Mechanical properties, in vitro biodegradable behavior, biocompatibility and osteogenic ability of additively manufactured Zn-0.8Li-0.1Mg alloy scaffolds

被引:25
|
作者
Liu, Aobo [1 ,2 ]
Lu, Yupu [3 ]
Dai, Jiabao [1 ,2 ]
Wen, Peng [1 ,2 ]
Xia, Dandan [3 ]
Zheng, Yufeng [4 ]
机构
[1] Tsinghua Univ, State Key Lab Tribol Adv Equipment, Beijing 100084, Peoples R China
[2] Tsinghua Univ, Dept Mech Engn, Beijing 100084, Peoples R China
[3] Peking Univ, Natl Engineerng Res Ctr Oral Biomat & Digital Med, Res Ctr Engn & Technol Computerized Dent, Dept Dent Mat,Natl Clin Res Ctr Oral Dis,Natl Ctr, Beijing 100081, Peoples R China
[4] Peking Univ, Sch Mat Sci & Engn, Beijing 100871, Peoples R China
来源
BIOMATERIALS ADVANCES | 2023年 / 153卷
基金
北京市自然科学基金;
关键词
Zn -Li -Mg alloy; Biodegradable metal; Laser powder bed fusion; Porous scaffolds; Bone implants; POWDER BED FUSION; ZN METAL PARTS; BONE DEFECTS; PURE ZINC; CORROSION; IMPLANTS; DESIGN; MICROSTRUCTURE;
D O I
10.1016/j.bioadv.2023.213571
中图分类号
TB3 [工程材料学]; R318.08 [生物材料学];
学科分类号
0805 ; 080501 ; 080502 ;
摘要
Alloying and structural design provide flexibility to modulate performance of biodegradable porous implants manufactured by laser powder bed fusion (L-PBF). Herein, bulk Zn-0.8Li-0.1Mg was first fabricated to indicate the influence of the ternary alloy system on strengthening effect. Porous scaffolds with different porosities, including 60 % (P60), 70 % (P70) and 80 % (P80), were designed and fabricated to study the influence of porosity on mechanical properties, in vitro degradation behavior, biocompatibility and osteogenic ability. Pure Zn (Zn-P70) scaffolds with a porosity of 70 % were utilized for the comparison. The results showed Zn-0.8Li-0.1Mg bulks had an ultimate tensile strength of 460.78 & PLUSMN; 5.79 MPa, which was more than 3 times that of pure Zn ones and was the highest value ever reported for Zn alloys fabricated by L-PBF. The compressive strength (CS) and elastic modulus (E) of scaffolds decreased with increasing porosities. The CS of P70 scaffolds was 24.59 MPa, more than 2 times that of Zn-P70. The weight loss of scaffolds during in vitro immersion increased with increasing porosities. Compared with Zn-P70, a lower weight loss, better biocompatibility and improved oste-ogenic ability were observed for P70 scaffolds. P70 scaffolds also exhibited the best biocompatibility and oste-ogenic ability among all the used porosities. Influence mechanism of alloying elements and structural porosities on mechanical behaviors, in vitro biodegradation behavior, biocompatibility and osteogenic ability of scaffolds were discussed using finite element analysis and the characterization of degradation products. The results indicated that the proper design of alloying and porosity made Zn-0.8Li-0.1Mg scaffolds promising for biode-gradable applications.
引用
收藏
页数:14
相关论文
共 50 条
  • [21] Additively manufactured porous Ti6Al4V Alloy with excellent mechanical properties, corrosion resistance, in vitro and in vivo biocompatibility
    Zhang, Lei
    Hu, Hongyan
    Wang, Quan
    Zhou, Jing
    Liu, Yan
    Li, Zonghao
    Zhang, Yonghui
    Kui, Zhitong
    He, Zhengyuan
    Jiang, Yehua
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 1009
  • [22] Regulating mechanical properties and degradation behavior of biodegradable Zn-0.6Mg alloy via ECAP plus cold rolling
    Ji, Chengwei
    Ma, Aibin
    Jiang, Jinghua
    Wu, Haoran
    Liu, Huan
    Guo, Sensen
    Yuan, Yuxuan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 937
  • [23] Microstructure, mechanical properties, biocompatibility, and in vitro corrosion and degradation behavior of a new Zn-5Ge alloy for biodegradable implant materials
    Tong, Xian
    Zhang, Dechuang
    Zhang, Xiaotuan
    Su, Yingchao
    Shi, Zimu
    Wang, Kun
    Lin, Jianguo
    Li, Yuncang
    Lin, Jixing
    Wen, Cuie
    ACTA BIOMATERIALIA, 2018, 82 : 197 - 204
  • [24] Synergistic effect of a biodegradable Mg-Zn alloy on osteogenic activity and anti-biofilm ability: an in vitro and in vivo study
    Yu, Weilin
    Chen, Daoyun
    Ding, Zhenyu
    Qiu, Manle
    Zhang, Zhiwang
    Shen, Ji
    Zhang, Xiaonong
    Zhang, Shaoxiang
    He, Yaohua
    Shi, Zhongmin
    RSC ADVANCES, 2016, 6 (51): : 45219 - 45230
  • [25] Fabrication of biodegradable Zn-Al-Mg alloy: Mechanical properties, corrosion behavior, cytotoxicity and antibacterial activities
    Bakhsheshi-Rad, H. R.
    Hamzah, E.
    Low, H. T.
    Kasiri-Asgarani, M.
    Farahany, S.
    Akbari, E.
    Cho, M. H.
    MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2017, 73 : 215 - 219
  • [26] Microstructure, Mechanical Properties, Corrosion Behavior and Biocompatibility of As-Extruded Biodegradable Mg-3Sn-1Zn-0.5Mn Alloy
    Hou, Lida
    Li, Zhen
    Zhao, Hong
    Pan, Yu
    Pavlinich, Sergey
    Liu, Xiwei
    Li, Xinlin
    Zheng, Yufeng
    Li, Li
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2016, 32 (09) : 874 - 882
  • [27] Effects of Li addition on the properties of biodegradable Zn-Fe-Li alloy: Microstructure, mechanical properties, corrosion behavior, and cytocompatibility
    Zhang, Jingdan
    Zhu, Xinglong
    Guo, Pushan
    Zhang, Yi
    Xu, Dingyang
    Pang, Yuan
    Song, Zhenlun
    Yang, Lijing
    MATERIALS TODAY COMMUNICATIONS, 2024, 39
  • [28] The Effect of Mn on the Mechanical Properties and In Vitro Behavior of Biodegradable Zn-2%Fe Alloy
    Ben Tzion-Mottye, Lital
    Ron, Tomer
    Eliezer, Dan
    Aghion, Eli
    METALS, 2022, 12 (08)
  • [29] Impact of scandium and terbium on the mechanical properties, corrosion behavior, and biocompatibility of biodegradable Mg-Zn-Zr-Mn alloys
    Munir, Khurram
    Lin, Jixing
    Tong, Xian
    Biesiekierski, Arne
    Li, Yuncang
    Wen, Cuie
    JOURNAL OF MAGNESIUM AND ALLOYS, 2024, 12 (02) : 546 - 572
  • [30] Microstructure,Mechanical Properties and In Vitro Degradation Behavior of a Novel Biodegradable Mg-1.5Zn-0.6Zr-0.2Sc Alloy
    Tao Li
    Hailong Zhang
    Yong He
    Ning Wen
    Xitao Wang
    JournalofMaterialsScience&Technology, 2015, 31 (07) : 744 - 750