Diaminoalkanes functionalized graphene oxide as corrosion inhibitors against carbon steel corrosion in simulated oil/gas well acidizing environment

被引:42
作者
Saleh, Tawfik A. [1 ]
Haruna, Kabiru [1 ,3 ]
Alharbi, Bader [2 ]
机构
[1] King Fahd Univ Petr & Minerals, Dept Chem, Dhahran 31261, Saudi Arabia
[2] Saudi Aramco, EXPEC Adv Res Ctr, Dhahran 31311, Saudi Arabia
[3] King Fahd Univ Petr & Minerals, Interdisciplinary Res Ctr Adv Mat, Dhahran 31261, Saudi Arabia
关键词
Acidizing; Waste graphite; Corrosion; TEM; Molecular Electrostatic Potential (MEP); MILD-STEEL; THERMAL-STABILITY; ADSORPTION; RESISTANCE; HCL; SPECTROSCOPY; DERIVATIVES; COATINGS; BEHAVIOR; CHLORIDE;
D O I
10.1016/j.jcis.2022.10.054
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Experimental weight loss and electrochemical measurements were used at ambient and high tempera-tures to evaluate the corrosion inhibition efficacies of diaminodecane functionalized graphene oxide (DAD-GO) and diaminododecane functionalized graphene oxide (DADD-GO) against carbon steel corro-sion in 15.0 % HCl, mimicking an acidizing environment in an oil/gas well. The GO was made from waste graphite and then grafted with the diaminoalkanes (DAD & DADD). The GO and functionalized GOs were described using FTIR, Raman, TEM, and TGA. Concentration and temperature effects on the inhibitors' performance were also looked into. The inhibition efficiency increased with concentration at room temperature, reaching a maximum of 84 % for DAD-GO and 78 % for DADD-GO at a concentration of 5 ppm for both. At the temperatures studied, the inhibitors performed well at extremely low concen-trations; however, as the temperature rises, the inhibitor's performance decreases. According to the PDP measurement, the inhibitors function primarily as mixed-type inhibitors. The Langmuir adsorption the-ory was found to be followed by the studied compound. AFM, SEM, EDX, and FTIR characterization of the steel surfaces revealed that the functionalized GOs molecules adsorbed on the steel to create a protective layer that insulated the steel from aggressive acid assault after the immersion time (24 h) in the inhibited solutions. DFT calculations were utilized to determine the relative stability of functionalized GOs to GO and to learn more about the inhibitor molecules' interactions with the steel surface. The DFT cal-culations corroborated the experimental findings. This study is important in tackling two significant envi-ronmental concerns: corrosion and waste management because GO is manufactured from waste graphite.(c) 2022 Elsevier Inc. All rights reserved.
引用
收藏
页码:591 / 610
页数:20
相关论文
共 50 条
  • [31] Corrosion Inhibition Performance of Composite Inhibitors for Carbon Steel in Simulated Seawater
    Liu, Fenzhao
    JOURNAL OF COASTAL RESEARCH, 2019, : 397 - 403
  • [32] Inhibition Effect of Environment-Friendly Inhibitors on the Corrosion of Carbon Steel in Recirculating Cooling Water
    He, Chengjun
    Tian, Zhipeng
    Zhang, Bingru
    Lin, Yu
    Chen, Xi
    Wang, Meijing
    Li, Fengting
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2015, 54 (07) : 1971 - 1981
  • [33] Comparison of the synergistic inhibition mechanism of two eco-friendly amino acids combined corrosion inhibitors for carbon steel pipelines in oil and gas production
    Zhang, Q. H.
    Li, Y. Y.
    Lei, Y.
    Wang, X.
    Liu, H. F.
    Zhang, G. A.
    APPLIED SURFACE SCIENCE, 2022, 583
  • [34] Aryl Aminoalcohols as Corrosion Inhibitors for Carbon Steel in Chloride-Contaminated Simulated Concrete Pore Solution
    Liu, J. Z.
    Zhao, D.
    Cai, J. S.
    Shi, L.
    Liu, J. P.
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2016, 11 (02): : 1135 - 1151
  • [35] Cardiospermum halicacabum leaves extract as a green corrosion inhibitor for mild steel in simulated oil well water medium
    Kavitha, K.
    Benitasherine, H.
    Rajendran, S.
    INTERNATIONAL JOURNAL OF CORROSION AND SCALE INHIBITION, 2021, 10 (04): : 1646 - 1660
  • [36] Corrosion Behavior of Coated Low Carbon Steel in a Simulated PEMFC Environment
    Avram, Diana Nicoleta
    Davidescu, Corneliu Mircea
    Hulka, Iosif
    Dan, Mircea Laurentiu
    Stanciu, Elena Manuela
    Pascu, Alexandru
    Mirza-Rosca, Julia Claudia
    MATERIALS, 2023, 16 (08)
  • [37] Carbon Dots as Environment-Friendly and Efficient Corrosion Inhibitors for Q235 Steel in 1 M HCl
    Pan, Liang
    Li, Guoxi
    Wang, Zhaoyang
    Liu, Dongbao
    Zhu, Weikang
    Tong, Chunyi
    Zhu, Rilong
    Hu, Shilin
    LANGMUIR, 2021, 37 (49) : 14336 - 14344
  • [38] The impact of minor Cr additions in low alloy steel on corrosion behavior in simulated well environment
    Gupta, Kapil K.
    Haratian, Saber
    Mishin, Oleg V.
    Ambat, Rajan
    NPJ MATERIALS DEGRADATION, 2023, 7 (01)
  • [39] Surface protection of steel in oil well acidizing fluids using L-theanine-based corrosion inhibitor formulations: Experimental and theoretical evaluation
    Ituen, Ekemini
    Mkpenie, Victor
    Dan, Emmanuel
    SURFACES AND INTERFACES, 2019, 16 : 29 - 42
  • [40] Synergistic corrosion inhibition of environment-friendly inhibitors on the corrosion of carbon steel in soft water
    Zhang, Bingru
    He, Chengjun
    Wang, Cheng
    Sun, Peidi
    Li, Fengting
    Lin, Yu
    CORROSION SCIENCE, 2015, 94 : 6 - 20