A novel method of enhancing valuable element recovery for ultra-high-titanium magnetite

被引:6
作者
Cheng, Gongjin [1 ,2 ,3 ,4 ]
Han, Tong [1 ]
Zhang, Xuefei [1 ]
Xue, Xiangxin [1 ,2 ,3 ,4 ]
Yang, He [1 ,2 ,3 ,4 ]
Bai, Ruiguo [5 ]
Zhang, Weijun [1 ]
机构
[1] Northeastern Univ, Sch Met, Shenyang 110819, Peoples R China
[2] Liaoning Key Lab Recycling Sci Met Resources, Shenyang 110819, Peoples R China
[3] Northeastern Univ, Innovat Res Inst Vanadium & Titanium Resource Ind, Shenyang 110819, Peoples R China
[4] Innovat Res Inst Comprehens Utilizat Technol Vanad, Chaoyang 122000, Peoples R China
[5] HBIS Grp ChengSteel, Chengde 067102, Peoples R China
基金
中国国家自然科学基金;
关键词
Ultra-high-titanium magnetite; Diboron trioxide; Metallization reduction-magnetic separation; Recovery ratio; VANADIUM TITANOMAGNETITE; SMELTING MECHANISM; CRUSHING STRENGTH; REDUCTION; CHROMIUM; IRON; B2O3; SEPARATION; BEHAVIOR; KINETICS;
D O I
10.1016/j.jclepro.2023.137184
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
The metallization reduction-magnetic separation process was adopted to carry out the experiments to promote the recovery ratio of valuable elements by adding diboron trioxide additive in this work. It is demonstrated that diboron trioxide has the function of destroying Si-O-Si bond for the reduction of ultra-high-titanium magnetite. The optimum experimental condition is found to be the reduction temperature of 1125 degrees C, the reduction time of 30min, and the diboron trioxide percent of 8 wt% for which the metallization ratio is 92%, and the recovery ratio of ferrum, vanadium, titanium is 90.9%, 78.5%, 76.1%, respectively. V and Ti are synchronously concentrated in non-magnetic materials. The phase composition transformation rule of the valuable components was Fe3O4 (FeTiO3) -> FeO -> Fe; FeTiO3 (-> FeTi2O5) -> (Fe,Mg)Ti2O5; FeTiO3 -> TiO2 -> Ti3O5 -> Ti2O3; (Fe3O4 + TiO2) -> Fe3Ti3O10 -> Fe. Increasing the temperature can promote the aggregation and growth of iron particles, but too high temperature is not conducive to the separation of Fe, V and Ti. It is evidently observed that when the temperature exceeds 1150 degrees C, the iron particles are closely connected with the gray titanium oxide, while at 1125 degrees C, the iron particles are relatively independent. Meanwhile, part of Ti is observed in silicate phase as solid-dissolved form because of high temperature and cause loss. Overall speaking, the metallization reduction-magnetic separation process with diboron trioxide as an additive has achieved the better separation of valu-able components, with a higher degree of metallization, and large-scale lowered reaction temperature and time.
引用
收藏
页数:11
相关论文
共 34 条
  • [1] Non-isothermal reduction mechanism and kinetics of high chromium vanadium-titanium magnetite pellets
    Cheng, G. -J.
    Liu, J. -X.
    Liu, Z. -G.
    Chu, M. -S.
    Xue, X. -X.
    [J]. IRONMAKING & STEELMAKING, 2015, 42 (01) : 17 - 26
  • [2] Effect of diboron trioxide on the crushing strength and smelting mechanism of high-chromium vanadium-titanium magnetite pellets
    Cheng, Gong-jin
    Gao, Zi-xian
    Yang, He
    Xue, Xiang-xin
    [J]. INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2017, 24 (11) : 1228 - 1240
  • [3] Coal-Based Reduction and Magnetic Separation Behavior of Low-Grade Vanadium-Titanium Magnetite Pellets
    Cheng, Gongjin
    Gao, Zixian
    Lv, Mengyang
    Yang, He
    Xue, Xiangxin
    [J]. MINERALS, 2017, 7 (06):
  • [4] Effect of TiO2 on the Crushing Strength and Smelting Mechanism of High-Chromium Vanadium-Titanium Magnetite Pellets
    Cheng, Gongjin
    Xue, Xiangxin
    Jiang, Tao
    Duan, Peining
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2016, 47 (03): : 1713 - 1726
  • [5] Effect of B2O3 on physical properties of LZAS vitrified bond and mechanical properties of diamond composites
    Cui, Lei
    Hao, Xiaojun
    Tang, Yu
    Zheng, Zhanghong
    Yuan, Yuxing
    Lu, Anxian
    [J]. INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2015, 52 : 50 - 54
  • [6] Department of Inorganic Chemistry Dalian University of Technology, 2018, INORG CHEM
  • [7] Du H., 1996, PRINCIPLE SMELTING V, V1st
  • [8] A novel recycling approach for efficient extraction of titanium from high-titanium-bearing blast furnace slag
    Fan, Gangqiang
    Wang, Meng
    Dang, Jie
    Zhang, Run
    Lv, Zepeng
    He, Wenchao
    Lv, Xuewei
    [J]. WASTE MANAGEMENT, 2021, 120 : 626 - 634
  • [9] Effects of smelting parameters on the slag/metal separation behaviors of Hongge vanadium-bearing titanomagnetite metallized pellets obtained from the gas-based direct reduction process
    Feng, Cong
    Chu, Man-sheng
    Tang, Jue
    Liu, Zheng-gen
    [J]. INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2018, 25 (06) : 609 - 622
  • [10] Gao Z., 2021, THESIS NE U SHENYANG