Micro-electrochemical insights into pit initiation site on aged UNS S32750 super duplex stainless steel

被引:21
|
作者
Amatsuka, Shuichiro [1 ]
Nishimoto, Masashi [1 ]
Muto, Izumi [1 ]
Kawamori, Makoto [2 ]
Takara, Yuya [2 ]
Sugawara, Yu [1 ]
机构
[1] Tohoku Univ, Grad Sch Engn, Dept Mat Sci, 6-6-02 Aza Aoba, Aoba Ku, Sendai 9808579, Japan
[2] Kobe Steel Ltd, Kobe Corp Res Labs, 5-5, Takatsukadai 1 Chome, Nishi Ku, Kobe, Hyogo 6512271, Japan
关键词
SIGMA-PHASE PRECIPITATION; PITTING CORROSION-RESISTANCE; HEAT-AFFECTED ZONE; MICROSTRUCTURE EVOLUTION; MNS INCLUSIONS; MICROELECTROCHEMICAL MEASUREMENTS; TREATMENT TEMPERATURE; BEHAVIOR; DISSOLUTION; SIZE;
D O I
10.1038/s41529-023-00335-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An aging treatment of UNS S32750 super duplex stainless steel at 1173 K for 1.0 ks produced sigma and secondary austenite (gamma(2)) phases in the alpha and gamma phase boundary regions. Small amount of Mn-Cr oxide and MnS complex inclusions were present in the steel. No pitting was observed during the potentiodynamic polarization of a small area (200 x 200 mu m) without inclusions in 1 M MgCl2 at 348 K. Because the electrode area included alpha, gamma, sigma, and gamma(2) phases, these phases and their boundaries alone could not act as initiation sites for pitting. The electrode area size was gradually reduced from 3 x 3 mm to 1 x 1 mm, and pitting corrosion was observed to occur at the Mn-Cr oxide and MnS complex inclusions in a region that appeared to be the gamma(2) phase near the sigma phase.
引用
收藏
页数:10
相关论文
共 50 条
  • [21] Optimization of hardness, tensile strengthand fatigue life of micro plasma arc welded super duplex stainless steel UNS S32750 using grey relational analysis
    Gurugubelli, Sasidhar
    Rao, V. V. S. Kesava
    INTERNATIONAL JOURNAL OF INTERACTIVE DESIGN AND MANUFACTURING - IJIDEM, 2025, 19 (04): : 2999 - 3013
  • [22] Precipitation condition and effect of volume fraction on corrosion properties of secondary phase on casted super-duplex stainless steel UNS S32750
    Shin, Byung-Hyun
    Kim, Dohyung
    Park, Sanghyup
    Hwang, Myungwon
    Park, Junghyun
    Chung, Wonsub
    ANTI-CORROSION METHODS AND MATERIALS, 2019, 66 (01) : 61 - 66
  • [23] Fatigue life of super duplex stainless steel sheets (UNS S32750) as influenced by micro plasma arc welding parameters: an investigation using the surface response method
    Gurugubelli, Sasidhar
    Rao, V. V. S. Kesava
    INTERNATIONAL JOURNAL OF INTERACTIVE DESIGN AND MANUFACTURING - IJIDEM, 2024, 18 (03): : 1183 - 1193
  • [24] Premature failure in UNS S32750 duplex stainless steel laying head pipes: The role of sigma phase precipitation
    Moreira, Guilherme Duarte
    Maia, Juliana de Fatima
    de Faria, Geraldo Lucio
    ENGINEERING FAILURE ANALYSIS, 2025, 169
  • [25] Altered microstructure characteristics and enhanced corrosion resistance of UNS S32750 duplex stainless steel via ultrasonic surface rolling process
    Zhang, Jiantao
    Zhu, Yuanzhi
    Xi, Xiaoying
    Xiao, Zhiyu
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2022, 309
  • [26] Effect of Solution Annealing on Austenite Morphology and Pitting Corrosion of Super Duplex Stainless Steel UNS S 32750
    Sung, Changwon
    Shin, Byung-Hyun
    Chung, Wonsub
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2021, 16 (08): : 1 - 10
  • [27] Effect of optimal weld parameters in the microstructure and mechanical properties of autogeneous gas tungsten arc weldments of super-duplex stainless steel UNS S32750
    Ramkumar, K. Devendranath
    Mishra, Debidutta
    Raj, B. Ganesh
    Vignesh, M. K.
    Thiruvengatam, G.
    Sudharshan, S. P.
    Arivazhagan, N.
    Sivashanmugam, N.
    Rabel, Arul Maximus
    MATERIALS & DESIGN, 2015, 66 : 356 - 365
  • [28] Study on the corrosion mechanism of S32750 super duplex stainless steel in NaCl solution containing formic acid
    He, Jiaxuan
    Zhao, Xuhui
    Tang, Yuming
    Zuo, Yu
    MATERIALS TODAY COMMUNICATIONS, 2024, 41
  • [29] Influence of Solution Treatment Duration on Microstructural Features of an Industrial Forged UNS S32750/1.4410/F53 Super Duplex Stainless Steel (SDSS) Alloy
    Cojocaru, Vasile Danut
    Raducanu, Doina
    Angelescu, Mariana Lucia
    Vintila, Adrian Nicolae
    Serban, Nicolae
    Dan, Ioan
    Cojocaru, Elisabeta Mirela
    Cinca, Ion
    JOM, 2017, 69 (08) : 1439 - 1445
  • [30] Effect of cooling rate after heat treatment on pitting corrosion of super duplex stainless steel UNS S 32750
    Shin, Byung-Hyun
    Park, Junghyun
    Jeon, Jongbae
    Heo, Sung-bo
    Chung, Wonsub
    ANTI-CORROSION METHODS AND MATERIALS, 2018, 65 (05) : 492 - 498