Translucency and Wear of Pressable Lithium Disilicate and Zirconia-reinforced Lithium Silicate Glass-ceramics: An In-vitro Study

被引:3
|
作者
Potdukhe, Shruti S. [1 ]
Iyer, Janani M. [1 ]
Nadgere, Jyoti B. [1 ]
机构
[1] MGM Dent Coll, Dept Prosthodont & Crown & Bridge, Navi Mumbai, Maharashtra, India
关键词
Aesthetics; Optical; Rehabilitation; Spectrophotometer; COMPOSITE RESIN; HUMAN ENAMEL; 2-BODY WEAR; RESISTANCE; TEETH;
D O I
10.7860/JCDR/2023/56402.17353
中图分类号
R5 [内科学];
学科分类号
1002 ; 100201 ;
摘要
Introduction: New ceramic materials have been introduced with less research on their aesthetic outcome and durability for clinical implications. Lithium disilicate is one of the widely used materials for restoration. Recently, Zirconia-reinforced Lithium Silicate (ZLS) glass-ceramic enriched with 10% zirconia in highly dispersed glass phase of ceramic has been introduced.Aim: To investigate the translucency of pressable Lithium Disilicate (LS2) and ZLS and their effects on wear of opposing enamel.Materials and Methods: This in-vitro study was carried out at MGM Dental College and Hospital, Mumbai, Maharashtra, India, between January 2017 and January 2020. Twenty disks of 15x3 mm; 10 each of LS2 and ZLS were fabricated by hot pressing method. For translucency Commission Internationale de l'Eclairage (CIE) L*a*b values for each sample were measured against black and white background using a laboratory reflectance spectrophotometer. Translucency was calculated using Translucency Parameter (TP)= {(L*B-L*W)(2)+(a*B-a*W)(2)+(b*B-b*W)(2)}(1/2). For wear testing same 20 disks were used as an antagonist. Enamel specimen of 20 maxillary premolar were abraded against each antagonist with two body wear testing machine in rotational motion under a constant load of 20 N at 350 rpm for 5000 cycles. The initial readings and final readings of enamel specimen in pm were measured using contact stylus profilometer. Non parametric Mann-Whitney U test was used to compare the significance of difference between two groups.Results: The TP values obtained were 23.07 and 24.04 for LS2 and ZLS, respectively (p-value=0.004). The mean wear values obtained were 0.71860 pm and 1.09500 pm for LS2 and ZLS, respectively (p-value=0.049). The difference for both the parameters was statistically significant.Conclusion: Within the limitation of this study, ZLS showed higher translucency values than LS2. Wear rate of opposing enamel was more with ZLS than LS2. Thus ZLS may provide excellent aesthetics which can be used as an option for rehabilitation in aesthetic zone.
引用
收藏
页码:ZC36 / ZC39
页数:4
相关论文
共 50 条
  • [41] In-vitro wear of natural tooth surface opposed with zirconia reinforced lithium silicate glass ceramic after accelerated ageing
    Fathy, Salma M.
    Swain, Michael V.
    DENTAL MATERIALS, 2018, 34 (03) : 551 - 559
  • [42] Lithium Disilicate based Glass-Ceramics for Dental Applications
    Gaddam, Anuraag
    Goyal, Mudit
    Jain, Sudhanshu
    Bhargava, Parag
    TRANSACTIONS OF THE INDIAN CERAMIC SOCIETY, 2013, 72 (01) : 56 - 60
  • [43] Fracture anisotropy in texturized lithium disilicate glass-ceramics
    Belli, Renan
    Wendler, Michael
    Cicconi, Maria Rita
    de Ligny, Dominique
    Petschelt, Anselm
    Werbach, Katharina
    Peterlik, Herwig
    Lohbauer, Ulrich
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2018, 481 : 457 - 469
  • [44] Investigation of two-body wear behavior of zirconia-reinforced lithium silicate glass-ceramic for biomedical applications; in vitro chewing simulation
    Yilmaz, Efe Cetin
    COMPUTER METHODS IN BIOMECHANICS AND BIOMEDICAL ENGINEERING, 2021, 24 (07) : 806 - 815
  • [45] Mechanical and biocompatibility testing of zirconia and lithium disilicate ceramics: An in vitro study
    Tafuri, Giuseppe
    Xhajanka, Edit
    Hysenaj, Neada
    Sinjari, Bruna
    JOURNAL OF PROSTHETIC DENTISTRY, 2025, 133 (02): : 593e1 - 593e8
  • [46] Influence of Different Surface Finishing Protocols on the Wear Behavior of Lithium Disilicate Glass-Ceramics
    Weber, Katia R.
    Satpathy, Megha
    Marocho, Susana Salazar
    Griggs, Jason A.
    Borba, Marcia
    INTERNATIONAL JOURNAL OF PROSTHODONTICS, 2024, 37 (03) : 293 - 299
  • [47] Effects of crystal refining on wear behaviors and mechanical properties of lithium disilicate glass-ceramics
    Zhang, Zhenzhen
    Guo, Jiawen
    Sun, Yali
    Tian, Beimin
    Zheng, Xiaojuan
    Zhou, Ming
    He, Lin
    Zhang, Shaofeng
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2018, 81 : 52 - 60
  • [48] Glass science behind lithium silicate glass-ceramics
    Lohbauer, Ulrich
    Fabris, Debora Cristina Niero
    Lubauer, Julia
    Abdelmaseh, Samuel
    Cicconi, Maria -Rita
    Hurle, Katrin
    de Ligny, Dominique
    Goetz-Neunhoeffer, Friedlinde
    Belli, Renan
    DENTAL MATERIALS, 2024, 40 (05) : 842 - 857
  • [49] Potential applications of glass and glass-ceramics based on lithium disilicate as biomaterials
    Palou, Martin
    Bakos, Dusan
    Kuzielova, Eva
    Labuda, Jan
    BIOCERAMICS, VOL 20, PTS 1 AND 2, 2008, 361-363 : 273 - +
  • [50] Finishing technique effect on strength of zirconia-reinforced lithium silicate ceramic
    Benalcazar-Jalkh, Ernesto Byron
    Cunha, Verena Souza
    Bergamo, Edmara Tatiely Pedroso
    Alves, Larissa Marcia Martins
    de Monteiro-Sousa, Raphaelle Santos
    Campos, Tiago Moreira Bastos
    Tanaka, Ricardo
    Marcolino, Giovana de Assis
    de Souza, Felipe Machado
    Bonfante, Estevam Augusto
    EUROPEAN JOURNAL OF ORAL SCIENCES, 2024, 132 (01)