Microstructure evolution and mechanical properties of 16Cr-25Ni superaustenitic stainless steel weld metal during 600 °C aging

被引:1
|
作者
Tian, Wenbin [1 ,2 ,3 ]
Dong, Wenchao [3 ]
Lu, Shanping [1 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, Shenyang 110016, Peoples R China
[2] Univ Sci & Technol China, Sch Mat Sci & Engn, Shenyang 110016, Peoples R China
[3] Chinese Acad Sci, Inst Met Res, CAS Key Lab Nucl Mat & Safety Assessment, Shenyang 110016, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2023年 / 22卷
关键词
Superaustenitic stainless steel; Weld metal; Carbide; Mechanical properties; Aging; COOLED FAST-REACTOR; STRESS RUPTURE PROPERTIES; TERM THERMAL EXPOSURE; SODIUM; BEHAVIOR; SUPERALLOY;
D O I
10.1016/j.jmrt.2022.11.134
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of high temperature aging on the microstructure evolution and mechanical properties of 16Cr-25Ni superaustenitic stainless steel weld metal was investigated at 600 degrees C for up to 5000 h. Interdendritic micro-size M6C carbide, nano-size M6C and M23C6 carbides were identified in the 200 h aged weld metal, which appeared in clusters and distributed dispersedly. With the aging time increased to 1000 h, the interdendritic region was filled with newly formed precipitates, which were identified as nano-size M12C and M23C6 carbides. Compared with M6C carbide, M12C carbide was preferred to precipitate for lower Gibbs free energy, and the pre-existed M6C carbide had transformed to M12C carbide through the release of C atoms to the matrix. As the aging time further increased to 5000 h, the M12C carbide kept stable with the M23C6 carbide. Due to the precipitation and coarsen of M12C and M23C6 carbides that consumed massive solute atoms from matrix, which weakened the precipitation strengthening effect and suppressed the dynamic strain aging, the tensile properties kept superior stability during aging. The evolution of impact toughness was also closely related to the interdendritic precipitates. As the interdendritic region was occupied by precipitates since the aging time increased from 200 h to 1000 h, the impact toughness rapidly decreased from 76 J to 39 J, and then slightly decreased to 33 J with the aging time increased to 5000 h.(c) 2022 The Author(s). Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:461 / 472
页数:12
相关论文
共 50 条
  • [31] Microstructural evolution and mechanical properties of an Fe-18Ni-16Cr-4Al base alloy during aging at 950A°C
    Wang, Man
    Sun, Yong-duo
    Feng, Jing-kai
    Zhang, Rui-qian
    Tang, Rui
    Zhou, Zhang-jian
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2016, 23 (03) : 314 - 322
  • [32] Evolution and Coarsening of Carbides in 2. 25Cr-1Mo Steel Weld Metal During High Temperature Tempering
    Tao Peng
    Zhang Chi
    Yang Zhi-gang
    Hiroyuki, Takeda
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2010, 17 (05) : 74 - 78
  • [33] Modeling the constitutive relationship of Cr20Ni25Mo4Cu superaustenitic stainless steel during elevated temperature
    Han, Ying
    Qiao, Guanjun
    Sun, Yu
    Zou, Dening
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 539 : 61 - 67
  • [34] Evolution of the microstructure and mechanical properties of Sanicro 25 austenitic stainless steel after long-term ageing
    Sroka, M.
    Zielinski, A.
    Golanski, G.
    Pawlyta, M.
    Purzynska, H.
    Novy, F.
    ARCHIVES OF CIVIL AND MECHANICAL ENGINEERING, 2023, 23 (03)
  • [35] A Study on the Microstructure and Mechanical Properties of Improved 25Ni-20Cr Steel via in Situ Testing
    Lei, Penghui
    Ji, Xiaoyu
    Chen, Jiahao
    Huang, Yunhao
    Lv, Nan
    Fan, Yulin
    Hou, Yongchao
    Shi, Xinsheng
    Yun, Di
    NANOMATERIALS, 2025, 15 (06)
  • [36] Microstructural evolution and mechanical properties of an Fe–18Ni–16Cr–4Al base alloy during aging at 950°C
    Man Wang
    Yong-duo Sun
    Jing-kai Feng
    Rui-qian Zhang
    Rui Tang
    Zhang-jian Zhou
    International Journal of Minerals Metallurgy and Materials, 2016, 23 (03) : 314 - 322
  • [37] Microstructural evolution and mechanical properties of an Fe–18Ni–16Cr–4Al base alloy during aging at 950°C
    Man Wang
    Yong-duo Sun
    Jing-kai Feng
    Rui-qian Zhang
    Rui Tang
    Zhang-jian Zhou
    International Journal of Minerals, Metallurgy, and Materials, 2016, 23 : 314 - 322
  • [38] Effects of Stabilization Heat Treatment on Microstructure and Mechanical Properties of Si-Bearing 15Cr–9Ni–Nb Austenitic Stainless Steel Weld Metal
    Yakui Chen
    Dong Wu
    Dianzhong Li
    Yiyi Li
    Shanping Lu
    Acta Metallurgica Sinica (English Letters), 2023, 36 : 637 - 649
  • [39] Microstructure Evolution and Precipitation Behavior of 0Cr16Ni5Mo Martensitic Stainless Steel during Tempering Process
    Yuan, Wu-hua
    Gong, Xue-hui
    Sun, Yong-qing
    Hang, Jian-xiong
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2016, 23 (04) : 401 - 408
  • [40] Effects of Cyclic Heat Treatment on Microstructure and Mechanical Properties of 13%Cr-4%Ni Martensitic Stainless Steel
    Singh, Jai
    Nath, S. K.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (04) : 2478 - 2490