Preparation and properties of AlN-BN composite ceramics through combined addition of c-BN and h-BN

被引:4
作者
Gu, Siyong [1 ,2 ]
Xu, Zhikai [1 ,2 ]
Zhang, Houan [1 ,2 ]
Li, Tao [3 ]
Zhong, Shumiao [1 ,2 ]
Ma, Jidong [1 ,2 ]
Lu, Huifeng [4 ]
Qiao, Dongxu [1 ,2 ]
Qin, Mingli [3 ]
机构
[1] Xiamen Univ Technol, Fujian Key Lab Funct Mat & Applicat, Xiamen 361024, Fujian, Peoples R China
[2] Xiamen Univ Technol, Xiamen Key Lab Powder Met Technol & Adv Mat, Xiamen 361024, Fujian, Peoples R China
[3] Beijing Univ Sci, Inst New Mat Technol, Beijing 10083, Peoples R China
[4] Xiamen Vantage Ceram Technol Co Ltd, Xiamen 361024, Fujian, Peoples R China
关键词
AlN/BN composite ceramics; Cubic boron nitride; Flexural strength; Anisotropy; Microstructure; MECHANICAL-PROPERTIES; THERMAL-CONDUCTIVITY; BORON-NITRIDE; MICROSTRUCTURE;
D O I
10.1016/j.ceramint.2023.10.231
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
"Lamellar" structure of hexagonal boron nitride (h-BN) is prone to the formation of pore defects and the establishment of directional alignment during sintering process, which lead to AlN/BN composite ceramics exhibiting low density and anisotropic flexural strength (a equivalent to, a perpendicular to, and a||) (Orientation Bias Index 'IOP' >> 1); these factors greatly limit the application of AlN/BN composite ceramics. In this work, cubic boron nitride (c-BN) was introduced as a reinforcing phase into AlN/BN composite ceramics, which were prepared via hot pressing sintering, and the effects of c-BN addition on microstructure, mechanical properties, and anisotropy were systematically investigated. The results show that during hot pressing sintering, c-BN phase changes into h-BN with "onion" structure, which effectively fills pore defects and reduces the degree of alignment of h-BN. 'IOP' of sample 0C25H (170) continues to decrease with the increase in c-BN amount up to 2.7%. and anisotropy is significantly reduced. With the increase in c-BN amount, a equivalent to and a perpendicular to first increase and then decrease, while a|| only increases. a equivalent to and a perpendicular to reach the highest values (a equivalent to = 362 MPa and a perpendicular to = 340 MPa) at a c-BN amount of 15% (sample 15C10H); these values are 20.5% and 15.6% higher than those of sample 0C25H (no c-BN added), respectively, and a|| reaches the highest value (a|| = 239 MPa) for sample 25C0H, which is 136.6% higher than that of sample 0C25H. Sample 25C0H exhibits the highest a|| value (239 MPa), which is 136.6% higher than that of sample 0C25H. The onion-like h-BN formed by phase transformation of c-BN not only provides significant toughening to AlN/BN composite ceramics but can also effectively reduce anisotropy in their mechanical properties.
引用
收藏
页码:1419 / 1427
页数:9
相关论文
共 29 条
  • [11] Mao C., 2023, J. Eur. Ceram. Soc., V43, DOI [10.1016/j.jeurceramsoc.2023, DOI 10.1016/J.JEURCERAMSOC.2023]
  • [12] Transient Liquid Phase Bonding of AlN to AlSiC for Durable Power Electronic Packages
    Pahinkar, Darshan G.
    Puckett, Waylon
    Graham, Samuel
    Boteler, Lauren
    Ibitayo, Dimeji
    Narumanchi, Sreekant
    Paret, Paul
    DeVoto, Douglas
    Major, Joshua
    [J]. ADVANCED ENGINEERING MATERIALS, 2018, 20 (10)
  • [13] Microstructure tailoring of red-emitting AlN-CaAlSiN3:Eu2+ composite phosphor ceramics with higher optical properties for laser lighting
    Peng, Xinglin
    Li, Shuxing
    Zhang, Buhao
    Liu, Zehua
    Zhang, Huihui
    Chen, Xiao
    Tian, Rundong
    Yao, Xiumin
    Huang, Zhengren
    Xie, Rong-Jun
    Liu, Xuejian
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2022, 42 (07) : 3339 - 3344
  • [14] Features of a cBN-to-graphite-like BN phase transformation under pressure
    Petrusha, IA
    [J]. DIAMOND AND RELATED MATERIALS, 2000, 9 (08) : 1487 - 1493
  • [15] Investigation on the microwave sintering heating process and mechanism of h-BN/ZrO2/SiC composites
    Qi, Yongshun
    Song, Bo
    Wang, Hailong
    Chen, Mao
    Fan, Bingbing
    Zhang, Rui
    Ma, Beiyue
    Li, Hongxia
    Chen, Yongqiang
    [J]. CERAMICS INTERNATIONAL, 2023, 49 (12) : 20594 - 20600
  • [16] Powder injection molding of complex-shaped aluminium nitride ceramic with high thermal conductivity
    Qin, Mingli
    Lu, Huifeng
    Wu, Haoyang
    He, Qing
    Liu, Chang
    Mu, Xiaodong
    Wang, Yuelong
    Jia, Baorui
    Qu, Xuanhui
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (04) : 952 - 956
  • [17] Refined phase diagram of boron nitride
    Solozhenko, VL
    Turkevich, VZ
    Holzapfel, WB
    [J]. JOURNAL OF PHYSICAL CHEMISTRY B, 1999, 103 (15): : 2903 - 2905
  • [18] Thermal Conductivity of Aluminum Scandium Nitride for 5G Mobile Applications and Beyond
    Song, Yiwen
    Perez, Carlos
    Esteves, Giovanni
    Lundh, James Spencer
    Saltonstall, Christopher B.
    Beechem, Thomas E.
    Yang, Jung In
    Ferri, Kevin
    Brown, Joseph E.
    Tang, Zichen
    Maria, Jon-Paul
    Snyder, David W.
    Olsson, Roy H., III
    Griffin, Benjamin A.
    Trolier-McKinstry, Susan E.
    Foley, Brian M.
    Choi, Sukwon
    [J]. ACS APPLIED MATERIALS & INTERFACES, 2021, 13 (16) : 19031 - 19041
  • [19] Fracture behavior of AlN ceramics with rare earth oxides
    Terao, R
    Tatami, J
    Meguro, T
    Komeya, K
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (07) : 1051 - 1059
  • [20] Role of h-BN content on microstructure and mechanical properties of hot-pressed ZrB2-SiC composites
    Vafa, Nasser Pourmohammadie
    Kakroudi, Mahdi Ghassemi
    Asl, Mehdi Shahedi
    [J]. CERAMICS INTERNATIONAL, 2020, 46 (13) : 21533 - 21541