Durability of internally cured concrete with silicon-aluminum based fine lightweight aggregate exposed to combined sulfate and wetting-drying attack

被引:1
作者
Zhang, Yating [1 ]
Lin, Jiaheng [1 ]
Fan, Ziwei [1 ]
Zhu, Xingyi [2 ]
机构
[1] Jiangnan Univ, Sch Environm & Civil Engn, Wuxi 214122, Peoples R China
[2] Tongji Univ, Key Lab Rd & Traff Engn, Minist Educ, Shanghai 200092, Peoples R China
基金
中国国家自然科学基金;
关键词
Internally cured concrete; Silicon-aluminum based fine lightweight aggregate; Durability; Sulfate attack; Wetting-drying protocols; AUTOGENOUS SHRINKAGE; HYDRATION; WATER; MICROSTRUCTURE; TEMPERATURE; PREVENTION; EFFICIENCY; CEMENTS; POWDER; SLAG;
D O I
10.1617/s11527-023-02261-2
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The durability of internally cured concrete (ICC) with silicon-aluminum based fine lightweight aggregate (FLWA) exposed to combined sulfate and wetting-drying attack were conducted through evaluating concrete mass, relative dynamic elastic moduli (RDEM), flexural strength, microstructure and erosion products, with the consideration of various FLWA contents, w/b ratios, volcanic minerals and wetting-drying protocols. Results showed that ICC containing 30% FLWA presented better sulfate resistance with less reduction in mass, RDEM and flexural strength since the internal curing and pozzolanic effect of the silicon-aluminum based FLWA contributed to a denser microstructure. Unfortunately, concrete durability decreased when the FLWA content increased to 60%. A higher w/b ratio of 0.55 weakened the sulfate resistance of ICC given a decrease of up to 0.37%, 4.07% and 24.49% in mass, RDEM and flexural strength, respectively, after 210-day attack. More erosion products as well as a higher strength loss were observed as fly ash content increased to 20%. Adding 10% blast furnace slag improved ICC's durability with an enhancement of 2.55% in flexural strength under 210 days of attack. An 80 degrees C-drying temperature speeded up ICC's deterioration with a strength loss of 83.41% at 168 days, and it also changed the damage mechanism by decomposing erosion products. An accelerated degradation process can be expected in the long-term given a drying temperature of 40 degrees C, which can be adopted as an erosion accelerator, despite it benefited the concrete durability at the early attack age.
引用
收藏
页数:14
相关论文
共 48 条
[1]   Effects of distribution of lightweight aggregates on internal curing of concrete [J].
Akcay, Burcu ;
Tasdemir, Mehmet Ali .
CEMENT & CONCRETE COMPOSITES, 2010, 32 (08) :611-616
[2]   Mechanical properties and durability of high-performance concrete internally cured using lightweight aggregates [J].
Alaskar, Abdulaziz ;
Alshannag, Mohammad ;
Higazey, Mahmoud .
CONSTRUCTION AND BUILDING MATERIALS, 2021, 288
[3]   Biphasic carbonation behaviour of structural lightweight aggregate concrete produced with different types of binder [J].
Alexandre Bogas, J. ;
Real, Sofia ;
Ferrer, Beatriz .
CEMENT & CONCRETE COMPOSITES, 2016, 71 :110-121
[4]   Influence of temperature and salt concentration on the salt weathering of a sedimentary stone with sodium sulphate [J].
Angeli, M. ;
Hebert, R. ;
Menendez, B. ;
David, C. ;
Bigas, J-P .
ENGINEERING GEOLOGY, 2010, 115 (3-4) :193-199
[5]  
[Anonymous], 2020, Testing Methods of Cement and Concrete for Highway Engineering
[6]  
[Anonymous], 2002, JGJ512002 MIN CONSTR
[7]  
[Anonymous], 2009, GB/T 50082-2009
[8]   Prevention of autogenous shrinkage in high-strength concrete by internal curing using wet lightweight aggregates [J].
Bentur, A ;
Igarashi, S ;
Kovler, K .
CEMENT AND CONCRETE RESEARCH, 2001, 31 (11) :1587-1591
[9]   Influence of internal curing and viscosity modifiers on resistance to sulfate attack [J].
Bentz, Dale P. ;
Davis, Jeffrey M. ;
Peltz, Max A. ;
Snyder, Kenneth A. .
MATERIALS AND STRUCTURES, 2014, 47 (04) :581-589
[10]   The effect of fineness on the properties of the blended cements incorporating ground granulated blast furnace slag and ground basaltic pumice [J].
Binici, Hanifi ;
Temiz, Huseyin ;
Kose, Mehmet M. .
CONSTRUCTION AND BUILDING MATERIALS, 2007, 21 (05) :1122-1128