Unravelling LaNi5 intrinsic degradation: New insights from DFT study on thermodynamics and hydrogen diffusion

被引:15
作者
Adarmouch, M. [1 ]
EL Kassaoui, M.
Jmal, S. Ait [1 ]
Mounkachi, O. [2 ,3 ,4 ]
Balli, M. [1 ,5 ]
机构
[1] Int Univ Rabat, AMEEC Team, LERMA, Parc Technopolis,Rocade Rabat, Sale 11100, Morocco
[2] Mohammed V Univ Rabat, Fac Sci, Dept Phys, Lab Condensed Matter & Interdisciplinary Sci, POB 1014, Rabat, Morocco
[3] Mohammed VI Polytech Univ, Coll Comp, Lot 660,Hay Moulay Rachid, Ben Guerir 43150, Morocco
[4] Mohammed VI Polytech Univ, Inst Appl Phys, Lot 660,Hay Moulay Rachid, Ben Guerir 43150, Morocco
[5] Univ Sherbrooke, Fac Genie, Dept Mech Engn, Quebec City, PQ J1K 2R1, Canada
关键词
Hydrogen storage; LaNi; 5; intermetallic; DFT calculation; Hydrogen-induced degradation; Hydrogen diffusion; KINETIC MONTE-CARLO; ELECTRONIC-PROPERTIES; STORAGE; ABSORPTION; TEMPERATURE; NEUTRON; ALLOYS; HYDRIDE; PERFORMANCE; OCCUPATION;
D O I
10.1016/j.est.2024.110664
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
The use of LaNi5 intermetallic for hydrogen storage is drastically limited due to its degradation during cycling. Despite extensive efforts in the literature to address this issue, a fundamental challenge remains - no one has been able to pinpoint the exact origin of this degradation. In this work, we elucidate the fundamental mechanisms behind this degradation using DFT calculations, a feat that couldn't be achieved through experimental methods alone. Particularly, our findings underscore the stability of the (2b) site in comparison to (6c1) and (6c2) sites. Hydrogen migration in the (x,y)-plane from (6c1)-site to (2b)-site is confirmed to be fast within the crystal structure, owing to a low barrier of 0.24 eV, which is much lower than that of MgH2. On the other hand, hydrogen diffusion from the (2b)-site to the (6c1)-site exhibits the highest energy barrier of 0.45 eV. These results emphasize the stability of the (2b)-site and provide a fundamental explanation for the degradation of LaNi5. Indeed, the occupation of the (2b)-site serves as the primary driving force behind the formation of stable hydrides that cannot be desorbed under ambient conditions.
引用
收藏
页数:9
相关论文
共 70 条
[41]   Theoretical model on the electronic properties of multi-element AB5-type metal hydride [J].
Panwar, Kuldeep ;
Srivastava, Sumita .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2021, 46 (18) :10819-10829
[42]   THE INTRINSIC DEGRADATION PHENOMENA OF LANI5 AND LANI4.7AL0.3 BY TEMPERATURE INDUCED HYDROGEN ABSORPTION-DESORPTION CYCLING [J].
PARK, JM ;
LEE, JY .
MATERIALS RESEARCH BULLETIN, 1987, 22 (04) :455-465
[43]   NEUTRON AND X-RAY-DIFFRACTION PROFILE ANALYSES AND STRUCTURE OF LANI5, LANI5-XALX AND LANI5-XMNX INTERMETALLICS AND THEIR HYDRIDES (DEUTERIDES) [J].
PERCHERONGUEGAN, A ;
LARTIGUE, C ;
ACHARD, JC ;
GERMI, P ;
TASSET, F .
JOURNAL OF THE LESS-COMMON METALS, 1980, 74 (01) :1-12
[44]  
Perdew JP, 1996, PHYS REV LETT, V77, P3865, DOI 10.1103/PhysRevLett.77.3865
[45]  
Pranevicius L., 2009, Int. J. Hydrogen Energy, P5131
[46]   NI-61 MOSSBAUER MEASUREMENTS OF NICKEL MICROPRECIPITATES PRODUCED IN LANI5 BY CYCLIC HYDROGEN ABSORPTION AND DESORPTION [J].
RUMMEL, H ;
COHEN, RL ;
GUTLICH, P ;
WEST, KW .
APPLIED PHYSICS LETTERS, 1982, 40 (06) :477-479
[47]   A review on the current progress of metal hydrides material for solid-state hydrogen storage applications [J].
Rusman, N. A. A. ;
Dahari, M. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2016, 41 (28) :12108-12126
[48]   A panoramic overview of hydrogen storage alloys from a gas reaction point of view [J].
Sandrock, G .
JOURNAL OF ALLOYS AND COMPOUNDS, 1999, 293 :877-888
[49]   A generalized solid-state nudged elastic band method [J].
Sheppard, Daniel ;
Xiao, Penghao ;
Chemelewski, William ;
Johnson, Duane D. ;
Henkelman, Graeme .
JOURNAL OF CHEMICAL PHYSICS, 2012, 136 (07)
[50]   Effect of temperature on fast forging process of Mg-Ni samples for fast formation of Mg2Ni for hydrogen storage [J].
Skryabina, Nataliya ;
Aptukou, Valery ;
de Rango, Patricia ;
Fruchart, Daniel .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2020, 45 (04) :3008-3015