Joining of textured PLS-SiC ceramic with CaO-Al2O3-MgO-TiO2-SiO2 glass filler

被引:3
|
作者
Zhan, Chuang-Tian [1 ]
Wu, Jin-Yuan [1 ]
Huang, Kun-Heng [1 ]
Li, Yun [2 ]
Wu, Li-Xiang [2 ]
He, Sheng-Jin [1 ]
Liu, Yang-Qing [1 ]
Zhang, Ze-Xi [1 ]
Guo, Wei-Ming [1 ]
Xue, Jia-Xiang [2 ]
Lin, Hua-Tay [1 ]
机构
[1] Guangdong Univ Technol, Sch Electromech Engn, Guangzhou 510006, Peoples R China
[2] China Nucl Power Technol Res Inst, Nucl Fuel & Mat Dept, Shenzhen 518026, Peoples R China
基金
中国国家自然科学基金;
关键词
SiC ceramic; Joining; Texture; Glass filler; Shear strength; SILICON-CARBIDE; CRYSTALLIZATION BEHAVIOR; BOROSILICATE GLASS; SHEAR-STRENGTH; COMPONENTS;
D O I
10.1016/j.ceramint.2023.10.125
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The pressureless-sintered silicon carbide ceramic with and without surface texturing was joined with CaO-Al2O3MgO-TiO2-SiO2 glass filler. The experimental results showed that without texturing applied to SiC substrates, the shear strength of SiC joints was 40.8 +/- 6.3 MPa, with failure occurring at the interlayer. Unfilled regions in the interlayer limited the shear strength of the joints. When texturing was applied to SiC substrates, SiO2 layer was formed on the surface of substrates due to high-temperature oxidation, which subsequently promoted the wettability of filler on substrates. The textured grooves on SiC substrates could be filled with glass material during joining process. The shear strength of textured SiC joints was 69.3 +/- 9.9 MPa with a mixed-mode failure when the direction of shear load was perpendicular to the texturing direction. The better wettability, larger joining area, and interlocking structure between the glass filler and substrates enhanced the shear strength of textured joints.
引用
收藏
页码:495 / 502
页数:8
相关论文
共 50 条
  • [31] The structure of model glasses of the amorphous phase of glass-ceramic glazes from the SiO2-Al2O3-CaO-MgO-Na2O-K2O-ZnO system
    Lesniak, Magdalena
    Jastrzebski, Witold
    Gajek, Marcin
    Partyka, Janusz
    Dorosz, Dominik
    Sitarz, Maciej
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2019, 515 : 125 - 132
  • [32] Effect of MgO/Al2O3 ratio on the crystallization behaviour of Li2O-MgO-Al2O3-SiO2 glass-ceramic and its wettability on Si3N4 ceramic
    Sun, Liangbo
    Fang, Jian
    Guo, Songsong
    Shan, Tipeng
    Wen, Yue
    Liu, Chunfeng
    Zhang, Jie
    CERAMICS INTERNATIONAL, 2022, 48 (14) : 20053 - 20061
  • [33] MgO-Al2O3-SiO2 Glass-Ceramic Prepared by Sol-Gel Method
    Yuan, Qiuhua
    Zhang, Peixin
    Gao, Li
    Peng, Hailin
    Ren, Xiangzhong
    Zhang, Dongyun
    POWDER TECHNOLOGY AND APPLICATION II, 2010, 92 : 131 - +
  • [34] Glass-ceramics in the CaO-MgO-Al2O3-SiO2 system as potential dental restorative materials
    Dimitriadis, Konstantinos
    Moschovas, Dimitrios
    Tulyaganov, Dilshat U.
    Agathopoulos, Simeon
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2021, 18 (06) : 1938 - 1949
  • [35] Effect of SiO2/Al2O3 ratio on the structure and electrical properties of MgO-Al2O3-SiO2 glass-ceramics doped with TiO2
    Li, Hao
    Yin, Zheyi
    Deng, Leibo
    Wang, Shuo
    Fu, Zhe
    Ma, Yonghong
    MATERIALS CHEMISTRY AND PHYSICS, 2020, 256 (256)
  • [36] Mixed alkali effect in SiO2-CaO-Al2O3-TiO2-R2O (R = Li, Na) glass ceramics
    Hou, Yong
    Zhang, Guo-Hua
    Chou, Kuo-Chih
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 856
  • [37] Computational Insight into the Thermal Conductivity of CaO-SiO2-Al2O3-MgO-Na2O Melts
    Wang, Zhe
    Huang, Shuheng
    Wen, Guanghua
    Jiang, Wenbo
    Tang, Ping
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2020, 51 (05): : 2391 - 2399
  • [38] Joining of SiC by tape-cast SiC-Al2O3-Y2O3 interlayer
    Tian, Wu-Bian
    Kita, Hideki
    Hyuga, Hideki
    Kondo, Naoki
    ADVANCED ENGINEERING CERAMICS AND COMPOSITES, 2011, 484 : 26 - 31
  • [39] Influences of additives on crystal multiformity and composition in a CaO-Al2O3-MgO-SiO2-based glass-ceramics
    Shi, Yu
    Song, Xiwen
    Han, Xiaoxing
    Zhang, Mingxing
    Dong, Mengyao
    ADVANCED COMPOSITES AND HYBRID MATERIALS, 2021, 4 (03) : 614 - 628
  • [40] Wear resistance glass-ceramics with a gahnite phase obtained in CaO-MgO-ZnO-Al2O3-B2O3-SiO2 system
    Herman, Daniela
    Okupski, Tomasz
    Walkowiak, Wieslaw
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2011, 31 (04) : 485 - 492