Effect of surface treatments on optical, topographical and mechanical properties of CAD/CAM reinforced lithium silicate glass ceramics

被引:9
|
作者
Al-Johani, Hanan [1 ,2 ]
Haider, Julfikar [1 ,3 ]
Silikas, Nick [1 ,4 ]
Satterthwaite, Julian [1 ]
机构
[1] Univ Manchester, Sch Med Sci, Div Dent, Manchester, England
[2] King Abdulaziz Univ, Dept Restorat Dent, Fac Dent, Div Biomat, Jeddah, Saudi Arabia
[3] Manchester Metropolitan Univ, Dept Engn, Manchester, England
[4] Univ Manchester, Sch Med Sci, Coupland 3 Bldg,Oxford Rd, Manchester M13 9PL, England
关键词
CAD/CAM Ceramic; Lithium disilicate; Zirconia-reinforced lithium silicate; Lithium aluminum disilicate; Surface treatment; Acid neutralization; Photometry; Topography; Biaxial flexural strength; MICROTENSILE BOND STRENGTH; 3 BALLS TEST; HYDROFLUORIC-ACID; FLEXURAL STRENGTH; PARTICLE ABRASION; RESIN BOND; TRANSLUCENCY; THICKNESS; ADHESION; RESPECT;
D O I
10.1016/j.dental.2023.07.004
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: To investigate the effect of different surface treatments on optical, topographical and mechanical properties of CAD/CAM lithium silicate-based glass ceramics (LSC's) and their combined effect on the output of a light curing unit (LCU). Methods: Four CAD/CAM LSC's were investigated: Lithium Disilicate (Emax CAD; EC), Zirconia-reinforced silicates (Vita Suprinity; VS and Celtra Duo;CD) and Lithium Aluminum Disilicate (CEREC Tessera; CT). Ceramic specimens (n = 240) were divided into six subgroups according to their surface treatment: (a) Control, (b) Hydrofluoric acid (HF) 5%, (c) HF 5% + Neutralizing agent (N), (d) HF 9%, (e) HF 9% +N and (f) Self-etching ceramic primer (SEP). Irradiance, power and radiant exposure of a LCU were measured with MARC-LC following ceramic specimen interposition. Direct light transmission (T%) and absorbance (Abs%) of the specimens were measured with UV-Vis spectrophotometry. Roughness (Sa, Sq) and wettability (theta degrees) were measured with optical profilometry and sessile drop profile analysis, respectively. Biaxial flexural strength (sigma) of the ceramic specimens was measured by the ball-on-three-balls method and ceramic specimens were examined microscopically. Statistical analyses was performed by two-way ANOVA followed by post hoc multiple comparisons (alpha = 0.05). Results: Acid neutralization decreased T% and increased Abs% in all LSC's and highest T% was exhibited with VS. Neutralized EC, VS and CD displayed higher Sa in HF9, while neutralized CT displayed higher Sa in HF5. Self-etch primer significantly reduced theta degrees (p < 0.001). sigma was observed in the followed ascending order: HF9 +N < HF9 < HF5 +N < HF5 < SEP < Control for all LSC's. Significance: Optical, topographical and mechanical properties of the CAD/CAM ceramic blocks were strongly dependent on the type of surface treatment. Results of neutralization post-etching indicate promising potential for future investigations.
引用
收藏
页码:779 / 789
页数:11
相关论文
共 50 条
  • [41] Influence of minimal extended firing on dimensional, optical, and mechanical properties of crystalized zirconia-reinforced lithium silicate glass ceramic
    Schweitzer, Florian
    Spintzyk, Sebastian
    Geis-Gerstorfer, Juergen
    Huettig, Fabian
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2020, 104
  • [42] Effect of surface treatments on wear and surface properties of different CAD-CAM materials and their enamel antagonists
    Cakmak, Gulce
    Subasi, Meryem Gulce
    Sert, Murat
    Yilmaz, Burak
    JOURNAL OF PROSTHETIC DENTISTRY, 2023, 129 (03) : 495 - 506
  • [43] Shear bond strength of cemented zirconia-reinforced lithium silicate ceramics (Celtra Duo) with two surface treatments (in vitro study)
    Abdulkader, Kamilia Faisal
    Elnaggar, Gihan Abd Elhady
    Kheiralla, Lamiaa Sayed
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2021, 35 (01) : 35 - 51
  • [44] Evaluation and Comparison of Mechanical Properties of Lithium Disilicate-Based CAD/CAM Blocks
    Zulkiffli, Sofya
    Take, Yeoh Oon
    Yahya, Noor Azlin
    Kutty, Muralithran Govindan
    SAINS MALAYSIANA, 2024, 53 (01): : 217 - 229
  • [45] Alternative surface treatments strategies for bonding to CAD/CAM resin-matrix ceramics
    Wanderico, Carolina Marino
    Picolo, Mayara Zaghi Dal
    Kury, Matheus
    Azevedo, Veber Luis Bonfim
    Giannini, Marcelo
    Cavalli, Vanessa
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2023, 37 (08) : 1471 - 1484
  • [46] Effect of different surface treatments on resin-matrix CAD/CAM ceramics bonding to dentin: in vitro study
    Fathy, Hanan
    Hamama, Hamdi H.
    El-Wassefy, Noha
    Mahmoud, Salah H.
    BMC ORAL HEALTH, 2022, 22 (01)
  • [47] Optical and Mechanical Properties of New Ceramic CAD/CAM Materials
    Reid, D. A.
    Matis, J. I.
    Lien, W.
    Raimondi, C. J.
    Arnason, S. C.
    DuVall, N. B.
    Vandewalle, K. S.
    OPERATIVE DENTISTRY, 2023, 48 (04) : 425 - 434
  • [48] Effect of different surface treatments on resin-matrix CAD/CAM ceramics bonding to dentin: in vitro study
    Hanan Fathy
    Hamdi H. Hamama
    Noha El-Wassefy
    Salah H. Mahmoud
    BMC Oral Health, 22
  • [49] The effect of coffee and whitening systems on surface roughness and gloss of CAD/CAM lithium disilicate glass cermaics
    Al-Angari, Sarah S.
    Meaigel, Shahad
    Almayouf, Nouf
    Quwayhis, Shahad
    Aldahash, Abdulelah
    Al-Angari, Nadia S.
    JOURNAL OF APPLIED BIOMATERIALS & FUNCTIONAL MATERIALS, 2021, 19
  • [50] Effect of thickness, cement shade, and coffee thermocycling on the optical properties of zirconia reinforced lithium silicate ceramic
    Cakmak, Gulce
    Donmez, Mustafa Borga
    Kashkari, Afnan
    Johnston, William M.
    Yilmaz, Burak
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2021, 33 (08) : 1132 - 1138