Microstructure evolution of Ti17 titanium with ultrahigh strength and moderate plasticity fabricated by laser powder bed fusion

被引:1
|
作者
Wang, Shuaiqi [1 ,2 ,3 ,4 ]
He, Bei [1 ,2 ,3 ,4 ]
Tang, Haibo [1 ,2 ,3 ,4 ]
机构
[1] Beihang Univ, Natl Engn Lab Addit Mfg Large Met Components, 37 Xueyuan Rd, Beijing, Peoples R China
[2] Beihang Univ, Minist Educ Laser Direct Mfg Large Met Components, Engn Res Ctr, 37 Xueyuan Rd, Beijing, Peoples R China
[3] Beihang Univ, Beijing Engn Technol Res Ctr Laser Direct Mfg Larg, 37 Xueyuan Rd, Beijing, Peoples R China
[4] Beihang Univ, Res Inst Frontier Sci, 37 Xueyuan Rd, Beijing, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2024年 / 893卷
基金
中国国家自然科学基金;
关键词
Titanium alloys; Additive manufacturing methods; Phase transformations; Plasticity; ADDITIVELY MANUFACTURED TI-6AL-4V; HEAT-TREATMENT; MECHANICAL-PROPERTIES; COARSENING BEHAVIOR; TI-17; ALLOY; GLOBULARIZATION; ALPHA;
D O I
10.1016/j.msea.2024.146142
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This study utilized laser powder bed fusion (LPBF) to fabricate Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti17) specimens, exploring their ultrahigh strength microstructural strengthening mechanisms and examining heat treatment effects on alpha lamellae and related mechanical property trends. In the as-deposited LPBF-Ti17, alpha lamellae features extremely fine dimensions, with an average lamellar thickness of 45 nm, and comprises approximately 52.2% of total volume. This finely dispersed alpha lamellar microstructure provides numerous alpha/beta phase interfaces, enabling LPBF-Ti17 mechanical properties to reach ultra-high strengths close to 1500 MPa. During heat treatment, the Ostwald ripening mechanism primarily drives growth in alpha-phase lamellar thickness. The rate of alpha lamellar thickness growth reaches its peak between 650 degrees C and 700 degrees C. The main dislocation distribution of LPBF-Ti17 lies at alpha lamellae edges, adjacent to beta phase, and dislocation density diminishes with rising heat treatment temperature. Concurrently, the Termination migration mechanism causes alpha lamellae ends to become progressively rounded from sharp features with increasing heat treatment temperature. The increase in alpha lamellar thickness and reduction in dislocation density collectively contribute to the effective enhancement of Ti17 plasticity.
引用
收藏
页数:10
相关论文
共 50 条
  • [21] Correlation of microstructure, mechanical properties, and residual stress of 17-4 PH stainless steel fabricated by laser powder bed fusion
    Moyle, M. S.
    Haghdadi, N.
    Luzin, V.
    Salvemini, F.
    Liao, X. Z.
    Ringer, S. P.
    Primig, S.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2024, 198 : 83 - 97
  • [22] Effect of powder bed preheating on the crack formation and microstructure in ceramic matrix composites fabricated by laser powder-bed fusion process
    Maurya, H. S.
    Kosiba, K.
    Juhani, K.
    Sergejev, F.
    Prashanth, K. G.
    ADDITIVE MANUFACTURING, 2022, 58
  • [23] High temperature high strength austenitic steel fabricated by laser powder-bed fusion
    Dryepondt, Sebastien
    Nandwana, Peeyush
    Unocic, Kinga A.
    Kannan, Rangasayee
    Zelaia, Patxi Fernandez
    List, Fred A., III
    ACTA MATERIALIA, 2022, 231
  • [24] Study on Morphology, Microstructure, and Tribo-Corrosion Behavior of Laser-Powder-Bed-Fusion-Fabricated Titanium Alloy
    Lu, Peipei
    Wang, Hongfeng
    Wu, Meiping
    ADVANCED ENGINEERING MATERIALS, 2023, 25 (23)
  • [25] Tailoring bimodal structure for high strength and ductility in pure titanium manufactured via laser powder bed fusion
    Wang, Chang-Shun
    Li, Cheng-Lin
    Zuo, Yu-Ting
    Hong, Jae-Keun
    Choi, Seong-Woo
    Zhang, Guo-Dong
    Mei, Qingsong
    Park, Chan Hee
    Yeom, Jong-Taek
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 901
  • [26] Microstructure and Mechanical Properties of a Novel Al-Mg-Sc-Ti Alloy Fabricated by Laser Powder Bed Fusion
    Shu, Zhiheng
    Liu, Yunzhong
    MATERIALS, 2024, 17 (03)
  • [27] Laser powder bed fusion of ultrahigh strength Fe-Cu alloys using elemental powders
    Zafari, A.
    Xia, K.
    ADDITIVE MANUFACTURING, 2021, 47
  • [28] Evaluation of microstructure heterogeneity in INCONEL 625 thin-wall fabricated by Laser Powder Bed Fusion additive manufacturing
    Mohammadpour, P.
    Yuan, H.
    Li, Z.
    Phillion, A. B.
    MATERIALIA, 2024, 35
  • [29] Fracture behavior of laser powder bed fusion fabricated Ti41Nb via in-situ alloying
    Huang, Sheng
    Kumar, Punit
    Yeong, Wai Yee
    Narayan, R. Lakshmi
    Ramamurty, Upadrasta
    ACTA MATERIALIA, 2022, 225
  • [30] Microstructure and defects in a Ni-Cr-Al-Ti γ/γ′ model superalloy processed by laser powder bed fusion
    De Luca, Anthony
    Kenel, Christoph
    Griffiths, Seth
    Joglekar, Shreyas S.
    Leinenbach, Christian
    Dunand, David C.
    MATERIALS & DESIGN, 2021, 201