Unravelling LaNi5 intrinsic degradation: New insights from DFT study on thermodynamics and hydrogen diffusion

被引:15
作者
Adarmouch, M. [1 ]
EL Kassaoui, M.
Jmal, S. Ait [1 ]
Mounkachi, O. [2 ,3 ,4 ]
Balli, M. [1 ,5 ]
机构
[1] Int Univ Rabat, AMEEC Team, LERMA, Parc Technopolis,Rocade Rabat, Sale 11100, Morocco
[2] Mohammed V Univ Rabat, Fac Sci, Dept Phys, Lab Condensed Matter & Interdisciplinary Sci, POB 1014, Rabat, Morocco
[3] Mohammed VI Polytech Univ, Coll Comp, Lot 660,Hay Moulay Rachid, Ben Guerir 43150, Morocco
[4] Mohammed VI Polytech Univ, Inst Appl Phys, Lot 660,Hay Moulay Rachid, Ben Guerir 43150, Morocco
[5] Univ Sherbrooke, Fac Genie, Dept Mech Engn, Quebec City, PQ J1K 2R1, Canada
关键词
Hydrogen storage; LaNi; 5; intermetallic; DFT calculation; Hydrogen-induced degradation; Hydrogen diffusion; KINETIC MONTE-CARLO; ELECTRONIC-PROPERTIES; STORAGE; ABSORPTION; TEMPERATURE; NEUTRON; ALLOYS; HYDRIDE; PERFORMANCE; OCCUPATION;
D O I
10.1016/j.est.2024.110664
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
The use of LaNi5 intermetallic for hydrogen storage is drastically limited due to its degradation during cycling. Despite extensive efforts in the literature to address this issue, a fundamental challenge remains - no one has been able to pinpoint the exact origin of this degradation. In this work, we elucidate the fundamental mechanisms behind this degradation using DFT calculations, a feat that couldn't be achieved through experimental methods alone. Particularly, our findings underscore the stability of the (2b) site in comparison to (6c1) and (6c2) sites. Hydrogen migration in the (x,y)-plane from (6c1)-site to (2b)-site is confirmed to be fast within the crystal structure, owing to a low barrier of 0.24 eV, which is much lower than that of MgH2. On the other hand, hydrogen diffusion from the (2b)-site to the (6c1)-site exhibits the highest energy barrier of 0.45 eV. These results emphasize the stability of the (2b)-site and provide a fundamental explanation for the degradation of LaNi5. Indeed, the occupation of the (2b)-site serves as the primary driving force behind the formation of stable hydrides that cannot be desorbed under ambient conditions.
引用
收藏
页数:9
相关论文
共 70 条
[31]   Hydrogen storage properties and cycling degradation of single-phase La0.60R0.15Mg0.25Ni3.45 alloys with A2B7-type superlattice structure [J].
Liu, Jingjing ;
Cheng, Honghui ;
Han, Shumin ;
Liu, Hongfei ;
Huot, Jacques .
ENERGY, 2020, 192
[32]   New insights into the hydrogen storage performance degradation and Al functioning mechanism of LaNi5-xAlx alloys [J].
Liu, Jingjing ;
Li, Kang ;
Cheng, Honghui ;
Yan, Kai ;
Wang, Yu ;
Liu, Yi ;
Jin, Huimin ;
Zheng, Zhi .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2017, 42 (39) :24904-24914
[33]   Crystal structure and hydrogen storage properties of (La,Ce)Ni5-xMx (M = Al, Fe, or Co) alloys [J].
Mi, Wan-liang ;
Liu, Zhao-sen ;
Kimura, Toru ;
Kamegawa, Atsunori ;
Wang, Hai-liang .
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2019, 26 (01) :108-113
[34]   VESTA 3 for three-dimensional visualization of crystal, volumetric and morphology data [J].
Momma, Koichi ;
Izumi, Fujio .
JOURNAL OF APPLIED CRYSTALLOGRAPHY, 2011, 44 :1272-1276
[35]   Hydrogen production, transportation, utilization, and storage: Recent advances towards sustainable energy [J].
Muhammed, Nasiru S. ;
Gbadamosi, Afeez O. ;
Epelle, Emmanuel I. ;
Abdulrasheed, Abdulrahman A. ;
Haq, Bashirul ;
Patil, Shirish ;
Al-Shehri, Dhafer ;
Kamal, Muhammad Shahzad .
JOURNAL OF ENERGY STORAGE, 2023, 73
[36]   THE THERMODYNAMICS OF THE LANI5-H2 SYSTEM BY DIFFERENTIAL HEAT-FLOW CALORIMETRY .1. TECHNIQUES - THE ALPHA+BETA 2-PHASE REGION [J].
MURRAY, JJ ;
POST, ML ;
TAYLOR, JB .
JOURNAL OF THE LESS-COMMON METALS, 1981, 80 (02) :201-209
[37]   Electronic structure and energetics of LaNi5, α-La2Ni10H and β-La2Ni10H14 [J].
Nakamura, H ;
Nguyen-Manh, D ;
Pettifor, DG .
JOURNAL OF ALLOYS AND COMPOUNDS, 1998, 281 (02) :81-91
[38]   Crystal structure and hydrogen occupation of LaNi4.9Al0.1Dx (5.0≤x≤6.1) on the desorption isotherm studied by in situ neutron powder diffraction [J].
Nakamura, Y ;
Ishigaki, T ;
Kamiyama, T ;
Akiba, E .
JOURNAL OF ALLOYS AND COMPOUNDS, 2004, 384 (1-2) :195-202
[39]   Variation of hydrogen occupation in LaNi4.78Sn0.22Dx along the P-C isotherms studied by in situ neutron powder diffraction [J].
Nakamura, Yumiko ;
Bowman, Robert C., Jr. ;
Akiba, Etsuo .
JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 431 (1-2) :148-154
[40]   SPECIAL POINTS FOR BRILLOUIN-ZONE INTEGRATIONS - REPLY [J].
PACK, JD ;
MONKHORST, HJ .
PHYSICAL REVIEW B, 1977, 16 (04) :1748-1749