Effect of sugar palm fibers on the properties of blended wheat starch/polyvinyl alcohol (PVA)-based biocomposite films

被引:14
作者
Mohammed, Abdulrahman A. B. A. [1 ]
Hasan, Zaimah [1 ]
Omran, Abdoulhdi A. Borhana [2 ,3 ]
Elfaghi, Abdulhafid M. [4 ]
Ali, Yasir Hassan [5 ]
Akeel, Norie A. A. [2 ]
Ilyas, R. A. [6 ,7 ,8 ]
Sapuan, S. M. [8 ]
机构
[1] Univ Tenaga Nas, Coll Engn, Dept Mech Engn, Jalan Ikram Uniten, Kajang 43000, Selangor, Malaysia
[2] Sohar Univ, Fac Engn, Dept Mech & Mechatron Engn, Sohar 311, Oman
[3] Sebha Univ, Coll Engn Sci & Technol, Dept Mech Engn, Sabha, Libya
[4] Univ Tun Hussein Onn Malaysia, Fac Mech & Mfg Engn, Parit Raja, Malaysia
[5] Northern Tech Univ, Tech Coll Mosul, Dept Power Mech Tech Engn, Mosul, Iraq
[6] Univ Teknol Malaysia, Fac Engn, Sch Chem & Energy Engn, Johor Baharu 81310, Johor, Malaysia
[7] Univ Teknol Malaysia, Ctr Adv Composite Mat CACM, Johor Baharu 81310, Johor, Malaysia
[8] Univ Putra Malaysia, Inst Trop Forestry & Forest Prod INTROP, Serdang 43400, Selangor, Malaysia
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2023年 / 24卷
关键词
Wheat starch; Biocomposite; Polyvinyl alcohol; Fructose; Sugar palm fiber; CELLULOSE NANOCRYSTALS; FT-IR; STARCH; WATER; SPECTROSCOPY;
D O I
10.1016/j.jmrt.2023.02.027
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Sugar palm fiber has been added to reinforce starch, polyvinyl alcohol (PVA) based film. The effect of reinforcement on different properties has been studied. It has been found that reinforcing plasticized starch/PVA matrix with palm fibers has considerably enhanced physical properties, the density of the polymer declined to 1.21 g/cm3 with untreated fibers and to 1.32 g/cm3 with treated fibers, which created a lighter weight bioplastic, and a reduction occurred in water absorption (for example 3% of treated fiber showed 143% absorbed water after 30 min immersing in water) and water solubility. When compared to the films without fibers filler, films reinforced with fibers demonstrated a c3onsiderable improvement in the crystal profile; at 9% fiber load, it improved over double. Additionally, it has been noted that thermal stability has increased. The existence of treated and untreated fibers in the hybrid matrix revealed 23.3% and 24.6% mass residues at 495 degrees C, respectively. However, this enhancement did not coincide with a rise in mechanical properties, Whilst, improvements in tensile strength and modulus occurred at 9% of treated fiber load, showing 12 MPa and 245 MPa, respectively. The highest elongation was 66.3% at 3% of treated fiber films. Meanwhile, films reinforced with treated sugar palm fibers showed higher mechanical properties than films with untreated sugar palm fibers. Scanning Electronic Microscope images exhibited higher interfacial interaction at 9% for both treated and untreated sugar palm fibers. (c) 2023 Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:1043 / 1055
页数:13
相关论文
共 50 条
  • [1] Effect of sugar alcohol on physicochemical properties of wheat starch
    Sun, Qingjie
    Nan, Chong
    Dai, Lei
    Ji, Na
    Xiong, Liu
    STARCH-STARKE, 2014, 66 (9-10): : 788 - 794
  • [2] Effect of Sugar Palm-derived Cellulose Reinforcement on the Mechanical and Water Barrier Properties of Sugar Palm Starch Biocomposite Films
    Sanyang, Muhammed Lamin
    Sapuan, S. M.
    Jawaid, Mohammad
    Ishak, Mohamad Ridzwan
    Sahari, Japar
    BIORESOURCES, 2016, 11 (02): : 4134 - 4145
  • [3] Dynamic and creep analysis of polyvinyl alcohol based films blended with starch and protein
    Jain, Naman
    Singh, Vinay K.
    Chauhan, Sakshi
    JOURNAL OF POLYMER ENGINEERING, 2019, 39 (01) : 35 - 47
  • [4] Thermoplastic Sugar Palm Starch Reinforced Graphene Nanoplatelets for Sustainable Biocomposite Films
    Rahmat, Noor Fadhilah
    Sajab, Mohd Shaiful
    Afdzaluddin, Atiqah Mohd
    Ding, Gongtao
    Chia, Chin Hua
    BIORESOURCES, 2024, 19 (01) : 1526 - 1541
  • [5] Preparation and Characterization of Polyvinyl Alcohol (PVA)/Carbonized Waste Rubber Biocomposite Films
    Zor, Mustafa
    Sen, Ferhat
    Candan, Zeki
    Ivanov, Evgeni
    Batakliev, Todor
    Georgiev, Vladimir
    Menseidov, Dzhihan
    POLYMERS, 2024, 16 (08)
  • [6] Effect of Acrylic Acid on The Mechanical Properties of PVA/Starch Blend Films
    Negim, El-Sayed
    Bakytzhanuly, B.
    Urkimbayeva, P., I
    Bekbayeva, L.
    Othman, M. B. H.
    Ibrahim, M. N. Mohamad
    Mun, G. A.
    EGYPTIAN JOURNAL OF CHEMISTRY, 2020, 63 (05): : 1911 - 1919
  • [7] Fabrication and properties of polyvinyl alcohol/starch blend films: Effect of composition and humidity
    Tian, Huafeng
    Yan, Jiaan
    Rajulu, A. Varada
    Xiang, Aimin
    Luo, Xiaogang
    INTERNATIONAL JOURNAL OF BIOLOGICAL MACROMOLECULES, 2017, 96 : 518 - 523
  • [8] Polyvinyl alcohol (PVA)-based films: insights from crosslinking and plasticizer incorporation
    Chousidis, Nikolaos
    ENGINEERING RESEARCH EXPRESS, 2024, 6 (02):
  • [9] Glutaraldehyde crosslinked polyvinyl alcohol/eggshell powder biocomposite films: Properties and biodegradability
    Alias N.F.
    Ismail H.
    Ismail, Hanafi (ihanafi@usm.my), 1600, Penerbit Universiti Sains Malaysia (31): : 45 - 60
  • [10] Glutaraldehyde Crosslinked Polyvinyl Alcohol/Eggshell Powder Biocomposite Films: Properties and Biodegradability
    Alias, Nur Fazreen
    Ismail, Hanafi
    JOURNAL OF PHYSICAL SCIENCE, 2020, 31 (02) : 45 - 60