Macro-micro crack and damage evolution characteristics of concrete: After the action of acidic drying-saturation cycle

被引:12
作者
Yang, Hengze [1 ,2 ]
Wang, Xiaoran [3 ]
Wang, Enyuan [1 ,2 ]
Song, Yue [1 ,2 ]
Chen, Dong [4 ]
Zhang, Yandong [3 ]
Liu, Weizhen [5 ]
机构
[1] State Key Lab Coal Mine Disaster Prevent & Control, Xuzhou 221116, Peoples R China
[2] China Univ Min & Technol, Sch Safety Engn, Xuzhou 221116, Peoples R China
[3] China Univ Min & Technol, State Key Lab Fine Explorat & Intelligent Dev Coal, Xuzhou 221116, Peoples R China
[4] State Key Lab Intelligent Construct & Hlth Operat, Xuzhou 221116, Jiangsu, Peoples R China
[5] Shandong Univ Sci & Technol, Coll Resources, Tai An 271019, Peoples R China
基金
中国国家自然科学基金;
关键词
Acidic drying-saturation cycle; Crack evolution; RA -AF value; Fractal dimension; Damage constitutive model; CONSTITUTIVE MODEL; FREEZE-THAW; ROCK;
D O I
10.1016/j.conbuildmat.2023.134601
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Repeated saturation and drying of acidic mine water have a major influence on the mechanical properties and stability monitoring of artificial dams (concrete walls) in underground reservoirs. A uniaxial compression acoustic emission (AE) monitoring test was conducted to quantify the evolution characteristics of micro cracks in concrete. In addition, the evolution characteristics of macro cracks during sample failure were quantitatively analyzed by fractal dimension theory and Image-Pro. Finally, the damage constitutive model was established and the damage evolution law was studied. The results of the study showed that the percentage of micro shear cracks in dry samples exhibited a decreasing and then increasing trend during the loading stage before the uniaxial compressive strength (UCS). However, after the acidic drying-saturation cycle (ADSC), this percentage of concrete showed an increasing trend. As the number of drying-saturation cycles increases or the pH decreases, the fractal dimension, total length, and area of the macro cracks also increase. The damage constitutive model, based on ADSC and loading conditions, works well. After the ADSC, the concrete sample will have three damage stages. Additionally, the strain at entry into each stage increases. Expansion and shrinkage of hydration products and chemical damage due to ion exchange are the mechanisms that change the mechanical properties and the macromicro crack evolution pattern of concrete after ADSC.
引用
收藏
页数:15
相关论文
共 38 条
[1]   Acoustic emission characterization of the fracture process in fibre reinforced concrete [J].
Aggelis, D. G. ;
Soulioti, D. V. ;
Sapouridis, N. ;
Barkoula, N. M. ;
Paipetis, A. S. ;
Matikas, I. E. .
CONSTRUCTION AND BUILDING MATERIALS, 2011, 25 (11) :4126-4131
[2]  
[Anonymous], 2002, Standard Test Methods for Flexural Properties of Unreinforced and Reinforced Plastics and Electrical Insulating Materials
[3]  
[Anonymous], 2009, STANDARD TEST METHOD
[4]   A Real-Time Visual Investigation on Microscopic Progressive Fatigue Deterioration of Granite Under Cyclic Loading [J].
Fan, L. F. ;
Qiu, B. ;
Gao, J. W. ;
Du, X. L. .
ROCK MECHANICS AND ROCK ENGINEERING, 2023, 56 (07) :5133-5147
[5]  
Fang J., 2018, J. China Coal Soc, V43, P412, DOI DOI 10.13225/J.CNKI.JCCS.2018.0629
[6]   Establishment of damage statistical constitutive model of loaded rock and method for determining its parameters under freeze-thaw condition [J].
Fang, Wen ;
Jiang, Nan ;
Luo, Xuedong .
COLD REGIONS SCIENCE AND TECHNOLOGY, 2019, 160 :31-38
[7]  
Gu D.Z., 2016, COAL SCI TECHNOL, V1, P1
[8]  
[顾大钊 Gu Dazhao], 2015, [煤炭学报, Journal of China Coal Society], V40, P239
[9]   Fractal characteristics of mesostructure and optimization of axial compression constitutive model of coal-fired slag concrete [J].
Guo, Zhongping ;
Liu, Weizhen ;
Wang, Chao ;
He, Chengqian ;
Zhang, Fuyu .
MATERIALS TODAY COMMUNICATIONS, 2021, 28
[10]   A statistical damage constitutive model under freeze-thaw and loading for rock and its engineering application [J].
Huang, Shibing ;
Liu, Quansheng ;
Cheng, Aiping ;
Liu, Yanzhang .
COLD REGIONS SCIENCE AND TECHNOLOGY, 2018, 145 :142-150