Effects of MgO on Ni/Al2O3 catalysts for CO2 reforming of methane to syngas
被引:12
|作者:
Al-Baqmaa, Yousef A.
[1
]
Al-Fatesh, Ahmed S.
[1
]
Ibrahim, Ahmed A.
[1
]
Bagabas, Abdulaziz A.
[2
]
Almubadde, Fahad S.
[1
]
Alromaeh, Abdulaziz I.
[2
]
Abu-Dahrieh, Jehad K.
[3
]
Abasaeed, Ahmed E.
[1
]
Fakeeha, Anis H.
[1
]
机构:
[1] King Saud Univ, Coll Engn, Chem Engn Dept, POB 800, Riyadh 11421, Saudi Arabia
[2] King Abdulaziz City Sci & Technol KACST, Execut Off, POB 6086, Riyadh 11442, Saudi Arabia
[3] Queens Univ Belfast, Sch Chem & Chem Engn, Belfast BT9 5AG, North Ireland
关键词:
Carbon dioxide reforming of methane;
Ni-based catalyst;
MgO modifier;
& gamma;
-Al2O3;
support;
CARBON DEPOSITION;
NI;
NICKEL;
CH4;
REDUCTION;
STABILITY;
PR;
GD;
D O I:
10.1007/s11164-023-05117-0
中图分类号:
O6 [化学];
学科分类号:
0703 ;
摘要:
Carbon dioxide reforming of methane (CRM) converts CH4 and CO2 greenhouse gases into syngas over nickel-based catalysts. We performed CRM in a tubular microreactor at 700 degrees C by using 5.0 wt.% NiO catalyst, supported over mixtures of ?-Al2O3 + x MgO (x = 20, 30, 63, and 70 wt.%). The process of impregnation was used to prepare the catalysts. For characterization, N-2-physisorption, XRD, H-2-TPR, TGA, and Raman spectroscopy techniques were employed. Among the examined catalysts, 5Ni/Al2O3 + 63%MgO was found the most active, where it showed ? 72% CH4 conversion, 73% CO2 conversion, and 0.82 H-2/CO mole ratio over 7 h of reaction. The MgO modifier was the primary component, which favorably affected both Ni dispersion and stability, for the good interaction between NiO and ?-alumina. The mono-supported samples displayed the lowest total hydrogen consumption. In TGA, the 5Ni/Al2O3 + 63%MgO exhibited a significant weight decrease (40%), reflecting its activity. Furthermore, the Raman spectroscopy analysis showed that the crystal-linity of the carbon over this catalyst was more pronounced than the others.