Engineering performance and expansion mechanism of MgO expansion agent in ultra-high performance concrete (UHPC)

被引:26
作者
Cui, Yong [1 ]
Li, Yanhe [2 ]
Wang, Qiang [1 ]
机构
[1] Tsinghua Univ, Dept Civil Engn, Beijing 100084, Peoples R China
[2] China Construct First Grp Corp Ltd, Beijing 100161, Peoples R China
关键词
UHPC; Compensation shrinkage; Restrained expansion; Expansion mechanism; MgO; AUTOGENOUS SHRINKAGE; POROUS MATERIALS; CRYSTAL-GROWTH; CRYSTALLIZATION; OPTIMIZATION; SENSITIVITY; BEHAVIOR; TENSILE;
D O I
10.1016/j.jobe.2023.106079
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Ultra-high performance concrete (UHPC), despite its excellent strength and toughness, has greater shrinkage. The effects of different reactivity (R-MgO, M -MgO and S-MgO) and content (0-12 wt%) of MgO expansive agent on the restrained expansion and mechanical properties of UHPC were investigated and the relationship among restrained expansion, hydration process, and pore structure was established. It was found that with 4-6 wt% R-MgO, the restrained expansion of UHPC in water for 14 days is (200-300) x 10-6, and the restrained shrinkage of UHPC cured in air for another 14 days is (100-180) x 10-6, which can meet the requirements of the national standard GB/T 50,119-2013 for compensation shrinkage without compromising the early me-chanical properties. The rate of restrained expansion of UHPC is controlled by the generation rate of Mg(OH)2, while the magnitude of restrained expansion of UHPC is controlled by the amount of Mg(OH)2. Under the same MgO amount, the restrained expansion of UHPC containing R-MgO was highest during 1-14 d. The restrained expansion of UHPC containing M -MgO exceeded that containing R-MgO during 14-28 d, while the restrained expansion of UHPC containing S-MgO reached the highest during 28-60 d. The dispersion coefficient was proposed and the mathe-matical model of UHPC at 14 d age regarding the relationship among restrained expansion, hy-dration process, and pore structure, epsilon re=(1.2 m x g(phi i) x Delta P-ft)/E, was developed.
引用
收藏
页数:16
相关论文
共 44 条
[1]   Ultra high performance concrete (UHPC) sleeper: Structural design and performance [J].
Bae, Younghoon ;
Pyo, Sukhoon .
ENGINEERING STRUCTURES, 2020, 210
[2]   Expansion mechanisms in calcium aluminate and sulfoaluminate systems with calcium sulfate [J].
Bizzozero, Julien ;
Gosselin, Christophe ;
Scrivener, Karen L. .
CEMENT AND CONCRETE RESEARCH, 2014, 56 :190-202
[3]   The influence of the hydration procedure of MgO expansive agent on the expansive behavior of shrinkage-compensating mortar [J].
Cao, Fengze ;
Yan, Peiyu .
CONSTRUCTION AND BUILDING MATERIALS, 2019, 202 :162-168
[4]   Hydration characteristics and expansive mechanism of MgO expansive agents [J].
Cao, Fengze ;
Miao, Miao ;
Yan, Peiyu .
CONSTRUCTION AND BUILDING MATERIALS, 2018, 183 :234-242
[5]   MECHANISM OF EXPANSION OF CONCRETE DUE TO THE PRESENCE OF DEAD-BURNT CAO AND MGO [J].
CHATTERJI, S .
CEMENT AND CONCRETE RESEARCH, 1995, 25 (01) :51-56
[6]   Rheological, deformation behaviors and mechanical changes of MgO-containing concretes with different strength [J].
Cui, Yong ;
Wang, Heng ;
Liu, Kuisheng ;
Wang, Qiang .
JOURNAL OF BUILDING ENGINEERING, 2023, 64
[7]   OPTIMIZATION OF ULTRA-HIGH-PERFORMANCE CONCRETE BY THE USE OF A PACKING MODEL [J].
DE LARRARD, F ;
SEDRAN, T .
CEMENT AND CONCRETE RESEARCH, 1994, 24 (06) :997-1009
[8]   Mixture-proportioning of high-performance concrete [J].
de Larrard, F ;
Sedran, T .
CEMENT AND CONCRETE RESEARCH, 2002, 32 (11) :1699-1704
[9]  
Dudziak L., 2017, Mitigating Autogenous Shrinkage of Ultra-high Performance Concrete by Means of Internal Curing Using Superabsorbent polymers
[10]   Optimized design of steel fibres reinforced ultra-high performance concrete (UHPC) composites: Towards to dense structure and efficient fibre application [J].
Fan Dingqiang ;
Rui Yu ;
Liu Kangning ;
Tan Junhui ;
Shui Zhonghe ;
Wu Chunfeng ;
Wang Shuo ;
Guan Zhenfeng ;
Hu Zhengdong ;
Su Qiqi .
CONSTRUCTION AND BUILDING MATERIALS, 2021, 273