Shade match comparison of CAD-CAM single crowns to a lithium disilicate crown

被引:1
作者
Li, Rui [1 ]
Lin, Yu-Chun [2 ]
Sadid-Zadeh, Ramtin [1 ,3 ]
机构
[1] Univ Buffalo, Dept Restorat Dent, Sch Dent Med, Buffalo, NY USA
[2] Augusta Univ, Dept Restorat Sci, Dent Coll Georgia, Augusta, GA USA
[3] Univ Buffalo, Dept Restorat Dent, Sch Dent Med, 222 Squire Hall, Buffalo, NY 14214 USA
来源
JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY | 2024年 / 33卷 / 03期
关键词
all-ceramic crown; shade assessment; shade match; spectrophotometer; IN-VITRO; ZIRCONIA; COLOR; TRANSLUCENCY; RESTORATIONS; THICKNESS; STRENGTH;
D O I
10.1111/jopr.13676
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
PurposeTo assess the shade match ability of four varieties of all-ceramic crowns to a neighboring bilayered lithium disilicate crown. Material and methodsA dentiform was used to fabricate a bilayered lithium disilicate crown on the maxillary right central incisor, following the anatomy and shade of a selected natural tooth. Two crowns (one full-contour, one cutback) were then designed on a prepared maxillary left central incisor, following the contour of the neighboring crown. The designed crowns were used to manufacture monolithic lithium disilicate, bilayered lithium disilicate, bilayered zirconia, and monolithic zirconia crowns, 10 each. An intraoral scanner and a spectrophotometer were used to assess the frequency of matched shades and to calculate the color difference (Delta E) between the two central incisors at the incisal, middle, and cervical thirds. Kruskal-Wallis and two-way ANOVA were used to compare the frequency of matched shades and Delta E values, respectively (alpha = 0.05). ResultsThere was no significant (p > 0.05) difference in frequencies of matched shades for each group at the three sites; except bilayered lithium disilicate crowns. Bilayered lithium disilicate crowns had significantly (p < 0.05) higher match frequency than monolithic zirconia at the middle third. The Delta E value was not significantly (p > 0.05) different among the groups at the cervical third. However, monolithic zirconia had significantly (p < 0.05) higher Delta E values than bilayered lithium disilicate and zirconia at the incisal and middle thirds. ConclusionsBilayered lithium disilicate and zirconia appeared to most closely match the shade of an existing bilayered lithium disilicate crown.
引用
收藏
页码:246 / 251
页数:6
相关论文
共 50 条
  • [41] Effect of brushing and thermocycling on the shade and surface roughness of CAD-CAM ceramic restorations
    Yuan, Judy Chia-Chun
    Barao, Valentim Adelino Ricardo
    Wee, Alvin G.
    Alfaro, Maria F.
    Afshari, Fatemeh S.
    Sukotjo, Cortino
    JOURNAL OF PROSTHETIC DENTISTRY, 2018, 119 (06) : 1000 - 1006
  • [42] Fracture resistance of endodontically treated premolars restored with lithium disilicate CAD/CAM crowns or onlays and luted with two luting agents
    Yu, Weiqiang
    Guo, Kewu
    Zhang, Baowei
    Weng, Weimin
    DENTAL MATERIALS JOURNAL, 2014, 33 (03) : 349 - 354
  • [43] In vitro analysis of the fracture resistance of CAD-CAM monolithic zirconia molar crowns with different occlusal thickness
    Sorrentino, Roberto
    Triulzio, Clementina
    Tricarico, Maria Gabriella
    Bonadeo, Giovanni
    Gherlone, Enrico Felice
    Ferrari, Marco
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2016, 61 : 328 - 333
  • [44] Fracture load of chairside CAD-CAM veneers fabricated with pre-and fully crystalized lithium disilicate ceramics
    Jurado, Carlos A.
    Yeh, Jacquelyn S.
    Vidal, Cristina M. P.
    Cho, Seok-Hwan
    Abuhammoud, Salahaldeen
    JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2024,
  • [45] CAD-CAM milled versus pressed lithium-disilicate monolithic crowns adhesively cemented after distinct surface treatments: Fatigue performance and ceramic surface characteristics
    Schestatsky, Ricardo
    Zucuni, Camila Pauleski
    Venturini, Andressa Borin
    de Lima Burgo, Thiago Augusto
    Bacchi, Atais
    Valandro, Luiz Felipe
    Rocha Pereira, Gabriel Kalil
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2019, 94 : 144 - 154
  • [46] Impact of Thermal Aging on Marginal Adaptation in Lithium Disilicate CAD/CAM Crowns with Deep Proximal Box Elevation
    Daghrery, Arwa
    Jabarti, Eman
    Mitwalli, Heba
    Moaleem, Mohammed M. Al
    Khojah, Maysaa Z.
    Khayat, Waad
    Albar, Nassreen H.
    MEDICAL SCIENCE MONITOR, 2025, 31
  • [47] Evaluation and Comparison of Mechanical Properties of Lithium Disilicate-Based CAD/CAM Blocks
    Zulkiffli, Sofya
    Take, Yeoh Oon
    Yahya, Noor Azlin
    Kutty, Muralithran Govindan
    SAINS MALAYSIANA, 2024, 53 (01): : 217 - 229
  • [48] Impact of liner treatment on the translucency of CAD/CAM multi-colored lithium disilicate and multi-layered zirconia implant-supported crowns, and evaluation of fracture strength of ceramic crowns
    Kim, Ji-Hyun
    Byeon, Seon-Mi
    Bae, Tae-Sung
    Jang, Yong-Seok
    Lee, Min-Ho
    Ahn, Seung-Geun
    ODONTOLOGY, 2025, 113 (02) : 645 - 654
  • [49] Fracture resistance of CAD-CAM monolithic ceramic and veneered zirconia molar crowns after aging in a mastication simulator
    Gungor, Merve Bankoglu
    Nemli, Secil Karakoca
    JOURNAL OF PROSTHETIC DENTISTRY, 2018, 119 (03) : 473 - 480
  • [50] Polishing the bonding surface, before or after crystallization, does not alter the fatigue behavior of bonded CAD-CAM lithium disilicate
    Pilecco, Rafaela Oliveira
    Zucuni, Camila Pauleski
    de Carvalho, Ana Beatriz Gomes
    Saavedra, Guilherme de Siqueira Ferreira Anzaloni
    Marinho, Renata Marques de Melo
    Pereira, Gabriel Kalil Rocha
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2023, 142