3D printing of honeycomb Si3N4 ceramic

被引:8
作者
Ma, Siqi [1 ,2 ]
Fu, Shuai [3 ]
Wang, Qikun [1 ,2 ]
Yang, Hualong [1 ,2 ]
Li, Wanlin [1 ,2 ]
He, Peigang [1 ,2 ]
Wang, Meirong [4 ]
Cai, Delong [5 ]
Duan, Xiaoming [1 ,2 ]
Jia, Dechang [1 ,2 ]
Lin, Hua-Tay [6 ]
Zhou, Yu [1 ,2 ]
机构
[1] Harbin Inst Technol, Inst Adv Ceram, Sch Mat Sci & Engn, Harbin, Peoples R China
[2] Harbin Inst Technol, Key Lab Adv Struct Funct Integrat Mat & Green Mfg, Harbin, Peoples R China
[3] Max Planck Inst Polymer Res, Mainz, Germany
[4] Harbin Inst Technol, Sch Mat Sci & Engn, Weihai, Peoples R China
[5] Harbin Engn Univ, Coll Mat Sci & Chem Engn, Key Lab Superlight Mat & Surface Technol, Minist Educ, Harbin, Peoples R China
[6] Guangdong Univ Technol, Sch Electromech Engn, Guangzhou, Peoples R China
基金
中国国家自然科学基金;
关键词
3D printing; honeycomb Si3N4 ceramics; non-catastrophic fracture; rheological properties; slump rates; SILICON-NITRIDE CERAMICS; FABRICATION; STRENGTH; MICROSTRUCTURE; PERFORMANCE; ABSORPTION; DENSE;
D O I
10.1111/ijac.14384
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this paper, a honeycomb Si3N4 ceramic was fabricated by 3D printing with a well-preserved structure. The effects of Si3N4 content on the rheological properties of Si3N4/sol-silica ink and the printing resolution of products were investigated. The microstructure, phase composition, liner shrinkage rate, and fracture behavior of printed samples before and after sintering were systematically characterized in detail. The results showed that the modified inks had the optimized rheological properties, and the stress-shear rate curves corresponding to each slurry could be well described by Bingham and Herschel-Bulkley fluid models. The corresponding slump rates of the printed samples with different Si3N4 to sol-silica mass ratios were all lower than 4%, and the linear shrinkage rate of all of the samples after sintering was below 20%. The fracture behavior under compressive loading of the honeycomb Si3N4 ceramics tended to be non-catastrophic fractures both before and after sintering. The compressive strengths of all of the printed samples decreased with the increase of the Si3N4 content, and the highest compressive strength of the honeycomb ceramics could reach 131.2 MPa after sintering at 1600 degrees C, which was about 366.9% higher than that of the samples in green state prior to the sintering.
引用
收藏
页码:2239 / 2248
页数:10
相关论文
共 50 条
  • [41] Ag/Ni Sintering Metallization on Si3N4 Ceramic Package Substrate
    Wang, Beiji
    Jia, Xiangya
    Xu, Shunjian
    Zhang, Xiangzhao
    Zhou, Yansheng
    Habila, Mohamed A.
    Hussain, Shahid
    Qiao, Guanjuan
    Liu, Guiwu
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, : 9499 - 9505
  • [42] Microstructure-permeability relation of porous β-Si3N4 ceramics
    Topates, Gulsum
    Mammitzsch, Lars
    Petasch, Uwe
    Adler, Joerg
    Kara, Ferhat
    Mandal, Hasan
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2013, 33 (09) : 1545 - 1551
  • [43] Defect-free Si3N4 ceramics by vat photopolymerization 3D printing with nitrogen-hydrogen debinding atmosphere
    Shen, Minhao
    Fu, Renli
    Zhang, Yi
    Sun, Kuang
    Xu, Wei
    Jiang, Yanlin
    Zhao, Zhe
    Liu, Ming
    CERAMICS INTERNATIONAL, 2024, 50 (21) : 42709 - 42720
  • [44] Multi-Material 3D and 4D Printing: A Survey
    Rafiee, Mohammad
    Farahani, Rouhollah D.
    Therriault, Daniel
    ADVANCED SCIENCE, 2020, 7 (12)
  • [45] Comparison in microstructure and mechanical properties of porous Si3N4 ceramics with SiC and Si3N4 coatings
    Li, Xiangming
    Yin, Xiaowei
    Zhang, Litong
    Pan, Tianhao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 527 (1-2): : 103 - 109
  • [46] Fabrication of porous Si3N4 ceramics with controlled porosity by milling of fibrous α-Si3N4 powder
    Xu, Zhaoyun
    Zhang, Yaming
    Wang, Bo
    Yang, Jianfeng
    Liu, Kaikai
    JOURNAL OF CERAMIC PROCESSING RESEARCH, 2016, 17 (08): : 840 - 844
  • [47] Preparation of Porous Si3N4 Ceramics with Controlled Porosity and Microstructure by Fibrous α-Si3N4 Addition
    Xu, Zhaoyun
    Wang, Bo
    Yang, Jianfeng
    Zhao, Zhongjian
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2014, 97 (11) : 3392 - 3395
  • [48] Novel design of a Si3N4/BaO-Al2O3-SiO2 coating with a heterogeneous- layer structure on porous Si3N4 ceramic
    Liu, Zhengdao
    Tong, Zongwei
    Yue, Sheng
    Li, Xiaolei
    Ji, Huiming
    CERAMICS INTERNATIONAL, 2021, 47 (01) : 1456 - 1461
  • [49] Effect of Si3N4 nanowires on the mechanical properties and dielectric constant of porous Si3N4 ceramics
    Zhang, Tianxiang
    Zhang, Xinghong
    Han, Wenbo
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2019, 127 (09) : 602 - 605
  • [50] Hard and tough novel high-pressure γ-Si3N4/Hf3N4 ceramic nanocomposites
    Li, Wei
    Yu, Zhaoju
    Wiehl, Leonore
    Jiang, Tianshu
    Zhan, Ying
    Ricohermoso, Emmanuel I. I. I.
    Etter, Martin
    Ionescu, Emanuel
    Wen, Qingbo
    Lathe, Christian
    Farla, Robert
    Teja, Dharma Teppala
    Bruns, Sebastian
    Widenmeyer, Marc
    Weidenkaff, Anke
    Molina-Luna, Leopoldo
    Riedel, Ralf
    Bhat, Shrikant
    JOURNAL OF ADVANCED CERAMICS, 2023, 12 (07): : 1418 - 1429