Investigation of failure modes and material structural responses of nanographite coatings on single-crystal silicon by nanoscratching

被引:4
作者
Brussel, Fabian [1 ]
Huang, Weihai [1 ]
Yan, Jiwang [1 ]
机构
[1] Keio Univ, Fac Sci & Technol, Dept Mech Engn, 3-14-1 Hiyoshi,Kohoku Ku, Yokohama 2238522, Japan
关键词
Nanoscratching; Nanographite coatings; Single-crystal silicon; Failure modes; Microstructural changes; RAMAN MICROSPECTROSCOPY; THERMAL-STABILITY; THIN-FILM; ADHESION; GLASS; MORPHOLOGY; SCATTERING; BEHAVIOR; OPTICS; SI;
D O I
10.1016/j.triboint.2024.109349
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The failure modes of a nanographite-on-silicon system and the effects of the coating on the load-induced phase transformation of the silicon substrate were investigated using a series of nanoscratching tests with a spherical diamond indenter. The critical normal load for the failure of the nanographite coating was determined based on the thickness of the coating. When the load increased beyond the critical point, cracks, press spallation, and lift spallation were observed, and the silicon substrate underwent a phase transformation from the original crystalline phase to a mixture of amorphous, Si-III and Si-XII phases. For a thin coating, the silicon substrate was free of phase transformation owing to the coating protection. These findings provide guidance for glass molding and other applications.
引用
收藏
页数:13
相关论文
共 44 条
[1]   Review on thin film coatings for precision glass molding [J].
Akhtar, Awais ;
Ruan, Haihui .
SURFACES AND INTERFACES, 2022, 30
[2]   Interactions, morphology and thermal stability of graphene-oxide reinforced polymer aerogels derived from star-like telechelic aldehyde-terminal benzoxazine resin [J].
Alhwaige, Almandi A. ;
Alhassan, Saeed M. ;
Katsiotis, Marios S. ;
Ishide, Hatsuo ;
Qutubuddin, Syed .
RSC ADVANCES, 2015, 5 (112) :92719-92731
[3]   Nano-scratch testing of (Ti,Fe)Nx thin films on silicon [J].
Beake, B. D. ;
Vishnyakov, V. M. ;
Harris, A. J. .
SURFACE & COATINGS TECHNOLOGY, 2017, 309 :671-679
[4]   Relationship between mechanical properties of thin nitride-based films and their behaviour in nano-scratch tests [J].
Beake, B. D. ;
Vishnyakov, V. M. ;
Harris, A. J. .
TRIBOLOGY INTERNATIONAL, 2011, 44 (04) :468-475
[5]   Triboactive coatings for wear and friction reduction in chain drives [J].
Bobzin, K. ;
Kalscheuer, C. ;
Moebius, M. P. ;
Rank, M. ;
Oehler, M. ;
Koch, O. .
TRIBOLOGY INTERNATIONAL, 2023, 185
[6]   An overview of the potential of quantitative coating adhesion measurement by scratch [J].
Bull, SJ ;
Berasetegui, EG .
TRIBOLOGY INTERNATIONAL, 2006, 39 (02) :99-114
[7]   FAILURE MODES IN SCRATCH ADHESION TESTING [J].
BULL, SJ .
SURFACE & COATINGS TECHNOLOGY, 1991, 50 (01) :25-32
[8]   Influence of mechanical properties on the nanoscratch behaviour of hard nanocomposite TiN/Si3N4 coatings on Si [J].
D Beake, B ;
Vishnyakov, VM ;
Valizadeh, R ;
Colligon, JS .
JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2006, 39 (07) :1392-1397
[9]   Reduced crater wear and improved high-speed dry cutting performance of B-containing AlTiBN coatings against Ti-6Al-4 V alloy [J].
Fang, Wei ;
Chen, Junkai ;
Cai, Fei ;
Zhou, Qi ;
Li, Mingxi ;
Zhang, Shihong .
TRIBOLOGY INTERNATIONAL, 2023, 187
[10]   Manufacture and mechanical-tribological assessment of diamond-reinforced Cu-based coatings for cutting/grinding tools [J].
Frutos, E. ;
Richhariya, V. ;
Silva, F. S. ;
Trindade, B. .
TRIBOLOGY INTERNATIONAL, 2023, 177