Appropriate fitted point on fracture limit curve of orthotropic materials to include the fracture process zone effects on mixed-mode I/II fracture criterion

被引:2
作者
Daneshjoo, Zahra [1 ]
Fakoor, Mahdi [2 ]
机构
[1] Shahid Beheshti Univ, Fac Mech & Energy Engn, Tehran, Iran
[2] Univ Tehran, Fac New Sci & Technol, Tehran, Iran
基金
英国科研创新办公室;
关键词
DELAMINATION GROWTH; FAILURE CRITERION; CRACK-GROWTH; FLY-ASH; COMPOSITES; WOOD; STRENGTH; PHYSICS;
D O I
10.1007/s00707-022-03468-0
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
The fracture phenomenon in orthotropic materials is associated with the formation of the fracture process zone at the crack tip. Several toughening mechanisms in this zone delay the fracture by absorbing energy. The activation of these mechanisms and the extent of their effects depend on the loading mode. In this paper, the behavior of the fracture process zone under different loading modes is investigated. In the following, considering the fracture process zone effects, a new mixed-mode I/II fracture criterion is presented to investigate the crack growth behavior of orthotropic materials. In this criterion, by extending the minimum strain energy density theory to orthotropic materials and fitting the fracture limit curve to a midpoint (a mixed-mode I/II point) instead of the pure mode I point, a greater portion of the energy absorbed in the fracture process zone is considered. To validate the presented criterion, the related fracture limit curves are compared with the available experimental data for laminated composites and wood species as orthotropic materials. The results show that the newly proposed criterion, unlike the available conservative ones, especially around predominantly mode II, is more compatible with the nature of the failure phenomena in orthotropic materials.
引用
收藏
页码:1489 / 1502
页数:14
相关论文
共 50 条
  • [41] Tangential strain-based criteria for mixed-mode I/II fracture toughness of cement concrete
    Mirsayar, M. M.
    Razmi, A.
    Berto, F.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2018, 41 (01) : 129 - 137
  • [42] Mixed-mode I/II fracture performances of glued laminated bamboo in the in-plane longitudinal direction
    Liu, Wen
    Li, Zhi
    Li, Zheng
    ENGINEERING FRACTURE MECHANICS, 2023, 281
  • [43] A novel strategy to obtain the fracture envelope under mixed-mode I plus II loading of composite bonded joints
    Moreira, R. D. F.
    de Moura, M. F. S. F.
    Silva, F. G. A.
    ENGINEERING FRACTURE MECHANICS, 2020, 232
  • [44] Statistics of acoustic emission waveforms in characterizing the fracture process zone in fibre-reinforced cementitious materials under mode I fracture
    Sagar, R. Vidya
    Saha, Indrashish
    Basu, Dibya Jyoti
    Kundu, Tribikram
    STRUCTURAL HEALTH MONITORING-AN INTERNATIONAL JOURNAL, 2024, 23 (04): : 2083 - 2101
  • [45] 3D-generalized maximum tangential strain criterion for predicting mixed-mode I/II/III fracture initiation of brittle materials considering T-stress effects
    Ju, Yang
    Zhang, Yihao
    Wang, Kai
    Zhou, Hongwei
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2024, 131
  • [46] Mixed-mode I/II fracture criteria for adhesively-bonded pultruded GFRP/steel joint
    Jiang, Zhengwen
    Fang, Zhi
    Yan, Libo
    Wan, Shui
    Fang, Yawei
    COMPOSITE STRUCTURES, 2021, 255
  • [48] Probabilistic micromechanical damage model for mixed mode I/II fracture investigation of composite materials
    Khansari, Nabi Mehri
    Fakoor, Mandi
    Berto, Filippo
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2019, 99 : 177 - 193
  • [49] Fracture investigation of wood under mixed mode I/II loading based on the maximum shear stress criterion
    M. Fakoor
    R. Rafiee
    Strength of Materials, 2013, 45 : 378 - 385
  • [50] Maximum tangential strain energy density criterion for general mixed mode I/II/III brittle fracture
    Ayatollahi, M. R.
    Saboori, B.
    INTERNATIONAL JOURNAL OF DAMAGE MECHANICS, 2015, 24 (02) : 263 - 278