Joining of textured PLS-SiC ceramic with CaO-Al2O3-MgO-TiO2-SiO2 glass filler

被引:3
|
作者
Zhan, Chuang-Tian [1 ]
Wu, Jin-Yuan [1 ]
Huang, Kun-Heng [1 ]
Li, Yun [2 ]
Wu, Li-Xiang [2 ]
He, Sheng-Jin [1 ]
Liu, Yang-Qing [1 ]
Zhang, Ze-Xi [1 ]
Guo, Wei-Ming [1 ]
Xue, Jia-Xiang [2 ]
Lin, Hua-Tay [1 ]
机构
[1] Guangdong Univ Technol, Sch Electromech Engn, Guangzhou 510006, Peoples R China
[2] China Nucl Power Technol Res Inst, Nucl Fuel & Mat Dept, Shenzhen 518026, Peoples R China
基金
中国国家自然科学基金;
关键词
SiC ceramic; Joining; Texture; Glass filler; Shear strength; SILICON-CARBIDE; CRYSTALLIZATION BEHAVIOR; BOROSILICATE GLASS; SHEAR-STRENGTH; COMPONENTS;
D O I
10.1016/j.ceramint.2023.10.125
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The pressureless-sintered silicon carbide ceramic with and without surface texturing was joined with CaO-Al2O3MgO-TiO2-SiO2 glass filler. The experimental results showed that without texturing applied to SiC substrates, the shear strength of SiC joints was 40.8 +/- 6.3 MPa, with failure occurring at the interlayer. Unfilled regions in the interlayer limited the shear strength of the joints. When texturing was applied to SiC substrates, SiO2 layer was formed on the surface of substrates due to high-temperature oxidation, which subsequently promoted the wettability of filler on substrates. The textured grooves on SiC substrates could be filled with glass material during joining process. The shear strength of textured SiC joints was 69.3 +/- 9.9 MPa with a mixed-mode failure when the direction of shear load was perpendicular to the texturing direction. The better wettability, larger joining area, and interlocking structure between the glass filler and substrates enhanced the shear strength of textured joints.
引用
收藏
页码:495 / 502
页数:8
相关论文
共 50 条
  • [41] Microstructure evolution and mechanical properties of porous Si3N4 and dense Si3N4 joints bonded using CaO Li2O-Al2O3 SiO2 glass-ceramic
    Fang, Jian
    Sun, Liangbo
    Qi, Qin
    Zhang, Jie
    Liu, Chunfeng
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (15) : 4545 - 4553
  • [42] Effect of CaO doping on the properties and crystallization behavior of Y2O3-Al2O3-SiO2 glass
    Yang, Shaobo
    Ma, Yujie
    Li, Jiali
    Kou, Sijie
    Chen, Bo
    Liu, Chidong
    Deng, Juanli
    Fan, Shangwu
    CERAMICS INTERNATIONAL, 2023, 49 (20) : 33188 - 33196
  • [43] Effect of Temperature on the Structure of CaO-MgO-Al2O3-SiO2 Nanocrystalline Glass-Ceramics Studied by Raman Spectroscopy
    Li Bao-wei
    Ouyang Shun-li
    Zhang Xue-feng
    Jia Xiao-lin
    Deng Lei-bo
    Liu Fang
    SPECTROSCOPY AND SPECTRAL ANALYSIS, 2014, 34 (07) : 1869 - 1872
  • [44] Preparation and characterization of MgO-Al2O3-SiO2 glass-ceramics with different MgO/Al2O3 ratio and La2O3 addition
    Zhan, Lingli
    Jia, Han
    Jiang, Chao
    Lin, Tiesong
    Li, Hong
    Wang, Mitang
    Xiong, Dehua
    MATERIALS TODAY COMMUNICATIONS, 2024, 38
  • [45] Crystallization behavior and properties of K2O-CaO-Al2O3-SiO2 glass-ceramics
    Wu, Jianfang
    Li, Zhen
    Huang, Yanqiu
    Li, Fei
    CERAMICS INTERNATIONAL, 2013, 39 (07) : 7743 - 7750
  • [46] Effect of TiO2 on fluoride evaporation from CaF2-CaO-Al2O3-MgO-Li2O-(TiO2) slag
    Ju, Jian-tao
    Ji, Guang-heng
    An, Jia-liang
    Tang, Chen-mei
    IRONMAKING & STEELMAKING, 2021, 48 (01) : 109 - 115
  • [47] STUDY OF ARTIFICIAL CERAMIC BINDER PROPERTIES IN THE SYSTEM Al2O3-SiO2-SiC
    Zaitsev, S. V.
    Doroganov, V. A.
    Doroganov, E. A.
    Evtushenko, E. I.
    REFRACTORIES AND INDUSTRIAL CERAMICS, 2017, 57 (05) : 526 - 530
  • [48] Phase-microstructure-property relationship in high quality factor MgO-Al2O3-SiO2-TiO2-La2O3 glass-ceramics
    Wang, Hui-Juan
    Zscheckel, Tilman
    Lin, Hui-Xing
    Li, Bo-Tao
    Ruessel, Christian
    Luo, Lan
    CERAMICS INTERNATIONAL, 2017, 43 (09) : 7073 - 7079
  • [49] Phase Evolution of SiO2-Al2O3-ZnO-CaO-ZrO2-TiO2-Based Glass with Added Y-PSZ Particles
    Wang, Xin
    Chen, Minghui
    Zhu, Shenglong
    Wang, Fuhui
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2013, 96 (05) : 1456 - 1463
  • [50] Microstructure and Strength of Al2O3/Al2O3 Joints Bonded with ZnO-Al2O3-B2O3-SiO2 Glass-Ceramic
    Zhu, Weiwei
    Chen, Jichun
    Hao, Chuanyong
    Zhang, Jinsong
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2014, 30 (09) : 944 - 948