Wear behavior of ceramic, composite, and ceramic/composite interfaces

被引:0
作者
Yildirim, Elif Sevilay [1 ]
Tekce, Neslihan [2 ]
Fidan, Sinan [3 ]
Tuncer, Safa [4 ]
Demirci, Mustafa [4 ]
机构
[1] Dis Sagligi Merkezi, Dept Restorat Dent, Sancaktepe Agizve, Istanbul, Turkiye
[2] Kocaeli Univ, Fac Dent, Dept Restorat Dent, Kocaeli, Turkiye
[3] Kocaeli Univ, Fac Aeronaut & Astronaut, Dept Airframe & Powerplant, Kocaeli, Turkiye
[4] Istanbul Univ, Fac Dent, Dept Restorat Dent, Istanbul, Turkiye
关键词
CAD; CAM; surface roughness; brushing abrasion; repair; SURFACE-ROUGHNESS; RESIN COMPOSITES; TOOTHBRUSH ABRASION; REPAIR; ZIRCONIA; GLOSS; STABILITY;
D O I
10.1088/2051-672X/acd5e9
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Objective. This study has aimed to evaluate the effects of toothbrushing on the wear behavior of two composites, three ceramic materials, and ceramic/composite interfaces. Material and Methods. Nanofilled (Filtek Ultimate), and nanohybrid composites (Spectra ST HV) were used for the repair of a hybrid ceramic (Vita Enamic), resin nanoceramic (Katana Avencia), and zirconia block (Katana Zirconia). Composites, ceramics, and ceramic/composite interfaces were examined before and after a period of one-month and one-year of toothbrush abrasion testing using non-contact optical profilometry and scanning electron microscopy (SEM). Data were analyzed by two-way ANOVA and Bonferroni correction. The statistical significance level was set at p < 0.05. Results. No difference was found between the surface roughness of the Vita Enamic, Katana Avencia, Filtek Ultimate, and Spectra surfaces after one month and one year of toothbrushing. Sa values in Katana Zirconia material were found to be significantly lower than those in the control group after one year of brushing. The surface roughness of the repair interfaces formed by repairing hybrid ceramic and resin nanoceramic CAD/CAM materials with nanofilled and nanohybrid composite materials was found to be similar after different brushing times. Conclusion. Vita Enamic, Katana Avencia, Filtek Ultimate, and Spectra materials can be preferred in clinical repair applications, since they exhibit similar wear behavior after brushing at different times. For the zirconia material, the repair interface had similar surface roughness as the ceramic and composite surfaces after one year of brushing. Periodic recalls and re-polishing may thus be necessary when these products are used clinically.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] Cutting performance and wear mechanisms of Sialon–Si3N4 graded nano-composite ceramic cutting tools
    Guangming Zheng
    Jun Zhao
    Zhongjun Gao
    Qingyuan Cao
    The International Journal of Advanced Manufacturing Technology, 2012, 58 : 19 - 28
  • [42] Cutting performance and wear mechanisms of Sialon-Si3N4 graded nano-composite ceramic cutting tools
    Zheng, Guangming
    Zhao, Jun
    Gao, Zhongjun
    Cao, Qingyuan
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2012, 58 (1-4) : 19 - 28
  • [43] Creep Behavior in Interlaminar Shear of a SiC/SiC Ceramic Composite with a Self-healing Matrix
    Ruggles-Wrenn, M. B.
    Pope, M. T.
    APPLIED COMPOSITE MATERIALS, 2014, 21 (01) : 213 - 225
  • [44] Polish of interface areas between zirconia, silicate-ceramic, and composite with diamond-containing systems
    Pott, Philipp-Cornelius
    Hoffmann, Johannes Philipp
    Stiesch, Meike
    Eisenburger, Michael
    JOURNAL OF ADVANCED PROSTHODONTICS, 2018, 10 (04) : 315 - 320
  • [45] Comparison of EDG, Diamond Grinding, and EDM Processing of Conductive Alumina Ceramic Composite
    Satyarthi, M. K.
    Pandey, Pulak M.
    MATERIALS AND MANUFACTURING PROCESSES, 2013, 28 (04) : 369 - 374
  • [46] Some observations in grinding SiC and silicon carbide ceramic matrix composite material
    Gong, Yadong
    Qu, Shuoshuo
    Yang, Yuying
    Liang, Chunyou
    Li, Pengfei
    She, Yuebing
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 103 (5-8) : 3175 - 3186
  • [47] Some observations in grinding SiC and silicon carbide ceramic matrix composite material
    Yadong Gong
    Shuoshuo Qu
    Yuying Yang
    Chunyou Liang
    Pengfei Li
    Yuebing She
    The International Journal of Advanced Manufacturing Technology, 2019, 103 : 3175 - 3186
  • [48] Surface and subsurface study on EDG and EDM processing of advanced ceramic composite material
    Satyarthi, M. K.
    Pandey, Pulak M.
    PROCEEDINGS OF THE ASME INTERNATIONAL MECHANICAL ENGINEERING CONGRESS AND EXPOSITION, 2013, VOL 2B, 2013,
  • [49] Extrusion behavior of metal-ceramic composite pipes in multi-billet extrusion process
    Chen, ZC
    Ikeda, K
    Murakami, T
    Takeda, T
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2001, 114 (02) : 154 - 160
  • [50] EVALUATION OF SURFACE ROUGHNESS AND ELASTIC MODULUS IN CERAMIC AND RESIN COMPOSITE CAD/CAM MATERIALS DURING AGEING
    Bai, Yunyang
    Yuan, Shenpo
    Wu, Jiaqi
    CERAMICS-SILIKATY, 2021, 65 (01) : 24 - 29