Effect of interfacial coatings on mechanical properties of 2.5D Nextel™ 720 fiber toughened zirconia-mullite matrix composites

被引:5
|
作者
Zhang, Zhuoke [1 ]
Yang, Lixia [1 ]
Chen, Zhaofeng [1 ]
Wang, Fei [1 ]
Huang, Rong [2 ]
Kou, Zongde [2 ]
机构
[1] Nanjing Univ Aeronaut & Astronaut, Coll Mat Sci & Technol, 29 Yudao St, Nanjing 210016, Peoples R China
[2] Nanjing Univ Sci & Technol, Herbert Gleiter Inst Nanosci, Sch Mat Sci & Engn, Nanjing 210094, Peoples R China
基金
中国国家自然科学基金;
关键词
Ceramic matrix composites(CMCs); NextelTM; 720; fibers; Mullite; Mechanical properties; Yttria-stabilized zirconia(YSZ); Precursor infiltration and pyrolysis (PIP); NEXTEL(TM)720/ALUMINA CERAMIC COMPOSITE; THERMAL-EXPANSION COEFFICIENT; YTTRIA-STABILIZED ZIRCONIA; VOLUME FRACTION; CREEP-BEHAVIOR; TEMPERATURE; MICROSTRUCTURE; FLUORESCENCE; ORIENTATION; DEPOSITION;
D O I
10.1016/j.matchar.2023.113381
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, 2.5D bent shallow cross-linked structure NextelTM 720 (N720) fiber-reinforced yttria-stabilized zirconia-mullite composites with pyrolytic carbon (PyC) and fugitive pyrolytic carbon (FC) interfacial coatings were prepared by using a precursor infiltration and pyrolysis approach (called as N720f/PyC/YSZ-Mu and N720f/ FC/YSZ-Mu, respectively). The effects of PyC and FC coatings on the failure mechanisms and mechanical properties of the composites were investigated. The N720f/PyC/YSZ-Mu composite shows ductile fracture behavior while the N720f/FC/YSZ-Mu composite shows brittle fracture behavior. The fracture toughness and flexural strength of the N720f/PyC/YSZ-Mu composite reach -7.00 MPa center dot m1/2 and - 120.79 MPa, respectively. In contrast, the corresponding properties of the N720f/FC/YSZ-Mu composite are -3.66 MPa center dot m1/2 and - 59.02 MPa, respectively. Microstructure analysis indicates that the weak PyC interfacial layer contributes to toughening by promoting fiber pull-out and debonding, thus enhancing the mechanical properties of the N720f/PyC/ YSZ-Mu composite. The retrogression of the mechanical properties of the N720f/FC/YSZ-Mu composite originates from the damage to N720 fibers during the preparation procedure. This paper provides a new idea for the development of high-performance oxide CMCs with a 2.5D structure.
引用
收藏
页数:11
相关论文
共 50 条
  • [31] Effects of sintering temperature on mechanical properties of 3D mullite fiber (ALF FB3) reinforced mullite composites
    Wang, Yi
    Cheng, Haifeng
    Liu, Haitao
    Wang, Jun
    CERAMICS INTERNATIONAL, 2013, 39 (08) : 9229 - 9235
  • [32] The effect of fabrication processes on the mechanical and interfacial properties of SiCf/Cu-matrix composites
    Luo Xian
    Yang Yanqing
    Li Jiankang
    Mei Yuanwang
    Yuan Meini
    Chen Yan
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2007, 38 (10) : 2102 - 2108
  • [33] Effect of graphene dispersion and interfacial bonding on the mechanical properties of metal matrix composites: An overview
    Ghodrati, Hanieh
    Ghomashchi, Reza
    FLATCHEM, 2019, 16
  • [34] Effect of interfacial debonding and matrix cracking on mechanical properties of multidirectional composites
    Rao, M. Venkat
    Mahajan, P.
    Mittal, R. K.
    COMPOSITE INTERFACES, 2008, 15 (04) : 379 - 409
  • [35] Effect of La2O3 Addition on the Thermal, Microstructure and Mechanical Properties of Mullite-Zirconia Composites
    Aydin, H.
    IRANIAN JOURNAL OF MATERIALS SCIENCE AND ENGINEERING, 2019, 16 (04) : 10 - 19
  • [36] Comparison of Physico-mechanical Properties of TiO2 and Cr2O3 Additives on Reaction Sintered Zirconia-mullite Composites
    Debasish CHANDRA
    China'sRefractories, 2019, 28 (01) : 11 - 21
  • [37] Interfacial mechanical properties of carbon nanotube-deposited carbon fiber epoxy matrix hierarchical composites
    Awan, Faizan S.
    Fakhar, Mohsin A.
    Khan, Laraib A.
    Zaheer, Usama
    Khan, Abdul F.
    Subhani, Tayyab
    COMPOSITE INTERFACES, 2018, 25 (08) : 681 - 699
  • [38] Effect of graphene and CNFs addition on the mechanical and electrical properties of dense alumina-toughened zirconia composites
    Rincon, Acacio
    Moreno, Rodrigo
    Chinelatto, Adriana S. A.
    Gutierrez, Carlos F.
    Dolores Salvador, Maria
    Borrell, Arnparo
    CERAMICS INTERNATIONAL, 2016, 42 (01) : 1105 - 1113
  • [39] Mechanical properties and microstructure of 2.5D (shallow straight-joint) quartz fibers-reinforced silica composites by silicasol-infiltration-sintering
    Liu, Yong
    Zhu, Jianxun
    Chen, Zhaofeng
    Jiang, Yun
    Li, Chengdong
    Li, Binbin
    Lin, Long
    Guan, Tianru
    Chen, Zhaohai
    CERAMICS INTERNATIONAL, 2012, 38 (01) : 795 - 800
  • [40] Effect of water and fiber length on the mechanical properties of polypropylene matrix composites
    N. Ferreira
    C. Capela
    J. M. Ferreira
    J. M. Costa
    Fibers and Polymers, 2014, 15 : 1017 - 1022