The effects of V or Sn addition on the microstructural characteristics and mechanical properties of Nb-16Si-22Ti-2Al-2Cr alloy

被引:1
|
作者
Li, Zhaobo [1 ]
Luo, Liangshun [1 ]
Wang, Binbin [1 ]
Su, Baoxian [1 ]
Luo, Lei [2 ]
Wang, Liang [1 ]
Su, Yanqing [1 ]
Guo, Jingjie [1 ]
Fu, Hengzhi [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Natl Key Lab Precis Hot Proc Met, Harbin 150001, Peoples R China
[2] Nanjing Univ Aeronaut & Astronaut, Coll Mat Sci & Technol, Nanjing 210016, Peoples R China
来源
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS | 2024年 / 120卷
基金
中国国家自然科学基金;
关键词
Alloying; Fracture toughness; Compressive strength; Crystallographic orientation relationship; FRACTURE-TOUGHNESS; OXIDATION RESISTANCE; NB; PHASE; EVOLUTION; TI; STRENGTH; CR; DEFORMATION; BEHAVIOR;
D O I
10.1016/j.ijrmhm.2024.106606
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Microstructural characteristics and mechanical properties of as-cast Nb-16Si-22Ti-2Al-2Cr-xV (x = 2, 5, 10, 15 and 20 at.%) and Nb-16Si-22Ti-2Al-2Cr-ySn (y = 1, 3, 5 and 7 at.%) alloys are systematically investigated in this study. The individual addition of V or Sn obviously promotes the eutectoid decomposition of metastable phase (Nb3Si). All alloys consist of the primary Nb5Si3 and the eutectic Nbss/Nb5Si3 structures. For the V-added alloys, the low content of added V (2 at.%) cannot change the constituent phases (Nbss and alpha-Nb5Si3) of Nb-16Si-22Ti2Al-2Cr alloy. However, the other V-added alloys consist of the primary beta-Nb5Si3 and the eutectic structures of Nbss/beta-Nb5Si3. Similarly, addition of 1 at.% Sn also cannot affect the constituent phases of Nb-16Si-22Ti-2Al-2Cr alloy, while the beta-Nb5Si3 and Nb3Sn are formed with the increase in Sn content. Moreover, the addition of V or Sn promotes the formation of chaotic eutectics and suppresses the appearance of reticulate and cellular eutectics. The fracture toughness of the alloys is continuously elevated by the V addition, while it gets weakened when the content of added Sn exceeds 1 at.%. The high-temperature compressive strength of the V-added alloys increases when the V content is below 10 at.%, and then it decreases with increasing V content. The Sn-added alloys, except 3Sn alloy, exhibit higher compressive strength than Nb-16Si-22Ti-2Al-2Cr alloy, due to the increase in volume fractions of brittle phases (beta-Nb5Si3 and Nb3Sn). Moreover, the crystallographic orientation relationships among the constituent phases are also explored before and after high-temperature compression.
引用
收藏
页数:15
相关论文
共 50 条
  • [41] Microstructural evolution and oxidation behaviour of Mo-Si-B coatings on an Nb-16Si-22Ti-7Cr-2Al-2Hf alloy at 1250 °C prepared by spark plasma sintering
    Wen, S. H.
    Zhou, C. G.
    Sha, J. B.
    SURFACE & COATINGS TECHNOLOGY, 2018, 352 : 320 - 329
  • [42] Effect of microstructure on fracture characteristics of Ti-6Al-2Sn-2Mo-2Zr-2Cr-Si alloy
    Niinomi, M
    Fukunaga, K
    Tono, G
    Koike, J
    Eylon, D
    Fujishiro, S
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2001, 87 (01): : 55 - 62
  • [43] Effect of Re addition on microstructure and mechanical properties of Nb-Si-Ti-Al-Cr-Hf ultrahigh temperature alloys
    Zhou, Zhecheng
    Wang, Qi
    Chen, Ruirun
    Zhao, Tianyu
    Chen, Dezhi
    Su, Yanqing
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2022, 105
  • [44] Microstructure evolution and a new mechanism of B2 phase on room temperature mechanical properties of Ti-47Al-2Cr-2Nb alloy prepared by hot isostatic pressing
    Li, Jizhan
    Song, Bo
    Nurly, Hasfi
    Xue, PengJu
    Wen, Shifeng
    Wei, Qingsong
    Shi, Yusheng
    MATERIALS CHARACTERIZATION, 2018, 140 : 64 - 71
  • [45] Microstructural control and mechanical properties of a β-solidified γ-TiAl alloy Ti-46Al-2Nb-1.5V-1Mo-Y
    Zhao, E. T.
    Niu, H. Z.
    Zhang, S. Z.
    Feng, L.
    Yang, S. Y.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 701 : 1 - 6
  • [46] Microstructure evolution and mechanical properties of Ti-22Al-25Nb alloy joints brazed with Ti-Ni-Nb alloy
    Wang, Y.
    Cai, X. Q.
    Yang, Z. W.
    Qiu, Q. W.
    Wang, D. P.
    Liu, Y. C.
    MATERIALS CHEMISTRY AND PHYSICS, 2016, 182 : 488 - 497
  • [47] Selective laser melting of Ti-22Al-25Nb intermetallic: Significant effects of hatch distance on microstructural features and mechanical properties
    Zhou, Y. H.
    Li, W. P.
    Zhang, L.
    Zhou, S. Y.
    Jia, X.
    Wang, D. W.
    Yan, M.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2020, 276 (276)
  • [48] Effect of nitrogen addition and aging treatment on microstructure and high temperature mechanical properties of Ti-48Al-2Cr-2Nb (at%) intermetallic alloy
    Ghorbani, Hamid Reza
    Kermanpur, Ahmad
    Rezaeian, Ahmad
    Sadeghi, Fazlollah
    Siahboumi, Abbas Ahmadi
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 904
  • [49] Effect of hafnium addition on microstructure and room temperature mechanical properties of the Ti-48Al-2Cr-2Nb intermetallic alloy
    Siahboumi, Abbas Ahmadi
    Kermanpur, Ahmad
    Ghorbani, Hamid Reza
    Belova, Lyubov
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 917
  • [50] Effects of Nb content in Ti-Ni-Nb brazing alloys on the microstructure and mechanical properties of Ti-22Al-25Nb alloy brazed joints
    Wang, Y.
    Cai, X. Q.
    Yang, Z. W.
    Wang, D. P.
    Liu, X. G.
    Liu, Y. C.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2017, 33 (07) : 682 - 689