Understand anisotropy dependence of damage evolution and material removal during nanoscratch of MgF2 single crystals

被引:142
作者
Li, Chen [1 ]
Piao, Yinchuan [1 ]
Zhang, Feihu [1 ]
Zhang, Yong [1 ]
Hu, Yuxiu [1 ]
Wang, Yongfei [1 ]
机构
[1] Harbin Inst Technol, State Key Lab Robot & Syst HIT, Harbin 150001, Peoples R China
基金
中国国家自然科学基金; 中国博士后科学基金;
关键词
anisotropy dependence; damage evolution; stress field; crack propagation; nanoscratch; MgF2 single crystal; DEFORMATION MECHANISM; BRITTLE MATERIALS; STRESS-FIELD; DEPTH; BEHAVIOR; SURFACE; INDENTATION; GENERATION; SAPPHIRE; SCRATCH;
D O I
10.1088/2631-7990/ac9eed
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
To understand the anisotropy dependence of the damage evolution and material removal during the machining process of MgF2 single crystals, nanoscratch tests of MgF2 single crystals with different crystal planes and directions were systematically performed, and surface morphologies of the scratched grooves under different conditions were analyzed. The experimental results indicated that anisotropy considerably affected the damage evolution in the machining process of MgF2 single crystals. A stress field model induced by the scratch was developed by considering the anisotropy, which indicated that during the loading process, median cracks induced by the tensile stress initiated and propagated at the front of the indenter. Lateral cracks induced by tensile stress initiated and propagated on the subsurface during the unloading process. In addition, surface radial cracks induced by the tensile stress were easily generated during the unloading process. The stress change led to the deflection of the propagation direction of lateral cracks. Therefore, the lateral cracks propagated to the workpiece surface, resulting in brittle removal in the form of chunk chips. The plastic deformation parameter indicated that the more the slip systems were activated, the more easily the plastic deformation occurred. The cleavage fracture parameter indicated that the cracks propagated along the activated cleavage planes, and the brittle chunk removal was owing to the subsurface cleavage cracks propagating to the crystal surface. Under the same processing parameters, the scratch of the (001) crystal plane along the [100] crystal-orientation was found to be the most conducive to achieving plastic machining of MgF2 single crystals. The theoretical results agreed well with the experimental results, which will not only enhance the understanding of the anisotropy dependence of the damage evolution and removal process during the machining of MgF2 crystals, but also provide a theoretical foundation for achieving the high-efficiency and low-damage processing of anisotropic single crystals.
引用
收藏
页数:17
相关论文
共 43 条
[1]   Sliding microindentation fracture of brittle materials: Role of elastic stress fields [J].
Ahn, Y ;
Farris, TN ;
Chandrasekar, S .
MECHANICS OF MATERIALS, 1998, 29 (3-4) :143-152
[2]  
Chen Zibin, 2021, Jgsymlmjgc, V41, P55, DOI 10.13394/j.cnki.jgsaa.2021.3.008
[3]   An analytical expression for the stress field around an elastoplastic indentation/contact [J].
Feng, G. ;
Qu, S. ;
Huang, Y. ;
Nix, W. D. .
ACTA MATERIALIA, 2007, 55 (09) :2929-2938
[4]   Unique crack behaviors of glass BK7 occurred in successive double scratch under critical load of median crack initiation [J].
Feng, Junyuan ;
Wan, Zhenping ;
Wang, Wei ;
Huang, Xiaofang ;
Ding, Xinrui ;
Tang, Yong .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2020, 40 (08) :3279-3290
[5]   All-precision-machining fabrication of ultrahigh-Q crystalline optical microresonators [J].
Fujii, Shun ;
Hayama, Yuka ;
Imamura, Kosuke ;
Kumazaki, Hajime ;
Kakinuma, Yasuhiro ;
Tanabe, Takasumi .
OPTICA, 2020, 7 (06) :694-701
[6]   Fundamentals of atomic and close-to-atomic scale manufacturing: a review [J].
Gao, Jian ;
Luo, Xichun ;
Fang, Fengzhou ;
Sun, Jining .
INTERNATIONAL JOURNAL OF EXTREME MANUFACTURING, 2022, 4 (01)
[7]  
Gao W., 2021, J DIAM ABRASIVES ENG, V41, P92
[8]   Investigation on friction behavior and processing depth prediction of polymer in nanoscale using AFM probe-based nanoscratching method [J].
Geng, Yanquan ;
Yan, Yongda ;
He, Yang ;
Hu, Zhenjiang .
TRIBOLOGY INTERNATIONAL, 2017, 114 :33-41
[9]   Scratch-induced microplasticity and microcracking in zirconium diboride-silicon carbide composite [J].
Ghosh, Dipankar ;
Subhash, Ghatu ;
Radhakrishnan, Ramachandran ;
Sudarshan, Tirumalai S. .
ACTA MATERIALIA, 2008, 56 (13) :3011-3022
[10]   Theoretical approach on the critical depth of cut of single crystal MgF2 and application to a microcavity [J].
Hayama, Yuka ;
Fujii, Shun ;
Tanabe, Takasumi ;
Kakinuma, Yasuhiro .
PRECISION ENGINEERING-JOURNAL OF THE INTERNATIONAL SOCIETIES FOR PRECISION ENGINEERING AND NANOTECHNOLOGY, 2022, 73 :234-243