White etching area damage induced by shear localization in rolling contact fatigue of bearing steel

被引:5
作者
Chen, Jin-Hua [1 ]
Xie, Chao [1 ,3 ]
Li, Shu-Xin [1 ,2 ,4 ]
Lu, Si-Yuan [1 ,2 ]
机构
[1] Ningbo Univ, Sch Mech Engn & Mech, Key Lab Impact & Safety Engn, Minist Educ, Ningbo, Peoples R China
[2] Ningbo Univ, Key Lab Part Rolling Zhejiang Prov, Ningbo, Peoples R China
[3] Ningbo Univ, Sch Mech Engn & Mech, Key Lab Impact & Safety Engn, Minist Educ, Ningbo 315211, Peoples R China
[4] Ningbo Univ, Key Lab Part Rolling Zhejiang Prov, Ningbo 315211, Peoples R China
基金
中国国家自然科学基金;
关键词
plastic strain accumulation; rolling contact fatigue; shear band; strain localization; white etching areas (WEAs); MICROSTRUCTURAL ALTERATIONS; NONMETALLIC INCLUSIONS; CRACKS WECS; MATTER; MECHANISM; FAILURE; STRESS; TRANSFORMATION; AMORPHIZATION; INITIATION;
D O I
10.1111/ffe.14182
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
White etching area (WEA) is a primary damage in rolling contact fatigue (RCF) of bearing steels. In spite of extensive investigations, there is a large discrepancy in the existing mechanisms of WEA formation. We attempt to unify the mechanisms from the perspective of shear localization and plastic damage accumulation based on ductile damage. RCF tests were conducted to generate WEAs with various microstructures and compositions. A thermodynamically consistent model of the ductile damage evolution from an inclusion was established by developing the phase field damage coupled with the crystal elastic-viscoplastic constitutive relationship under RCF. The model was implemented into the FE framework through a user materials subroutine. The results indicated that the WEA is the shear band resulting from shear localization. The large inhomogeneity and scatter in WEA's microstructure are due to the influence of the crystal orientation. The development and orientation of SBs predicted by the model and the experimental observation of the WEA are in good agreement. The large micro-shear strain in the WEA provides the driving force for mechanically controlled austenite phase transformation. The shear band center, which has the largest strain and the least stress, is where cracks initiate. This demonstrates that contrary to earlier reports that WEA is induced by previously formed crack faces friction, cracks actually initiate from the interior of the WEA.
引用
收藏
页码:170 / 186
页数:17
相关论文
共 50 条
[41]   Rolling contact fatigue resistance and damage evolution of carburized bearing steel treated by surface ultrasonic rolling process (SURP) [J].
Zhu, Xiaotong ;
Pan, Jinzhi ;
Liu, Deyi ;
Zhao, Xiujuan ;
Ren, Ruiming .
WEAR, 2023, 524
[42]   Modelling of surface initiated rolling contact fatigue damage [J].
Hannes, Dave ;
Alfredsson, Bo .
FATIGUE DESIGN 2013, INTERNATIONAL CONFERENCE PROCEEDINGS, 2013, 66 :766-774
[43]   A new damage-mechanics-based model for rolling contact fatigue analysis of cylindrical roller bearing [J].
Li, Fukai ;
Hu, Weiping ;
Meng, Qingchun ;
Zhan, Zhixin ;
Shen, Fei .
TRIBOLOGY INTERNATIONAL, 2018, 120 :105-114
[44]   A novel oxide layer for achieving ultra-high rolling contact fatigue life of bearing steel [J].
Xia, Zhuofan ;
Wu, Di ;
Hao, Long ;
Li, Yifeng ;
Wang, Jianqiu ;
Han, En-Hou .
TRIBOLOGY INTERNATIONAL, 2025, 207
[45]   Micromechanical response of dual-hardening martensitic bearing steel before and after rolling contact fatigue [J].
Loaiza, Tania ;
Fischer, Tim ;
Babu, Revathy Prasath ;
Hedstrom, Peter .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 29 :4728-4734
[46]   Effect of lubricants on bearing damage in rolling-sliding conditions: Evolution of white etching cracks [J].
Paladugu, Mohanchand ;
Lucas, Douglas R. ;
Hyde, R. Scott .
WEAR, 2018, 398 :165-177
[47]   Rolling contact fatigue of white etching layer: Part 1 - Crack morphology [J].
Carroll, R. I. ;
Beynon, J. H. .
WEAR, 2007, 262 (9-10) :1253-1266
[48]   Reproduction of white etching cracks under rolling contact loading on thrust bearing and two-disc test rigs [J].
Guzman, F. Gutierrez ;
Oezel, M. ;
Jacobs, G. ;
Burghardt, G. ;
Broeckmann, C. ;
Janitzky, T. .
WEAR, 2017, 390-391 :23-32
[49]   Rolling Contact Fatigue Behaviors of High Carbon Bainitic Bearing Steel [J].
Zheng C. ;
She L. ;
Wang Y. ;
Yang Z. ;
Zhang F. .
Jixie Gongcheng Xuebao/Journal of Mechanical Engineering, 2017, 53 (24) :110-117
[50]   Influence of Cu nanofluids on the rolling contact fatigue life of bearing steel [J].
Thapliyal, Prashant ;
Thakre, Gananath D. .
ENGINEERING FAILURE ANALYSIS, 2017, 78 :110-121