Chemical resistance of alkali-activated mortar with nano silica and polypropylene fiber

被引:29
作者
Hussein, Twana Ahmed [2 ,3 ]
Dheyaaldin, Mahmood Hunar [1 ]
Mosaberpanah, Mohammad Ali [2 ]
Ahmed, Younus M. S. [3 ]
Mohammed, Hariwan A. [3 ]
Omer, Raian R. [3 ]
Hamid, Saad M. [3 ]
Alzeebaree, Radhwan [4 ,5 ]
机构
[1] Cihan Univ Erbil, Dept Civil Engn, Erbil, Iraq
[2] Cyprus Int Univ, Civil Engn Dept, Nicosia, North Cyprus, Turkiye
[3] Tishk Int Univ, Civil Engn Dept, Erbil, Iraq
[4] Duhok Polytech Univ, Highway & Bridge Dept, Duhok, Iraq
[5] Nawroz Univ, Civil Engn Dept, Duhok, Iraq
关键词
Polypropylene fiber; Nanosilica; Alkali activator mortar; Chemical resistant; Sorptivity; Mechanical properties; Durability; WASTE-GLASS POWDER; FLY-ASH; COMPRESSIVE STRENGTH; MECHANICAL PERFORMANCE; GEOPOLYMER CONCRETE; STEEL FIBERS; DURABILITY; ACID;
D O I
10.1016/j.conbuildmat.2022.129847
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In this study, the mechanical and long-term performance of alkali-activated mortar (AAM) were investigated. In the fresh phase, the flow table and fresh density were evaluated. The compressive and flexural strengths were investigated at 28 and 56 days. In addition, the water absorption, sorptivity, and chemical resistance (sulfuric acid, magnesium sulfate, and sodium chloride) of AAM were investigated after 56 days of exposure Nano silica with and without polypropylene fiber was added to the AAM mixtures and cured at ambient temperature (23 +/- 2 degrees C). Sodium silicates (Na2SiO3) and sodium hydroxide (NaOH) were used as alkaline-activated solution with a ratio of 1.5 to 2.5. The results show that the workability, water absorption, and sorptivity were better, with a ratio of 2.5 (the ratio of sodium silicates to sodium hydroxide). Nevertheless, the simultaneous use of fiber and nano-silica was adversely influenced. On the other hand, better hardened performanc was achieved with the ratio of 1.5. Moreover, the together use of fiber and nano-silica were reduced the flexural and compressive strengths when exposed to sulfuric acid, magnesium sulfate, and sodium chloride. In contrast, an increment of compressive strength was recorded for sodium chloride exposure.
引用
收藏
页数:13
相关论文
共 68 条
  • [1] A.C.C.-19 on Concrete C. Aggregates, 2013, STANDARD SPECIFICATI
  • [2] Effect of nano-silica on strength and durability of fly ash based geopolymer mortar
    Adak, D.
    Sarkar, M.
    Mandal, S.
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2014, 70 : 453 - 459
  • [3] Sugarcane bagasse ash-based engineered geopolymer mortar incorporating propylene fibers
    Akbar, Arslan
    Farooq, Furqan
    Shafique, Muhammad
    Aslam, Fahid
    Alyousef, Rayed
    Alabduljabbar, Hisham
    [J]. JOURNAL OF BUILDING ENGINEERING, 2021, 33
  • [4] Recycling of geopolymer concrete
    Akbarnezhad, A.
    Huan, M.
    Mesgari, S.
    Castel, A.
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2015, 101 : 152 - 158
  • [5] Bond Strength and Fracture Toughness of Alkali Activated Self-Compacting Concrete Incorporating Metakaolin or Nanosilica
    Alzeebaree, Radhwan
    [J]. SUSTAINABILITY, 2022, 14 (11)
  • [6] [Anonymous], 2015, 19612015 BS EN, P3
  • [7] [Anonymous], 1981, CAN BUILD DIG
  • [8] [Anonymous], 2020, AC109109M ASTM, P11
  • [9] [Anonymous], 2010, Annual Book of ASTM Standards, DOI DOI 10.1520/C0230
  • [10] Experimental mechanical-damage assessment of earthen mixes reinforced with micro polypropylene fibers
    Araya-Letelier, G.
    Concha-Riedel, J.
    Antico, F. C.
    Sandoval, C.
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2019, 198 : 762 - 776