298 - 304
  • [37] Influence of bainite/martensite-content on the tensile properties of low carbon dual-phase steels
    Kumar, A.
    Singh, S. B.
    Ray, K. K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 474 (1-2): : 270 - 282
  • [38] Strain partitioning in dual-phase steels containing tempered martensite
    Han, Qihang
    Asgari, Alireza
    Hodgson, Peter D.
    Stanford, Nicole
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 611 : 90 - 99
  • [39] NEAR-THRESHOLD FATIGUE CRACK-PROPAGATION RATES OF DUAL-PHASE STEELS
    HORNG, JL
    FINE, ME
    MATERIALS SCIENCE AND ENGINEERING, 1984, 67 (02): : 185 - 195
  • [40] Deformation and fracture mechanisms in fine- and ultrafine-grained ferrite/martensite dual-phase steels and the effect of aging
    Calcagnotto, Marion
    Adachi, Yoshitaka
    Ponge, Dirk
    Raabe, Dierk
    ACTA MATERIALIA, 2011, 59 (02) : 658 - 670