Influence of Defects in Surface Layer of Al2O3/TiC and SiAlON Ceramics on Physical and Mechanical Characteristics

被引:5
|
作者
Grigoriev, Sergey N. [1 ]
Volosova, Marina A. [1 ]
Okunkova, Anna A. [1 ]
Fedorov, Sergey V. [1 ]
机构
[1] Moscow State Univ Technol STANKIN, Dept High Efficiency Proc Technol, Vadkovskiy Per 3A, Moscow 127994, Russia
来源
CERAMICS-SWITZERLAND | 2023年 / 6卷 / 02期
关键词
Al2O3; TiC ceramics; defects; diamond grinding; fracture resistance; lapping; polishing; SiAlON ceramics; surface layer condition; wear resistance; WEAR MECHANISM; CUTTING PERFORMANCE; THERMAL FACTOR; TOOL LIFE; STEEL; DRY; PVD; TEMPERATURE; SIMULATION; FRACTURE;
D O I
10.3390/ceramics6020047
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The paper studies the influence of diamond grinding, lapping, and polishing on the surface layer and defectiveness of the Al2O3/TiC and SiAlON ceramic samples. The index of defectiveness I-D, which is the product of the defect density and the defective layer's thickness (R-t), and a method for its evaluation are proposed to quantify the defectiveness of the ceramic surfaces. Lapping reduces the R-t parameter by 2.6-2.7 times when the density of defects was decreased by 2 times. After polishing, the R-t parameter decreases to 0.42 & mu;m for Al2O3/TiC and 0.37 & mu;m for SiAlON samples. The density of defects decreases many times after polishing: up to 0.005 and 0.004, respectively. The crack resistance of the polished samples increased by 5-7%. The volumetric wear of polished samples decreased by 1.5-1.9 times compared to the ground ones after 20 min of abrasion wear. The polished samples show a decrease in the coefficient of friction at 800 & DEG;C and a decrease in the volumetric wear by 1.5 and 1.3 times, respectively, compared to the ground ones after 200 m of friction distance. The volumetric wear at high-temperature friction of sliding for polished specimens was 55% and 42% less than for the ground ones, respectively.
引用
收藏
页码:818 / 836
页数:19
相关论文
共 50 条
  • [41] Improved Corrosion Resistance and Mechanical Properties of CrN Hard Coatings with an Atomic Layer Deposited Al2O3 Inter layer
    Wan, Zhixin
    Zhang, Teng Fei
    Lee, Han-Bo-Ram
    Yang, Ji Hoon
    Choi, Woo Chang
    Han, Byungchan
    Kim, Kwang Ho
    Kwon, Se-Hun
    ACS APPLIED MATERIALS & INTERFACES, 2015, 7 (48) : 26716 - 26725
  • [42] Microstructure and mechanical properties of ZrO2-40 wt% Al2O3 composite ceramics
    Abden, M. J.
    Afroze, J. D.
    Mamun, M. A.
    Haque, M. M.
    MATERIALS EXPRESS, 2014, 4 (04) : 317 - 323
  • [43] Influence of Co-enriched surface zones in cemented carbides on the microstructure and mechanical properties of TiN/TiC0.6N0.4/ α-Al2O3 coatings
    Konstantiniuk, Fabian
    Krobath, Martin
    Ecker, Werner
    Tkadletz, Michael
    Czettl, Christoph
    Schalk, Nina
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2023, 110
  • [44] Influence of Al2O3 sol concentration on the microstructure and mechanical properties of Cu-Al2O3 composite coatings
    Wei, Xiaojin
    Yang, Zhendi
    Tang, Ying
    Gao, Wei
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2015, 29 (10-11):
  • [45] Effect of sintering additives of carbon black, SiC, Al2O3, and Al2O3 + Y2O3 on microstructure and mechanical properties of B4C ceramics
    Zhang, Wei
    Zhang, Jie
    JOURNAL OF THE KOREAN CERAMIC SOCIETY, 2024, 61 (06) : 1079 - 1090
  • [46] Mechanical and CMAS resistance properties of Al2O3 modified Yb2Si2O7 ceramics
    Zang, Kai
    Liang, Wenping
    Miao, Qiang
    Sun, Yuanyuan
    Tan, Xiaoqi
    Wu, Min
    Liu, Qijia
    CERAMICS INTERNATIONAL, 2025, 51 (04) : 4847 - 4860
  • [47] Preparation, microstructures, and mechanical properties of directionally solidified Al2O3/Lu3Al5O12 eutectic ceramics
    Sun, Haofei
    Zhou, Cui
    Du, Tiefeng
    Wu, Zhen
    Xian, Quangang
    Sun, Luchao
    Liu, Jing
    Wang, Jingyang
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2022, 19 (02) : 695 - 702
  • [48] Microwave sintering and mechanical properties of La2O3/Nb2O5 toughened Al2O3 ceramics
    Liu, Jin
    Liang, Bingliang
    Ai, Yunlong
    Zhang, Jianjun
    He, Fei
    He, Wen
    Liu, Zhiyong
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2021, 22 (03): : 296 - 300
  • [49] Toughening of the Al2O3-TiC ceramics by depositing thin coatings
    Konyashin, IY
    SURFACE & COATINGS TECHNOLOGY, 1996, 79 (1-3) : 192 - 199
  • [50] Capacitance-conductance characteristics of Au/Ti/Al2O3/n-GaAs structures with very thin Al2O3 interfacial layer
    Turut, A.
    Karabulut, A.
    Ejderha, K.
    Biyikli, N.
    MATERIALS RESEARCH EXPRESS, 2015, 2 (04)