Synthesis of Ti2AlC MAX phase and Ti2C MXene by activated combustion

被引:8
作者
Aydinyan, S. [1 ,2 ]
机构
[1] NAS RA, AB Nalbandyan Inst Chem Phys, P Sevak 5-2, Yerevan 0014, Armenia
[2] Tallinn Univ Technol, Ehitajate Tee 5, EE-19086 Tallinn, Estonia
关键词
MAX phase; MXene; Self -propagating high -temperature synthesis; Thermokinetic coupling; Heating rate; AL-C SYSTEM; ELEMENTAL POWDERS; TI3ALC2; FABRICATION; REDUCTION; MECHANISM; TI3SIC2;
D O I
10.1016/j.ceramint.2024.01.130
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The preparation of the Ti2AlC MAX phase by activated self-propagating high-temperature synthesis from a mixture of elemental powders using the thermokinetic coupling approach is reported. The underlying mechanism in the Ti-Al-C system has been elucidated. Ti2C MXene was produced by exfoliation of its MAX counterpart. The combustion wave sensitive parameters were determined, the influence of promoter and ambient gas pressure on the phase composition and evolution of the microstructure was revealed. The Ti2AlC MAX phase was successfully prepared in an energy-efficient pathway with some controlled amount of TiC. The interaction mechanism, simulated at comparatively higher heating rates (beta = 600-4800 degrees C<middle dot>min(-1)), demonstrated the evolution of the following phases: Ti3Al, TiC, Ti3AlC, Ti2AlC, T3AlC2, Al3Ti. Etching for only 2h in combination with double ultrasonic treatment made it possible to delaminate the nanolayered structure of the parent MAX phase and obtain Ti2C MXene.
引用
收藏
页码:12263 / 12269
页数:7
相关论文
共 50 条
  • [21] Synthesis of MAX phases Ti2AlC and V2AlC by carburization of hydrogenated alloys Ti2AlHx and V2AlHx
    Bokov, Arseniy
    Shelyug, Anna
    Kurlov, Alexey
    [J]. CERAMICS INTERNATIONAL, 2024, 50 (02) : 3289 - 3298
  • [22] Halogen Etch of Ti3AlC2 MAX Phase for MXene Fabrication
    Jawaid, Ali
    Hassan, Asra
    Neher, Gregory
    Nepal, Dhriti
    Pachter, Ruth
    Kennedy, W. Joshua
    Ramakrishnan, Subramanian
    Vaia, Richard A.
    [J]. ACS NANO, 2021, 15 (02) : 2771 - 2777
  • [23] Relative Ti2AlC Scale Volatility under 1300 °C Combustion Conditions
    Smialek, James L.
    [J]. COATINGS, 2020, 10 (02)
  • [24] Effect of temperature on the healing capacity and mechanical properties of Ti2AlC MAX phase ceramics
    Suh, Minji
    Lee, Dong Heon
    Sloof, Willem G.
    Lee, Kee Sung
    [J]. INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2024, 21 (04) : 2757 - 2770
  • [25] On the interactions of Ti2AlC, Ti3AlC2, Ti3SiC2 and Cr2AlC with palladium at 900 °C
    Bentzel, G. W.
    Sokol, M.
    Griggs, J.
    Lang, A. C.
    Barsoum, M. W.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 771 : 1103 - 1110
  • [26] Butane Dry Reforming Catalyzed by Cobalt Oxide Supported on Ti2AlC MAX Phase
    Ronda-Lloret, Maria
    Marakatti, Vijaykumar S.
    Sloof, Willem G.
    Delgado, Juan Jose
    Sepulveda-Escribano, Antonio
    Ramos-Fernandez, Enrique V.
    Rothenberg, Gadi
    Shiju, N. Raveendran
    [J]. CHEMSUSCHEM, 2020, 13 (23) : 6401 - 6408
  • [27] Ti2AlC MAX phase for resistance against CMAS attack to thermal barrier coatings
    Guo, Lei
    Yan, Zheng
    Wang, Xiaohui
    He, Quanjun
    [J]. CERAMICS INTERNATIONAL, 2019, 45 (06) : 7627 - 7634
  • [28] Sputter deposition from a Ti2AlC target: Process characterization and conditions for growth of Ti2AlC
    Frodelius, J.
    Eklund, P.
    Beckers, M.
    Persson, P. O. A.
    Hogberg, H.
    Hultman, L.
    [J]. THIN SOLID FILMS, 2010, 518 (06) : 1621 - 1626
  • [29] Preparation of Ti2AlC and Ti3AlC2 MAX Phases by Self-Propagating High-Temperature Synthesis with the Reduction Stage
    V. I. Vershinnikov
    D. Yu. Kovalev
    [J]. Russian Journal of Non-Ferrous Metals, 2020, 61 : 554 - 558
  • [30] Preparation of Ti2AlC and Ti3AlC2MAX Phases by Self-Propagating High-Temperature Synthesis with the Reduction Stage
    Vershinnikov, V. I.
    Kovalev, D. Yu.
    [J]. RUSSIAN JOURNAL OF NON-FERROUS METALS, 2020, 61 (05) : 554 - 558