The effect of repair protocols and chewing simulation on the microtensile bond strength of two resin matrix ceramics to composite resin

被引:2
作者
Elkassaby, Annan Ahmed [1 ]
Kandil, Mohamed M. [1 ]
Alian, Ghada Atef [1 ]
机构
[1] Ain Shams Univ, Dept Dent Biomat Dent, Cairo, Egypt
关键词
Polymer infiltrated ceramic network; Resin nanoceramics; Cyclic loading; Artificial aging; Mechanical fatigue; Mechanical aging; SURFACE TREATMENTS; CAD/CAM MATERIALS; BLOCKS; CEMENT;
D O I
10.1186/s12903-024-03932-4
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Background To assess the micro tensile bond strength (mu TBS) of two resin matrix ceramic (RMC) blocks bonded to composite resin by using different repair protocols with and without chewing simulation (CS). Materials and methods Two resin matrix ceramic blocks (Vita Enamic and Lava Ultimate) were divided into 4 groups according to the surface treatments: Bur grinding (control), Bur grinding + silane, 9.5% HF acid etching, and 9.5% HF acid etching + silane. The single bond universal adhesive was applied on all specimens after the surface treatments according to the manufacturer's instructions, it was administered actively on the treated surface for 20 s and then light cured for 10 s, followed by incremental packing of composite resin to the treated surface. Each group was further divided into 2 subgroups (with/without chewing simulation for 500,000 cycles). A micro tensile bond strength test was performed for each group (n = 15). The effect of surface treatments on the materials was examined by using a scanning electron microscope (SEM). The micro tensile bond strength (MPa) data were analyzed with a three-way ANOVA, the independent t-test, and one-way ANOVA followed by the Tukey post-hoc test. Results mu TBS results were significantly higher for Lava Ultimate than Vita Enamic for all the surface treatment protocols with (p < 0.01). The chewing simulation significantly negatively affected the micro-tensile bond strength (p < 0.001). Bur grinding + saline exhibited the highest bond strength values for Lava Ultimate, both with and without chewing simulation. For Vita Enamic, bur grinding + saline and HF acid + saline showed significantly higher bond strength values compared to other surface treatments, both with and without chewing simulation (p <= 0.05). Conclusion Bur grinding + silane could be recommended as a durable repair protocol for indirect resin matrix ceramics blocks with composite resin material.
引用
收藏
页数:8
相关论文
共 36 条
[1]   Impact of the Microstructure of CAD/CAM Blocks on the Bonding Strength and the Bonded Interface [J].
Abouelleil, Hazem ;
Colon, Pierre ;
Jeannin, Christophe ;
Goujat, Alexis ;
Attik, Nina ;
Laforest, Laurent ;
Gauthier, Remy ;
Grosgogeat, Brigitte .
JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2022, 31 (01) :72-78
[2]   An in vitro evaluation of the effect of polishing on the stainability of different CAD/CAM ceramic materials [J].
Abu-Obaid, Ala'a ;
AlMawash, Amjad ;
Alyabis, Noura ;
Alzaaqi, Nouf .
SAUDI DENTAL JOURNAL, 2020, 32 (03) :135-141
[3]   Effect of Aging Regimens on Resin Nanoceramic Chairside CAD/CAM Material [J].
Al-Harbi, Fahad A. ;
Ayad, Neveen M. ;
ArRejaie, Aws S. ;
Bahgat, Hala A. ;
Baba, Nadim Z. .
JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2017, 26 (05) :432-439
[4]   Repair bond strength of dental computer-aided design/computer-aided manufactured ceramics after different surface treatments [J].
AL-Turki, Lulwa ;
Merdad, Yasser ;
Abuhaimed, Tariq A. ;
Sabbahi, Dania ;
Almarshadi, Mazen ;
Aldabbagh, Raghad .
JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2020, 32 (07) :726-733
[5]   Repair bond strength and nanoleakage of artificially aged CAD-CAM composite resin [J].
Arpa, Carmen ;
Ceballos, Laura ;
Victoria Fuentes, Maria ;
Perdigao, Jorge .
JOURNAL OF PROSTHETIC DENTISTRY, 2019, 121 (03) :523-530
[6]   Evaluation of the repair capacities and color stabilities of a resin nanoceramic and hybrid CAD/CAM blocks [J].
Bahadir, Hasibe Sevilay ;
Bayraktar, Yusuf .
JOURNAL OF ADVANCED PROSTHODONTICS, 2020, 12 (03) :140-149
[7]   Effect of Different Surface Treatments on Bond Strength of Resin Cement to a CAD/CAM Restorative Material [J].
Barutcigil, Kubilay ;
Barutcigil, Cagatay ;
Kul, Esra ;
Ozarslan, Mehmet Mustafa ;
Buyukkaplan, Ulviye Sebnem .
JOURNAL OF PROSTHODONTICS-IMPLANT ESTHETIC AND RECONSTRUCTIVE DENTISTRY, 2019, 28 (01) :71-78
[8]   Effect of Er:YAG laser pulse duration on repair bond strength of resin-based and hybrid CAD/CAM restorative materials [J].
Bayraktar, Yusuf ;
Demirtag, Zulfikar ;
Celik, Cigdem .
JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2022, 36 (06) :606-619
[9]   Micro-shear bond strength of different resin cements to ceramic/glass-polymer CAD-CAM block materials [J].
Cekic-Nagas, Isil ;
Ergun, Gulfem ;
Egilmez, Ferhan ;
Vallittu, Pekka Kalevi ;
Lassila, Lippo Veli Juhana .
JOURNAL OF PROSTHODONTIC RESEARCH, 2016, 60 (04) :265-273
[10]   Effect of surface treatments on the bond strength of indirect resin composite to resin matrix ceramics [J].
Celik, Ersan ;
Sahin, Sezgi Cinel ;
Dede, Dogu Omur .
JOURNAL OF ADVANCED PROSTHODONTICS, 2019, 11 (04) :223-231