共 83 条
ZIF-67 derived Co nanoparticles on ZIF-Derived carbon for hydrogen spillover and storage
被引:15
作者:
Tseng, Po-Sen
[1
]
Chang, Lun-Xin
[1
]
Ou, Yi-Sheng
[1
]
Chou, Che-Min
[2
]
Tsao, Cheng-Si
[3
,4
]
Wu, Yawei
[5
]
Chou, Jyh-Pin
[6
]
Chen, Peng-Jen
[6
]
Wang, Cheng-Yu
[1
]
机构:
[1] Natl Yang Ming Chiao Tung Univ, Dept Mat Sci & Engn, Hsinchu 30010, Taiwan
[2] Natl Synchrotron Radiat Res Ctr, Hsinchu, Taiwan
[3] Inst Nucl Energy Res, Taoyuan 32546, Taiwan
[4] Natl Taiwan Univ, Dept Mat Sci & Engn, Taipei 10617, Taiwan
[5] City Univ Hong Kong, Dept Mech Engn, Kowloon, Hong Kong 999077, Peoples R China
[6] Natl Changhua Univ Educ, Dept Phys, Changhua 50007, Taiwan
关键词:
Hydrogen spillover;
ZIF-derived carbon;
Cobalt nanoparticle;
N-doped carbon;
Hydrogen storage;
METAL-ORGANIC FRAMEWORKS;
POROUS CARBON;
CATALYTIC-HYDROGENATION;
TEMPERATURE;
NITROGEN;
ADSORPTION;
ENERGY;
PERFORMANCE;
INSIGHTS;
CAPACITY;
D O I:
10.1016/j.apsusc.2023.158097
中图分类号:
O64 [物理化学(理论化学)、化学物理学];
学科分类号:
070304 ;
081704 ;
摘要:
Hydrogen spillover involves the dissociation of H2 on transition metal nanoparticles and further atomic hydrogen surface migration on catalyst supports. Hence, the spillover phenomenon has been reported in applications of heterogeneous catalysis in hydrogenation and room-temperature hydrogen storage. However, a proper catalyst design is requisite to initiate hydrogen spillover, considering the transition metal particle dispersion, sorbent surface modification, porosity, etc. In this report, we pyrolyzed the zeolitic imidazolate framework ZIF-67 for residual Co metal nanoparticles and N-dopant on ZIF-derived carbon (ZDC) for hydrogen adsorption via spillover effect. Catalyst optimization by proper ZIF carbonization process regarding manipulated pyrolytic temperatures, atmospheres, and ramping rates, results in different properties in ZDCs. Well-distributed Co nanoparticles can be obtained on N-rich graphitic sorbent ZDCs with retained high specific surface area. The Co on ZDC exhibits improved room-temperature hydrogen capacity of 0.77 wt% than neat ZIF-67 of 0.09 wt% at 30 bar, 300 K. The adsorption sites were examined experimentally by nitrogen hydrogenation, and possible atomic hydrogen diffusion was evaluated theoretically showing energy barrier reduced by over 0.1 eV. It demonstrates that cobalt nanoparticles can successfully initiate hydrogen spillover on ZIF-derived carbon with nitrogen functionality, even without noble metals.