The Influence of Plasticizers and Accelerated Ageing on Biodegradation of PLA under Controlled Composting Conditions

被引:24
作者
Brdlik, Pavel [1 ]
Novak, Jan [1 ]
Boruvka, Martin [1 ]
Behalek, Lubos [1 ]
Lenfeld, Petr [1 ]
机构
[1] Tech Univ Liberec, Fac Mech Engn, Studentska 1402-2, Liberec 46117, Czech Republic
关键词
PLA films; plasticizers; biodegradation; ageing; composting; POLY(LACTIDE)/POLY(ETHYLENE GLYCOL) BLENDS; POLY(LACTIC ACID); MECHANICAL-PROPERTIES; TRIBUTYL CITRATE; LACTIC-ACID; DEGRADATION; POLYLACTIDE; BEHAVIOR; PEG; CHITOSAN;
D O I
10.3390/polym15010140
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The overall performance of plasticizers on common mechanical and physical properties, as well as on the processability of polylactic acid (PLA) films, is well-explored. However, the influence of plasticizers on biodegradation is still in its infancy. In this study, the influence of natural-based dicarboxylic acid-based ester plasticizers (MC2178 and MC2192), acetyl tributyl citrate (ATBC Citroflex A4), and polyethylene glycol (PEG 400) on the biodegradation of extruded PLA films was evaluated. Furthermore, the influence of accelerated ageing on the performance properties and biodegradation of films was further investigated. The biodegradation of films was determined under controlled thermophilic composting conditions (ISO 14855-1). Apart from respirometry, an evaluation of the degree of disintegration, differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), Fourier transform infrared spectroscopy (FT-IR), and scanning electron microscopy (SEM) of film surfaces was conducted. The influence of melt-processing with plasticizers has a significant effect on structural changes. Especially, the degree of crystallinity has been found to be a major factor which affects the biodegradation rate. The lowest biodegradation rates have been evaluated for films plasticized with PEG 400. These lower molecular weight plasticizers enhanced the crystallinity degrees of the PLA phase due to an increase in chain mobility. On the contrary, the highest biodegradation rate was found for films plasticized with MC2192, which has a higher molecular weight and evoked minimal structural changes of the PLA. From the evaluated results, it could also be stated that migration of plasticizers, physical ageing, and chain scission of films prompted by ageing significantly influenced both the mechanical and thermal properties, as well as the biodegradation rate. Therefore, the ageing of parts has to be taken into consideration for the proper evolution of the biodegradation of plasticized PLA and their applications.
引用
收藏
页数:31
相关论文
共 59 条
  • [21] Analysis of the Structure-Properties Relationships of Different Multiphase Systems Based on Plasticized Poly(Lactic Acid)
    Courgneau, Cecile
    Domenek, Sandra
    Guinault, Alain
    Averous, Luc
    Ducruet, Violette
    [J]. JOURNAL OF POLYMERS AND THE ENVIRONMENT, 2011, 19 (02) : 362 - 371
  • [22] Darie-Nita RN, 2016, J APPL POLYM SCI, V133, DOI [10.1002/app.43223, 10.1002/APP.43223]
  • [23] Thermal degradation of poly(3-hydroxybutyrate) plasticized with acetyl tributyl citrate
    Erceg, M
    Kovacic, T
    Klaric, I
    [J]. POLYMER DEGRADATION AND STABILITY, 2005, 90 (02) : 313 - 318
  • [24] Physical and mechanical properties of PLA, and their functions in widespread applications - A comprehensive review
    Farah, Shady
    Anderson, Daniel G.
    Langer, Robert
    [J]. ADVANCED DRUG DELIVERY REVIEWS, 2016, 107 : 367 - 392
  • [25] Effect of Extrusion Screw Speed and Plasticizer Proportions on the Rheological, Thermal, Mechanical, Morphological and Superficial Properties of PLA
    Galvez, Jaime
    Correa Aguirre, Juan P.
    Hidalgo Salazar, Miguel A.
    Vera Mondragon, Bairo
    Wagner, Elizabeth
    Caicedo, Carolina
    [J]. POLYMERS, 2020, 12 (09)
  • [26] Influence of plasticizer configurational changes on the dielectric characteristics of highly plasticized poly(vinyl chloride)
    Gibbons, WS
    Kusy, RP
    [J]. POLYMER, 1998, 39 (14) : 3167 - 3178
  • [27] Hydrolysis and Biodegradation of Poly(lactic acid)
    Gorrasi, Giuliana
    Pantani, Roberto
    [J]. SYNTHESIS, STRUCTURE AND PROPERTIES OF POLY(LACTIC ACID), 2018, 279 : 119 - 151
  • [28] Thermal behavior of PLA plasticized by commercial and cardanol-derived plasticizers and the effect on the mechanical properties
    Greco, Antonio
    Ferrari, Francesca
    [J]. JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2021, 146 (01) : 131 - 141
  • [29] Hao Y., 2021, ARESTY RURJ, V1, P57
  • [30] New approach on the development of plasticized polylactide (PLA): Grafting of poly(ethylene glycol) (PEG) via reactive extrusion
    Hassouna, Fatima
    Raquez, Jean-Marie
    Addiego, Frederic
    Dubois, Philippe
    Toniazzo, Valerie
    Ruch, David
    [J]. EUROPEAN POLYMER JOURNAL, 2011, 47 (11) : 2134 - 2144